Sealant material

Inventors: Anna Prell (Heidelberg, DE); Eadaoin Ledwidge (Dublin, DE)
Assignee: Henkel IP & Holding GmbH
C09K3/1028C09D5/34C09K3/10C09K2200/0447C09K2200/0695D06M13/144F16L15/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,066,587
App. No.
15/643,796
Granted
Jul 20, 2021
Kind
B2
Abstract

Use of a sealing material which is a multifilament or spun yarn coated with a joint sealing composition to seal a joint in a pipe system in which system a fluid having corrosion inhibitors such as diammonium dimolybdate or benzotriazole; and/or sludge removers; and/or an alcohol such as propane diol, or ethylene glycol; and/or a hydrocarbon such as diesel, including biodiesel, fuel oil, or hydraulic oil; and/or steam at a temperature of at least 180° C. and a pressure of at least 10 bar (1000 kPa); is to be passed through the sealed joint. It is surprising that the sealing materials of the invention can maintain a sealed joint despite exposure to such materials.

Claims (29)

1. A process for using a sealing material consisting of a plurality of yarns coated with a non-curable joint sealing composition to seal a joint in a pipe system, comprising the steps of:

applying the sealing material to a surface of the joint and mating the sealing material-applied surface of the joint with another part to form the pipe system, and thereafter passing through the pipe system a fluid, wherein the fluid comprises at least two of:

(a) corrosion inhibitor selected from the group consisting of diammonium dimolybdate and benzotriazole;

(b) sludge remover;

(c) alcohol selected from the group consisting of propane diol and ethylene glycol;

(d) hydrocarbon selected from the group consisting of diesel, fuel oil and hydraulic oil; or

(e) steam at a temperature of at least 180° C. and a pressure of at least 10 bar (1000 kPa),

wherein the plurality of yarns is constructed from polyamide, and

wherein the non-curable joint sealing composition comprises silicone oil and a filler selected from the group consisting of a mineral filler, a powdered polymer filler and chopped fibre filler material.

2. The process according to claim 1 wherein the fluid is at an elevated temperature.

3. The process according to claim 2 wherein the elevated temperature is at least about 150° C.

4. The process of claim 1 wherein the yarn is a multifilament yarn or a spun yarn.

5. A process for using a plurality of yarns together with a non-curable joint sealing composition in the manufacture of a sealing material for sealing a joint in a pipe system, comprising the steps of:

applying the sealing material to a joint and mating the sealing material-applied joint with another part to form a pipe system, and thereafter passing through the pipe system a fluid, wherein the fluid comprises at least two of:

(a) corrosion inhibitor selected from the group consisting of diammonium dimolybdate and benzotriazole;

(b) sludge remover;

(c) alcohol selected from the group consisting of propane diol and ethylene glycol;

(d) hydrocarbon selected from the group consisting of diesel, fuel oil and hydraulic oil; or

(e) steam at a temperature of at least 180° C. and a pressure of at least 10 bar (1000 kPa),

wherein the plurality of yarns are constructed from polyamide, and

wherein the non-curable joint sealing composition comprises silicone oil and a filler selected from the group consisting of a mineral filler, a powdered polymer filler and chopped fibre filler material.

6. A system through which a fluid passes, wherein the system comprises a pipe system in which there is at least one joint, the joint being sealed with a sealing material comprising a plurality of yarns coated with a non-curable joint sealing composition, and a fluid passing through the sealed joint, the fluid comprising at least two of:

(a) corrosion inhibitor selected from the group consisting of diammonium dimolybdate and benzotriazole;

(b) sludge remover;

(c) alcohol selected from the group consisting of propane diol and ethylene glycol;

(d) hydrocarbon selected from the group consisting of diesel, fuel oil and hydraulic oil; or

(e) steam at a temperature of at least 180° C. and a pressure of at least 10 bar (1000 kPa),

wherein the yarn is constructed from polyamide, and

wherein the non-curable joint sealing composition comprises silicone oil and a filler selected from the group consisting of a mineral filler, a powdered polymer filler and chopped fibre filler material.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 9, 2022
From: HENKEL IP & HOLDING GMBH
To: HENKEL AG & CO. KGAA
Reel/Frame 059357/0267 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 14, 2021
From: PRELL, ANNA; LEDWIDGE, EADAOIN
To: HENKEL IRELAND OPERATIONS & RESEARCH LIMITED
Reel/Frame 056531/0031 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 14, 2021
From: HENKEL IRELAND OPERATIONS & RESEARCH LIMITED
To: HENKEL IP & HOLDING GMBH
Reel/Frame 056531/0097 →
Priority Claims (1)
GB 1500754 · Jan 16, 2015 · national
Continuity (2)
Continuation PCTEP2015080683 · Dec 18, 2015
Related Publication 20170306203A1 · Oct 26, 2017