IP Library Granted Patent US 10,239,764
Granted Patent B2
US 10,239,764 · App. 15/577,507 · Granted Mar 26, 2019

Aqueous cobalt chloride solution purification method

Inventors: Toshirou Tan (Niihama, JP); Masatoshi Takano (Niihama, JP); Hideki Ohara (Niihama, JP); Satoshi Asano (Niihama, JP)
Assignee: SUMITOMO METAL MINING CO., LTD.
C01G51/085C22B3/46C22B23/00C22B23/0469C22B23/06H01M4/525H01M2004/028Y02P10/234
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,239,764
App. No.
15/577,507
Granted
Mar 26, 2019
Kind
B2
Abstract

An aqueous cobalt chloride solution purification method, in which impurities can be efficiently removed from a cobalt salt solution, includes bringing metallic nickel into contact with an aqueous solution containing cobalt chloride to remove an impurity by a substitution reaction, in which the pH of the aqueous solution containing cobalt chloride is adjusted to not less than 1.5 and not more than 2.5. Since the pH of the aqueous solution containing cobalt chloride is adjusted to not less than 1.5 and not more than 2.5, a passive film on a surface of the metallic nickel can be effectively removed, and the metallic nickel comes in contact with the aqueous solution containing cobalt chloride, so that an impurity more noble than the metallic nickel can be precipitated by the substitution reaction. The metallic nickel is only brought into contact with the aqueous solution containing cobalt chloride, and the impurity can be easily removed.

Claims (8)

1. An aqueous cobalt chloride solution purification method, comprising the step of:

bringing metallic nickel into contact with an aqueous solution containing cobalt chloride, thereby removing an impurity by a substitution reaction,

wherein a pH of the aqueous solution containing cobalt chloride is adjusted to not less than 1.5 and not more than 2.5.

2. The aqueous cobalt chloride solution purification method according to claim 1 , wherein a temperature of the aqueous solution containing cobalt chloride is maintained at higher than 50° C. and not higher than 80° C.

3. The aqueous cobalt chloride solution purification method according to claim 1 , wherein the impurity is copper.

4. The aqueous cobalt chloride solution purification method according to claim 1 , wherein the aqueous solution containing cobalt chloride from which the impurity has been removed is used as a raw material of a positive electrode material containing in the composition of the positive electrode material nickel and cobalt in a nonaqueous electrolyte secondary battery.

5. The aqueous cobalt chloride solution purification method according to claim 4 , wherein the aqueous solution containing cobalt chloride is a process liquid in a nickel smelting process.

6. The aqueous cobalt chloride solution purification method according to claim 2 , wherein a temperature of the aqueous solution containing cobalt chloride is maintained at not lower than 60° C. and not higher than 80° C.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 12, 2018
From: TAN, TOSHIROU; TAKANO, MASATOSHI; OHARA, HIDEKI; ASANO, SATOSHI
To: SUMITOMO METAL MINING CO., LTD.
Reel/Frame 045177/0817 →
Priority Claims (1)
JP 2015-110666 · May 29, 2015 · national
Continuity (1)
Related Publication 20180148344A1 · May 31, 2018