IP Library Granted Patent US 10,688,737
Granted Patent B2
US 10,688,737 · App. 15/704,073 · Granted Jun 23, 2020

Method for forming fiber-reinforced polymer components

Inventor: Bensely Albert (Greenville, SC)
Assignee: General Electric Company
B29C70/543B29B15/122B29C35/0805B29C64/165B29C70/38B29C70/382B29C70/541B29D99/0025B29D99/0028B33Y10/00B33Y80/00B29B15/125B29C70/16B29C70/546B29C2035/0827B29K2105/0058B29L2031/085B33Y30/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,688,737
App. No.
15/704,073
Granted
Jun 23, 2020
Kind
B2
Abstract

The present disclosure is directed to a method for forming a fiber-reinforced polymer component. The method includes impregnating a first fiber tow with a polymerizable liquid contained within a reservoir to form a first impregnated fiber tow. The method also includes positioning the first impregnated fiber tow within a build region of the reservoir. The build region has a shape and size corresponding to a cross-sectional shape of the fiber-reinforced polymer component. Furthermore, the method includes irradiating the build region of the reservoir to form a polymerized solid from the polymerizable liquid within the build region. The polymerized solid encases a portion of the first fiber tow to form at least a portion of the fiber-reinforced polymer component.

Claims (32)

1. A method for forming a fiber-reinforced polymer component, the method comprising:

impregnating a first fiber tow with a polymerizable liquid contained within a reservoir to form a first impregnated fiber tow;

positioning the first impregnated fiber tow within a build region of the reservoir, the build region having a shape and size corresponding to a cross-section of the fiber-reinforced polymer component;

irradiating the build region of the reservoir to form a polymerized solid from the polymerizable liquid within the build region, the polymerized solid encasing a portion of the first fiber tow to form at least a portion of the fiber-reinforced polymer component; and,

adjusting at least one of a shape, a size, or a position of the build region as the cross-section of the fiber-reinforced polymer component changes.

2. The method of claim 1 , further comprising:

adjusting a position of the first fiber tow as the cross-section of the fiber-reinforced polymer component changes.

3. The method of claim 2 , wherein adjusting the position of the first fiber tow comprises adjusting the position of the first fiber tow with a guide tool positioned within a dead zone of the reservoir, the dead zone being positioned between a bottom wall of the reservoir and the build region, the dead zone containing oxygen for preventing polymerization of the polymerizable liquid.

4. The method of claim 1 , further comprising:

impregnating a second fiber tow with the polymerizable liquid contained within the reservoir to form a second impregnated fiber tow; and,

positioning the second impregnated fiber tow within the build region of the reservoir, the second impregnated fiber tow being position in a different portion of the build region than the first fiber tow.

5. The method of claim 1 , further comprising:

supplying oxygen to the reservoir through an oxygen-permeable portion of the reservoir to create a dead zone within the reservoir, the dead zone being positioned between a bottom wall of the reservoir and the build region, the oxygen preventing polymerization of the polymerizable liquid.

6. The method of claim 1 , wherein irradiating the build region comprises directing radiation into the build region of the reservoir with a mirror.

7. The method of claim 1 , wherein the polymerized solid is coupled to a build plate.

8. The method of claim 7 , further comprising:

continuously moving the build plate away from the build region as the build region is irradiated.

9. The method of claim 1 , wherein irradiating the build region comprises irradiating the build region with ultraviolet radiation.

10. The method of claim 1 , wherein the fiber-reinforced polymer component is a continuous fiber-reinforced polymer component.

11. The method of claim 1 , wherein the first fiber tow comprises a plurality of carbon or glass fibers.

12. The method of claim 1 , wherein the fiber-reinforced polymer component is a wind turbine component.

13. The method of claim 12 , wherein the wind turbine component is a shear web.

14. A method for forming a lattice portion of a continuous fiber-reinforced polymeric wind turbine component, the method comprising:

impregnating first and second fiber tows with a polymerizable liquid contained within a reservoir to form first and second impregnated fiber tows;

positioning the first and second impregnated fiber tows within a build region of the reservoir, the first fiber tow being positioned at a different location within the build region than the second fiber tow, the build region having a shape and size corresponding to a cross-section of the lattice portion of the fiber-reinforced polymeric wind turbine component;

irradiating the build region of the reservoir to form a polymerized solid from the polymerizable liquid within the build region, the polymerized solid being coupled to a build plate, the polymerized solid encasing a portion of the first and second fiber tows to form at least a portion of the lattice portion of the fiber-reinforced polymeric wind turbine component;

continuously moving the build plate away from the build region when the build region is irradiated; and,

adjusting at least one of a shape or a size of the build region when the cross-section of the lattice portion of the fiber-reinforced polymeric wind turbine being forced changes.

15. The method of claim 14 , further comprising:

adjusting the positions of the first and second fiber tows as the cross-section of the continuous fiber-reinforced polymeric wind turbine component changes.

16. The method of claim 15 , wherein adjusting the position of the first and second fiber tows comprises adjusting the position of the first fiber tow with a first guide tool and adjusting the position of the second fiber tow with a second guide tool, the first and second guide tools being positioned within a dead zone of the reservoir, the dead zone being positioned between a bottom wall of the reservoir and the build region, the dead zone containing oxygen for preventing polymerization of the polymerizable liquid.

17. The method of claim 14 , wherein the continuous fiber-reinforced polymeric wind turbine component is a shear web.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 22, 2024
From: LM WIND POWER US TECHNOLOGY APS
To: GE INFRASTRUCTURE TECHNOLOGY LLC
Reel/Frame 066869/0770 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 9, 2023
From: GENERAL ELECTRIC COMPANY
To: LM WIND POWER US TECHNOLOGY APS
Reel/Frame 065531/0160 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 14, 2017
From: ALBERT, BENSELY
To: GENERAL ELECTRIC COMPANY
Reel/Frame 043585/0163 →
Continuity (1)
Related Publication 20190077096A1 · Mar 14, 2019