Edging method and edging device

Inventors: Yoji Nakamura (Tokyo, JP); Toshiaki Saitoh (Tokyo, JP); Satoru Mashiko (Tokyo, JP); Tetsuo Kishimoto (Tokyo, JP); Akihisa Tsuruta (Tokyo, JP); Tatsuya Nakada (Tokyo, JP); Naoki Kataoka (Tokyo, JP)
Assignee: NIPPON STEEL CORPORATION
B21B37/22B21B1/02B21B1/024B21B15/00B21B39/14B21B15/0035B21B37/68B21B39/16B21B2261/06B21B2261/21B21B2263/12
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,799,925
App. No.
15/542,206
Granted
Oct 13, 2020
Kind
B2
Abstract

An edging method including changing an incident angle of a slab with respect to a pair of edging members that are disposed on a conveyance line of the slab and that edge the slab based on information relating to the slab acquired at at least one of prior to edging or after edging.

Claims (8)

1. An edging method comprising changing an incident angle of a slab having a width direction across its width with respect to a pair of edging units that are disposed on a conveyance line of the slab and that edge the slab based on information relating to the slab acquired at at least one of prior to edging or after edging, wherein:

the information includes

(i) a temperature distribution across the width direction of the slab prior to edging, or

(ii) a slab thickness variation across the width direction of the slab at at least one of prior to edging or after edging, or

(iii) a variation between coefficients of friction of both lateral faces of the slab, which are separated by the width direction of the slab, with respect to the edging units prior to edging; and

the incident angle of the slab is changed according to the temperature distribution, the slab thickness variation, or the variation between the coefficients of friction.

2. The edging method of claim 1 , wherein the incident angle of the slab is also changed based on, in addition to the information, at least one of a dimension of the slab, an edging amount of the slab, or a type of steel of the slab.

3. The edging method of claim 1 , wherein the incident angle is changed by contacting a moving member capable of moving in the width direction of the slab against a lateral face in the width direction of the slab further upstream than the pair of edging units on the conveyance line.

Assignments (2)
CHANGE OF NAME Recorded May 14, 2019
From: NIPPON STEEL & SUMITOMO METAL CORPORATION
To: NIPPON STEEL CORPORATION
Reel/Frame 049257/0828 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 7, 2017
From: NAKAMURA, YOJI; SAITOH, TOSHIAKI; MASHIKO, SATORU; KISHIMOTO, TETSUO; TSURUTA, AKIHISA; NAKADA, TATSUYA; KATAOKA, NAOKI
To: NIPPON STEEL & SUMITOMO METAL CORPORATION
Reel/Frame 042933/0574 →