Electrolyte material, liquid composition and membrane/electrode assembly for polymer electrolyte fuel cell

Inventors: Satoru Hommura (Chiyoda-ku, JP); Susumu Saito (Chiyoda-ku, JP); Hiroyuki Watabe (Chiyoda-ku, JP)
Assignee: AGC Inc.
H01M8/1039C08F8/12C08F214/184C08J5/2237C08L29/10H01B1/06H01B1/122H01M4/926H01M8/02H01M8/10H01M8/1018C08J2327/14H01M2008/1095
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,879,551
App. No.
15/627,861
Granted
Dec 29, 2020
Kind
B2
Abstract

To provide a membrane/electrode assembly excellent in the power generation characteristics in a wide temperature range and a wide humidity range; an electrolyte material suitable for a catalyst layer of the membrane/electrode assembly; and a liquid composition suitable for forming a catalyst layer of the membrane/electrode assembly. To use an electrolyte material which is formed of a polymer (H) obtained by converting precursor groups in a polymer (F) having structural units (A) based on a perfluoromonomer having a precursor group represented by the formula (g1), structural units (B) represented by the formula (u2), and structural units (C) based on tetrafluoroethylene, wherein the proportion of the structural units (A) is from 8 to 19 mol %, the proportion of the structural units (B) is from 65 to 80 mol %, and the proportion of the structural units (C) is from 1 to 27 mol %, to ion exchange groups.

Claims (39)

1. An electrolyte material, comprising a polymer (H) prepared by converting one or more —SO 2 F groups in a polymer (F) to ion exchange groups by a treatment method selected from the group consisting of a hydrolysis treatment and an acid-form conversion treatment:

Polymer (F): a polymer consisting of:

structural units (A) represented by the following formula (u1),

structural units (B) represented by the following formula (u2),

structural units (C), which is tetrafluoroethylene, and

structural unit (D), which is optional, selected from the group consisting of chlorotrifluoroethylene, trifluoroethylene, vinylidene fluoride, vinyl fluoride, ethylene, propylene, perfluoro(3-butenyl vinyl ether), perfluoro(allyl vinyl ether), a perfluoro α-olefin, a (perfluoroalkyl)ethylene, a (perfluoroalkyl)propene, a perfluoro(alkyl vinyl ether), the following monomer (m3),

CF 2 ═CF(CF 2 ) s OCF 2 —CFZ-Q-SO 2 F  (m3)

wherein Q is a single bond or a perfluoroalkylene group which may have an etheric oxygen atom, Z is a fluorine atom or a monovalent perfluoro organic group, and s is 0 or 1,

wherein the proportion of the structural units (A) is from 8 to 19 mol %, the proportion of the structural units (B) is from 65 to 80 mol %, and the proportion of the structural units (C) is from 1 to 27 mol %, in 100 mol % of all structural units:

wherein:

Q 1 is a perfluoroalkylene group;

Q 2 is a single bond or a perfluoroalkylene group;

Y is a fluorine atom or a monovalent perfluoro organic group;

q is 0 or 1;

each of R 11 and R 12 which are independent of each other, is a fluorine atom or a C 1-5 perfluoroalkyl group; and

each of and R 13 and R 14 which are independent of each other, is a fluorine atom, a C 1-5 perfluoroalkyl group or a C 1-5 perfluoroalkoxy group,

wherein the following TQ value of the polymer (F) is from 255 to 300° C.:

TQ value: a temperature at which the extrusion rate becomes 100 mm 3 /sec, when the polymer (F) is subjected to melt-extrusion under an extrusion pressure condition of 2.94 MPa from a nozzle having a length of 1 mm and an inner diameter of 1 mm.

2. The electrolyte material according to claim 1 , wherein the proportion of the structural units (A) is from 13 to 18 mol %, the proportion of the structural units (B) is from 67 to 78 mol %, and the proportion of the structural units (C) is from 4 to 20 mol %, in 100 mol % of all structural units constituting the polymer (F).

3. The electrolyte material according to claim 1 , wherein the TQ value of the polymer (F) is from 260 to 290° C.

4. The electrolyte material according to claim 1 , wherein the ion exchange capacity of the polymer (H) is from 0.7 to 1.29 meq/g dry resin.

5. The electrolyte material according to claim 1 , wherein at least one type of structural units (A′) obtained by converting precursor groups of the structural units (A) to ion exchange groups is structural units represented by the following formula (u′1):

wherein:

R f is a perfluoroalkyl group;

X is an oxygen atom, a nitrogen atom or a carbon atom, such that a=0 when X is an oxygen atom, a=1 when X is a nitrogen atom, and a=2 when X is a carbon atom; and

q is 0 or 1.

6. The electrolyte material according to claim 1 , wherein each of Q 1 and Q 2 which are independent of each other, is a C 1-6 perfluoroalkylene group.

7. The electrolyte material according to claim 6 , wherein at least one of Q 1 and Q 2 is a C 1-6 perfluoroalkylene group having an etheric oxygen atom.

8. The electrolyte material according to claim 1 , wherein at least one type of the structural units (B) is structural units represented by the following formula (u2-1):

9. A liquid composition, comprising a dispersion medium and the electrolyte material as defined in claim 1 , dispersed in the dispersion medium, wherein the dispersion medium comprises contains an organic solvent having a hydroxy group.

10. The liquid composition according to claim 9 , comprising from 1 to 50 mass % of the electrolyte material.

11. A catalyst layer in an electrode of a membrane/electrode assembly for a polymer electrolyte fuel cell, the catalyst layer comprising a proton conductive polymer formed of the electrolyte material of claim 1 .

12. A membrane/electrode assembly for a polymer electrolyte fuel cell, the membrane/electrode assembly comprising an anode having a catalyst layer containing a proton conductive polymer, a cathode having a catalyst layer containing a proton conductive polymer, and a polymer electrolyte membrane disposed between the anode and the cathode,

wherein the proton conductive polymer contained in the catalyst layer of at least one of the cathode and the anode is the electrolyte material of claim 1 .

13. The electrolyte material according to claim 1 , wherein Q 1 is a perfluoroalkylene group which comprises an etheric oxygen atom.

14. The electrolyte material according to claim 1 , wherein Q 2 is a single bond.

15. The electrolyte material according to claim 1 , wherein Q 2 is a perfluoroalkylene group.

16. The electrolyte material according to claim 14 , wherein said perfluoroalkylene group comprises an etheric oxygen atom.

17. The electrolyte material according to claim 5 , wherein R f is a perfluoroalkylene group which comprises an etheric oxygen atom.

Assignments (2)
CHANGE OF NAME Recorded Aug 7, 2018
From: ASAHI GLASS COMPANY, LIMITED
To: AGC INC.
Reel/Frame 046730/0786 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 20, 2017
From: HOMMURA, SATORU; SAITO, SUSUMU; WATABE, HIROYUKI
To: ASAHI GLASS COMPANY, LIMITED
Reel/Frame 042757/0963 →
Priority Claims (1)
JP 2014-262600 · Dec 25, 2014 · national
Continuity (2)
Continuation PCTJP2015085561 · Dec 18, 2015
Related Publication 20170288249A1 · Oct 5, 2017