US 10,364,361 · App. 15/535,480 · Granted Jul 30, 2019

Weatherproof aqueous wood coatings

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,364,361
App. No.
15/535,480
Granted
Jul 30, 2019
Kind
B2
Abstract

An aqueous based coating composition comprising a fatty amine quaternary having the structure of formula (I): R 1 R 2 R 3 R 4 N + X − wherein R 1 , R 2 , R 3 , and R 4 are independently selected from saturated or unsaturated, linear or branched, substituted or unsubstituted alkyl, aralkyl, or alkenyl groups comprising from 1 to 30 carbon atoms, whereby at least one of R 1 , R 2 , R 3 , and R 4 is a C12-C30 group, and X − is an anion from an inorganic or organic acid, is provided. The fatty amine quaternary may contain ethoxy and/or propoxy groups. One or more of R 1 , R 2 , R 3 , and R 4 may be substituted and contain one or more hydroxyl substituents or ether linkages. Methods for imparting water resistance to a wood substrate having up to 100% moisture by applying a coating composition having the fatty amine quaternary of formula (I), and for preparing an aqueous coating composition comprising the fatty amine quaternary of formula (I) are provided. Also provided is a coated water resistant wood substrate comprising the fatty amine quaternary of formula (I).

Claims (25)

1. An aqueous coating composition comprising:

an aqueous solvent,

a fatty amine quaternary having the following structure:

R 1 R 2 R 3 R 4 N + X −

 wherein R 1 , R 2 , R 3 , and R 4 are independently chosen from saturated or unsaturated, linear or branched, substituted or unsubstituted, alkyl, aralkyl, or alkenyl groups, comprising from 1 to 30 carbon atoms, wherein at least one of R 1 , R 2 , R 3 , and R 4 includes both a C12-C30 group and ethoxy and/or propoxy groups, wherein X − is an anion from an inorganic or organic acid, and wherein the number average molecular weight of the fatty amine quaternary is between about 100 g/mol and about 1500 g/mol, and

binder in an amount of between 40% to 90% by weight of the aqueous coating composition.

2. The aqueous coating composition of claim 1 , wherein at least one of R 1 , R 2 , R 3 , and R 4 contains a hydroxyl substituent or ether linkage.

3. The aqueous coating composition of claim 1 , wherein the number of ethoxy groups is between 1 and 30.

4. The aqueous coating composition of claim 1 , wherein the number of propoxy groups is between 1 and 10.

5. The aqueous coating composition of claim 1 , wherein the number of ethoxy and propoxy groups is between 1 and 40.

6. The aqueous coating composition of claim 5 , wherein the ethoxy and/or propoxy groups are in random or block configuration.

7. The aqueous coating composition of claim 1 , wherein the fatty amine quaternary comprises a fatty acid component selected from the group consisting of tallow, coconut, soya, palm, palm kernel, tall oil, rapeseed, lard, sunflower oil, corn oil, safflower oil, canola oil, olive oil, and peanut oil.

8. The aqueous coating composition of claim 1 , wherein the fatty amine quaternary comprises a fatty acid that is oleic acid or erucic acid.

9. The aqueous coating composition of claim 1 , wherein at least two of R 1 , R 2 , R 3 , and R 4 comprise at least six carbon atoms.

10. The aqueous coating composition of claim 1 , wherein the fatty amine quaternary is present in an amount of from about 0.1 wt % to about 20 wt % of the aqueous coating composition.

11. A method of imparting water resistance to a wood substrate, the method comprising applying from 0.1 grams to 10 grams of the aqueous coating composition of claim 1 per 100 cm 2 of substrate surface area.

12. The method of claim 11 , wherein the wood substrate has a moisture content between about 30% and about 50%, and wherein applying the aqueous coating to the wood substrate provides at least 70% water resistance to the wood substrate.

13. The method of claim 11 , wherein the wood substrate has a moisture content between about 10% and about 80%.

14. A method of preparing an aqueous coating composition with early moisture resistance, comprising the step of:

combining the fatty amine quaternary of claim 1 with an aqueous coating composition containing a binder, such that the aqueous coating composition with early moisture resistance comprises the binder in an amount of between 40% to 90% by weight.

15. The aqueous coating composition of claim 1 , wherein at least two of R 1 , R 2 , R 3 , and R 4 comprise at least twelve carbon atoms.

16. The aqueous coating composition of claim 1 , wherein at least three of R 1 , R 2 , R 3 , and R 4 comprise at least twelve carbon atoms.

17. The aqueous coating composition of claim 1 , wherein at least two of R 1 , R 2 , R 3 , and R 4 comprise at least eighteen carbon atoms.

18. The aqueous coating composition of claim 1 , wherein at least three of R 1 , R 2 , R 3 , and R 4 comprise at least eighteen carbon atoms.

19. The aqueous coating composition of claim 1 , wherein a ratio of ethoxy groups to propoxy groups is between 2:1 and 6:1.

Assignments (3)
CHANGE OF NAME Recorded Sep 18, 2019
From: AKZO NOBEL CHEMICALS INTERNATIONAL B.V.
To: NOURYON CHEMICALS INTERNATIONAL B.V.
Reel/Frame 050426/0671 →
SECURITY INTEREST Recorded Oct 1, 2018
From: STARFRUIT US MERGER SUB 1 LLC; STARFRUIT US MERGER SUB 2 LLC; AKZO NOBEL SURFACE CHEMISTRY LLC; AKZO NOBEL CHEMICALS B.V.; AKZO NOBEL CHEMICALS INTERNATIONAL B.V.
To: WILMINGTON TRUST (LONDON) LIMITED, AS COLLATERAL AGENT
Reel/Frame 047231/0001 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 13, 2017
From: YU, HUA; SHEN, LINGJUAN
To: AKZO NOBEL CHEMICALS INTERNATIONAL B.V.
Reel/Frame 042689/0162 →