IP Library Granted Patent US 10,836,939
Granted Patent B2
US 10,836,939 · App. 15/410,510 · Granted Nov 17, 2020

One-part polyurethane adhesive composition, method of making a laminate, and laminate

Inventors: Anthony J. Ostlund (Forest Lake, MN); Dorian P. Nelson (St. Paul, MN); Wayne G. Eklund (Scandia, MN); Marlen A. Valverde (Stillwater, MN)
Assignee: H.B. Fuller Company
C09J175/04B32B5/022B32B5/024B32B5/18B32B5/245B32B5/26B32B5/32B32B7/12B32B15/043B32B15/046B32B15/08B32B15/082B32B15/085B32B15/088B32B15/09B32B15/12B32B15/14B32B15/20B32B23/04B32B23/042B32B23/048B32B23/06B32B23/08B32B23/10B32B27/06B32B27/065B32B27/08B32B27/10B32B27/12B32B27/16B32B27/302B32B27/304B32B27/306B32B27/32B32B27/34B32B27/36B32B27/365B32B29/002B32B29/005B32B29/007B32B29/02B32B29/08B32B37/12B65D65/14B65D65/40C08G18/10C08G18/12C08G18/34C08G18/36C08G18/4854C08G18/6625C08G18/68C08G18/7671C09J5/04C09J175/08B32B2250/20B32B2250/22B32B2250/24B32B2250/26B32B2255/10B32B2255/205B32B2255/26B32B2262/02B32B2262/0253B32B2262/0261B32B2262/0276B32B2262/062B32B2266/025B32B2266/0207B32B2266/0278B32B2307/306B32B2307/54B32B2307/546B32B2307/7246B32B2307/732B32B2323/04B32B2323/046B32B2323/10B32B2367/00B32B2375/00B32B2439/70B32B2439/80B32B2457/00B32B2457/20B32B2553/00B65D31/02B65D75/26
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,836,939
App. No.
15/410,510
Granted
Nov 17, 2020
Kind
B2
Abstract

Disclosed is a one-part, atmospheric curing, polyurethane adhesive composition that includes a polyurethane prepolymer that includes a reaction product of a polyol component and an isocyanate component, the polyol component comprising an unsaturated fatty acid esterified polyol comprising a reaction product of a first polyol and at least one of an ethylenically unsaturated oil and an ethylenically unsaturated fatty acid, the first polyol comprising at least three hydroxyl groups, and a % NCO of from at least 4% by weight to no greater than 7% by weight based on the weight of the prepolymer, the adhesive composition exhibiting a viscosity of no greater than 15,000 centipoise at 60° C., and a T-peel value of greater than 40 grams per 25 millimeter in no greater than 4 hours, a method of making a laminate, and a laminate that includes a one-part, atmospheric curing, polyurethane adhesive composition.

Claims (52)

1. A one-part, atmospheric curing, polyurethane adhesive composition comprising:

a polyurethane prepolymer comprising

a reaction product of a polyol component and an isocyanate component, the polyol component comprising an unsaturated fatty acid esterified polyol comprising a reaction product of a first polyol and an ethylenically unsaturated component selected from the group consisting of ethylenically unsaturated oil, an ethylenically unsaturated fatty acid, and combinations thereof,

the first polyol comprising at least three hydroxyl groups, and

a % NCO of from at least 4% by weight to no greater than 7% by weight based on the weight of the prepolymer,

the adhesive composition exhibiting

a viscosity of no greater than 15,000 centipoise (cP) at 60° C., and

a T-Peel value of greater than 40 grams per 25 millimeter (g/25 mm) within no greater than 4 hours when tested according to T-Peel Adhesion Test Method II.

2. The one-part adhesive composition of claim 1 , wherein the adhesive composition exhibits a viscosity of no greater than 11,000 centipoise (cP) at 60° C.

3. The one-part adhesive composition of claim 1 , wherein the adhesive composition exhibits a PAA Food Migration Value of no greater than 10 microgram/kilogram within 3 days.

4. The one-part adhesive composition of claim 1 , wherein the adhesive composition exhibits a T-Peel value of greater than 250 g/25 mm in less than 6 hours when tested according to T-Peel Adhesion Test Method II.

5. The one-part adhesive composition of claim 1 , wherein the adhesive composition further comprises a second polyol comprising a polyether polyol.

6. The one-part adhesive composition of claim 1 , wherein the prepolymer comprises from at least 4% by weight NCO to no greater than 6% by weight NCO based on the weight of the prepolymer.

7. The one-part adhesive composition of claim 1 , wherein the adhesive composition exhibits a PAA Food Migration Value that is less than 35% of the Control within 3 days.

8. A laminate comprising

a first substrate,

a second substrate comprising a sealant film, and

a cured adhesive composition derived from the adhesive composition of claim 1 ,

the first substrate being bonded to the second substrate through the cured adhesive composition.

9. The laminate of claim 8 , wherein the first and the second substrates are flexible substrates comprising a polymer film selected from the group consisting of a metallized polymer film, polyethylene terephthalate, polypropylene, polyethylene, metallized polypropylene, metalized polyethylene terephthalate, polyamide, metal foil, paper, polylactic, and combinations thereof.

10. The laminate of claim 8 , wherein the laminate exhibits a PAA Food Migration Value of no greater than 10 micrograms/kilogram within 3 days.

11. A food package comprising:

a food product; and

the laminate of claim 8 at least partially surrounding the product.

