IP Library Granted Patent US 10,744,600
Granted Patent B2
US 10,744,600 · App. 15/489,835 · Granted Aug 18, 2020

Metal plate for laser processing and method for producing stainless steel plate for laser processing

Inventors: Kazuyoshi Fujisawa (Tokyo, JP); Masayuki Shibuya (Tokyo, JP); Kouichi Takeuchi (Tokyo, JP)
Assignee: NIPPON STEEL CORPORATION
B23K26/40B05C21/005B21B1/26B21B1/38B23K1/0016B23K3/0638B23K3/08B23K26/14B23K26/382B23K26/384C21D1/28C21D1/30C21D8/0226C21D8/0236C21D8/0247C21D8/0273C21D9/46C22C14/00C22C38/001C22C38/02C22C38/04C22C38/18C22C38/38C22C38/40C22C38/48C22C38/58C22F1/183B21B2001/386B23K2101/18B23K2101/42B23K2103/05B23K2103/10B23K2103/14B23K2103/26C21D2211/001C21D2211/005C21D2261/00C22C38/002Y10T428/12Y10T428/12361
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,744,600
App. No.
15/489,835
Granted
Aug 18, 2020
Kind
B2
Abstract

A metal plate for laser processing (such as a stainless steel plate or a titanium plate) and preferably an austenitic stainless steel plate suitable for use as a metal mask or the like which undergoes fine processing with a laser has an average grain diameter d (μm) and a plate thickness t (μm) which satisfy the equation d≤0.0448·t−1.28.

Claims (6)

1. A method of making a metal mask comprising:

providing a metal plate selected from an austenitic stainless steel plate, a ferritic stainless steel plate, and a titanium plate, the metal plate having a centerline surface roughness of at most 0.16 μm, a plate thickness t of at most 400 μm, and an average grain diameter d, wherein the plate thickness t and average grain diameter d satisfy the following Equation (1):

d≤ 0.0448· t− 1.28  (1);

where a unit of d and t is μm;

cutting the metal plate into a metal mask using a laser beam so that a pattern of holes or slits is formed in the metal mask;

the metal plate having a spreading value of at most 10% of the plate thickness wherein the spreading value is determined by subtracting a cut width of the hole or slit in a surface of the metal plate on an exit side of the laser beam from a cut width of the hole or slit in a surface of the metal plate on an incident side of the laser beam.

Assignments (1)
CHANGE OF NAME Recorded May 14, 2019
From: NIPPON STEEL & SUMITOMO METAL CORPORATION
To: NIPPON STEEL CORPORATION
Reel/Frame 049257/0828 →
Priority Claims (1)
JP 2011-043907 · Mar 1, 2011 · national
Continuity (2)
Continuation 14002398
Related Publication 20170239755A1 · Aug 24, 2017
Cited By (1)
US 12,635,380