IP Library Granted Patent US 9,999,808
Granted Patent B2
US 9,999,808 · App. 15/467,020 · Granted Jun 19, 2018

Golf ball covers made from plasticized thermoplastic materials

Inventors: Michael J. Sullivan (Old Lyme, CT); Mark L. Binette (Mattapoisett, MA); Robert Blink (Newport, RI); David A. Bulpett (Boston, MA); Brian Comeau (Berkley, MA); Douglas S. Goguen (New Bedford, MA)
Assignee: Acushnet Company
A63B37/0043A63B37/0024A63B37/0039A63B37/0075A63B37/0076A63B37/0092
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,999,808
App. No.
15/467,020
Granted
Jun 19, 2018
Kind
B2
Abstract

Multi-layered golf balls containing a two or three-layered cover assembly are provided. In one embodiment, the cover assembly includes a relatively hard inner cover and relatively soft outer cover. Alternatively, the cover assembly may include a relatively soft inner cover with a relatively hard outer cover. Three-layered covers comprising an inner cover, intermediate cover, and outer cover layer also may be prepared. Preferably, at least one of the layers is formed from a thermoplastic composition that preferably comprises: a) ethylene acid copolymer, b) plasticizer, and c) cation source. A fatty acid ester such as ethyl oleate is preferably used as the plasticizer. The cover assembly has good impact durability and helps provide the ball with relatively high resiliency at given compressions.

Claims (18)

1. A golf ball, comprising:

i) a core having at least one layer;

ii) an inner cover layer comprising a thermoplastic material, the inner cover layer being disposed about the core and having a Shore D midpoint hardness in the range of about 55 to about 75, the thermoplastic material comprising:

a) an acid copolymer of ethylene and an α,β-unsaturated carboxylic acid, optionally including a softening monomer selected from the group consisting of alkyl acrylates and methacrylates;

b) a plasticizer in an amount from about 3 to about 50% by weight, the plasticizer being an alkyl oleate selected from the group consisting of methyl oleate, ethyl oleate, propyl oleate, butyl oleate, and octyl oleate, and mixtures thereof; and

c) a cation source present in an amount sufficient to neutralize from about 0 to about 100% of all acid groups present in the material; and

iii) an outer cover layer disposed about the inner cover layer and having a Shore D surface hardness in the range of about 15 to about 60, wherein the hardness of the outer cover layer is less than the hardness of the inner cover layer.

2. The golf ball of claim 1 , wherein the thermoplastic material comprises an ethylene acid copolymer containing acid groups such that 70% or less of the acid groups are neutralized.

3. The golf ball of claim 1 , wherein the thermoplastic material comprises an ethylene acid copolymer containing acid groups such that greater than 70% of the acid groups are neutralized.

4. The golf ball of claim 3 , wherein 90% or greater of the acid groups are neutralized.

5. The golf ball of claim 1 , wherein the ethylene acid copolymer is selected from the group consisting of ethylene/(meth)acrylic acid/n-butyl acrylate; ethylene/(meth)acrylic acid/ethyl acrylate; ethylene/(meth)acrylic acid/methyl acrylate; ethylene/(meth)acrylic acid/n-butyl acrylate; and ethylene/(meth)acrylic acid/isobutyl acrylate copolymers.

6. A golf ball, comprising:

i) a core having at least one layer;

ii) an inner cover layer comprising a thermoplastic material, the inner cover layer being disposed about the core and having a Shore D midpoint hardness in the range of about 55 to about 75

iii) an outer cover layer comprising a second thermoplastic material, the outer cover disposed about the inner cover layer and having a Shore D surface hardness in the range of about 15 to about 60, wherein the hardness of the outer cover layer is less than the hardness of the inner cover layer, the second thermoplastic material comprising:

a) an acid copolymer of ethylene and an α,β-unsaturated carboxylic acid, optionally including a softening monomer selected from the group consisting of alkyl acrylates and methacrylates;

b) plasticizer in an amount from about 3 to about 50% by weight, the plasticizer being an alkyl oleate selected from the group consisting of methyl oleate, ethyl oleate, propyl oleate, butyl oleate, and octyl oleate, and mixtures thereof; and

c) a cation source present in an amount sufficient to neutralize from about 0 to about 100% of all acid groups present in the material.

Assignments (4)
ASSIGNMENT OF SECURITY INTEREST IN PATENTS (ASSIGNS 051618-0777) Recorded Aug 3, 2022
From: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS RESIGNING ADMINISTRATIVE AGENT
To: JPMORGAN CHASE BANK, N.A., AS SUCCESSOR ADMINISTRATIVE AGENT
Reel/Frame 061069/0731 →
SECURITY INTEREST Recorded Aug 3, 2022
From: ACUSHNET COMPANY
To: JPMORGAN CHASE BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 061099/0236 →
SECURITY INTEREST Recorded Jan 15, 2020
From: ACUSHNET COMPANY
To: WELLS FARGO BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 051618/0777 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 23, 2017
From: SULLIVAN, MICHAEL J.; BINETTE, MARK L.; BLINK, ROBERT; BULPETT, DAVID A.; COMEAU, BRIAN; GOGUEN, DOUGLAS S.
To: ACUSHNET COMPANY
Reel/Frame 041696/0822 →
Continuity (12)
Continuation 15417398 · Jan 27, 2017
Continuation In Part 14527857 · Oct 30, 2014
Continuation 14511221 · Oct 10, 2014
Continuation In Part 14460416 · Aug 15, 2014
Continuation In Part 14145578 · Dec 31, 2013
Continuation In Part 13323128 · Dec 12, 2011
Division 12423921 · Apr 15, 2009
Continuation In Part 12407856 · Mar 20, 2009
Continuation In Part 11972240 · Jan 10, 2008
Continuation In Part 12407865 · Mar 20, 2009
Continuation In Part 11972240 · Jan 10, 2008
Related Publication 20170189763A1 · Jul 6, 2017