Inducibly degradable polyacetal compositions for use in subterranean formations

Inventors: Robert Lawrence Blackbourn (Houston, TX); Paul Richard Weider (Houston, TX); Jonathan Joseph Brege (Spring, TX); Allen Dale Gabrysch (Paige, TX); Ryan Matthew Van Zanten (Katy, TX)
Assignee: SHELL OIL COMPANY
C09K8/035C09K8/50C09K8/62
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,894,909
App. No.
15/573,034
Granted
Jan 19, 2021
Kind
B2
Abstract

Inducibly degradable compositions comprising polyacetal and associated methods and systems.

Claims (27)

1. A method comprising:

placing a sand control screen in a wellbore penetrating a subterranean formation, the sand control screen comprising an inducibly degradable composition comprising polyacetal; and

activating an autocatalytic degradation of the polyacetal, the activating comprising contacting the sand screen with an inducer to form an alpha hydroxy sulfonic acid, the inducer comprising at least one of a sulfur dioxide and a sulfur dioxide precursor, wherein the inducer further comprises at least one of a strong acid, a halide, and a brine.

2. The method of claim 1 , wherein the subterranean formation has a temperature in a range of from 120° F. to 320° F.

3. The method of claim 1 , wherein the polyacetal has a crystallinity in the range of from 75% to 85%.

4. The method of claim 1 , wherein the polyacetal is a co-polymer of trioxane and ethylene oxide.

5. The method of claim 1 , wherein the inducibly degradable composition is a solid.

6. The method of claim 1 , wherein the inducibly degradable composition is a coating on the sand control screen.

7. The method of claim 1 , wherein the inducibly degradable composition further comprises at least one of: a strong acid and a halide.

8. The method of claim 1 , wherein the sulfur dioxide or sulfur dioxide precursor is generated in the wellbore.

9. The method of claim 1 , wherein the inducibly degradable composition further comprises formaldehyde.

10. The method of claim 1 , wherein the inducer includes at least said brine.

11. The method of claim 10 , wherein the brine comprises one or more of KCl, ZnBr 2 , CaBr 2 , and CaCl 2 .

12. The method of claim 1 , wherein the inducer includes at least said halide.

13. The method of claim 1 , wherein the inducer includes at least said strong acid.

14. A method comprising: inducing an autocatalytic degradation of an inducibly degradable composition comprising polyacetal, wherein the inducing is performed in a wellbore that penetrates a subterranean earth formation and the inducibly degradable composition is a solid,

wherein inducing degradation comprises contacting the inducibly degradable composition with an inducer to form an alpha hydroxy sulfonic acid, the inducer comprising at least one of a sulfur dioxide and a sulfur dioxide precursor, wherein the inducer further comprises at least one of a strong acid, a halide, and a brine.

15. The method of claim 14 , wherein the solid is a sand control screen, a liner, a gasket, a ball sealer, a flow diverter, a flapper valve, or a plug.

16. The method of claim 15 , wherein the solid comprises a sulfur dioxide precursor.

17. The method of claim 14 , wherein the inducibly degradable composition further comprises formaldehyde.

18. The method of claim 14 , wherein the inducer includes at least said brine.

19. The method of claim 18 , wherein the brine comprises one or more of KCl, ZnBr 2 , CaBr 2 , and CaCl 2 .

20. The method of claim 14 , wherein the inducer includes at least said halide.

21. The method of claim 14 , wherein the inducer includes at least said strong acid.

22. The method of claim 16 , wherein the polyacetal has a crystallinity in the range of from 75% to 85%.

23. The method of claim 16 , wherein the polyacetal is a co-polymer of trioxane and ethylene oxide.

24. The method of claim 16 , wherein the polyacetal is a coating on a surface of the solid.

Assignments (2)
CHANGE OF NAME Recorded Mar 7, 2022
From: SHELL OIL COMPANY
To: SHELL USA, INC.
Reel/Frame 059694/0819 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 2, 2020
From: BLACKBOURN, ROBERT LAWRENCE; WEIDER, PAUL RICHARD; BREGE, JONATHAN JOSEPH; GABRYSCH, ALLEN DALE; VAN ZANTEN, RYAN MATTHEW
To: SHELL OIL COMPANY
Reel/Frame 053673/0488 →
Continuity (2)
Provisional Application 62160194 · May 12, 2015
Related Publication 20180105730A1 · Apr 19, 2018