12. The one-part, atmospheric curing, polyurethane adhesive composition claim 1 , wherein the unsaturated fatty acid esterified polyol has an average hydroxyl functionality of from 1.5 to 2.5.

13. The one-part, atmospheric curing, polyurethane adhesive composition claim 1 , wherein the unsaturated fatty acid esterified polyol is a reaction product of trimethylol propane and soybean oil.

14. The one-part, atmospheric curing, polyurethane adhesive composition claim 1 , wherein the ethylenically unsaturated oil comprises a vegetable oil selected from the group consisting of soybean oil, linseed oil, tung oil, sunflower oil, safflower oil, tall oil, olive oil, cottonseed oil, and combinations thereof, and the ethylenically unsaturated fatty acid is selected from the group consisting of oleic acid, linoleic acid, linolenic acid, eicosadienoic acid, arachidonic acid, and combinations thereof.

15. The one-part, atmospheric curing, polyurethane adhesive composition claim 1 , wherein the first polyol is selected from the group consisting of trimethylol propane, ditrimethylol propane, glycerol, pentaerythritol, dipentaerythritol, trimethylolethane, xylitol, sorbitol, mannitol, sucrose, castor oil, and combinations thereof.

16. A laminate comprising:

a first substrate;

a cured adhesive composition derived from a polyurethane prepolymer that is a reaction product of a polyol component and an isocyanate component, the polyol component comprising an unsaturated fatty acid esterified polyol that is a reaction product of a first polyol and at least one of an ethylenically unsaturated oil and an ethylenically unsaturated fatty acid, the first polyol being selected from the group consisting of trimethylol propane, ditrimethylol propane, glycerol, pentaerythritol, dipentaerythritol, trimethylolethane, xylitol, sorbitol, mannitol, sucrose, castor oil, and combinations thereof; and

a second substrate bonded to the first substrate through the cured adhesive composition,

the laminate exhibiting at least one of

a PAA Food Migration Value of no greater than 10 micrograms/kilogram within 2 days, and

a T-Peel value of at least 40 g/25 mm within no greater than 4 hours when tested according to T-Peel Adhesion Test Method I.

17. The laminate of claim 16 , wherein the ethylenically unsaturated oil comprises a vegetable oil comprising soybean oil, linseed oil, tung oil, sunflower oil, safflower oil, tall oil, olive oil, cottonseed oil, or a combination thereof, and the ethylenically unsaturated fatty acid comprises oleic acid, linoleic acid, linolenic acid, eicosadienoic acid, arachidonic acid, or a combination thereof.

18. The laminate of claim 16 , wherein the first polyol is selected from the group consisting of trimethylol propane, ditrimethylol propane, glycerol, pentaerythritol, dipentaerythritol, trimethylolethane, xylitol, sorbitol, mannitol, sucrose, castor oil, and combinations thereof.

19. A one-part, atmospheric curing, polyurethane adhesive composition comprising:

a polyurethane prepolymer comprising

a reaction product of a polyol component and an isocyanate component, the polyol component comprising an unsaturated fatty acid esterified polyol comprising a reaction product of a first polyol and at least one of an ethylenically unsaturated oil and an ethylenically unsaturated fatty acid,

the first polyol comprising at least three hydroxyl groups and being selected from the group consisting of trimethylol propane, ditrimethylol propane, glycerol, pentaerythritol, dipentaerythritol, trimethylolethane, xylitol, sorbitol, mannitol, sucrose, castor oil, and combinations thereof,

the ethylenically unsaturated oil being selected from the group consisting of soybean oil, linseed oil, tung oil, sunflower oil, safflower oil, tall oil, olive oil, cottonseed oil, and combinations thereof, and the ethylenically unsaturated fatty acid being selected from the group consisting of oleic acid, linoleic acid, linolenic acid, eicosadienoic acid, arachidonic acid, and combinations thereof, and

a % NCO of from at least 4% by weight to no greater than 7% by weight based on the weight of the prepolymer,

the adhesive composition exhibiting

a viscosity of no greater than 15,000 centipoise (cP) at 60° C., and

a T-Peel value of greater than 40 grams per 25 millimeter (g/25 mm) within no greater than 4 hours when tested according to T-Peel Adhesion Test Method II.

20. A method of making the laminate of claim 16 , the method comprising:

applying a one-part, atmospheric curable adhesive composition to the first substrate, and

contacting the adhesive composition with the second substrate to form the laminate,

the laminate further exhibiting a PAA Food Migration Value that is less than 35% of the Control within 3 days.

21. The method of claim 20 , wherein the laminate further exhibits a T-Peel value of greater than 250 g/25 mm in less than 6 hours when tested according to T-Peel Adhesion Test Method I.

22. The method of claim 20 , wherein the first and the second substrates are flexible substrates comprising a polymer film selected from the group consisting of a metallized polymer film, polyethylene terephthalate, polypropylene, polyethylene, metallized polypropylene, metalized polyethylene terephthalate, polyamide, metal foil, paper, polylactic, and combinations thereof.

Assignments (2)
SECURITY INTEREST Recorded Feb 16, 2023
From: H.B. FULLER COMPANY; H.B. FULLER CONSTRUCTION PRODUCTS INC.; ADCO PRODUCTS, LLC
To: JPMORGAN CHASE BANK, N.A., AS COLLATERAL AGENT
Reel/Frame 062775/0944 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 10, 2017
From: OSTLUND, ANTHONY J; NELSON, DORIAN P; EKLUND, WAYNE G; VALVERDE, MARLEN A
To: H. B. FULLER COMPANY