Electrode, method for manufacturing the electrode, and roller for manufacturing the electrode

Inventors: Sang Kyun Lee (Daejeon, KR); Seok Jin Kim (Daejeon, KR); Cha Hun Ku (Daejeon, KR)
H01M4/0435H01M4/0404H01M4/13H01M4/139
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,196,031
App. No.
15/757,886
Granted
Dec 7, 2021
Kind
B2
Abstract

The present invention relates to an electrode, for reducing a difference in ductility between a non-coating portion and a coating portion of the electrode, a method for manufacturing the electrode, and a roller for manufacturing the electrode. Also, the electrode according to the present invention includes an electrode foil, a coating portion coated with an electrode active material on one surface of the electrode foil, and a non-coating portion which is disposed adjacent to the coating portion on the one surface of the electrode foil, and is not coated with the electrode active material and on which a pattern is disposed.

Claims (5)

1. An electrode comprising:

an electrode foil;

a coating portion coated with an electrode active material on one surface of the electrode foil; and

a non-coating portion which is disposed adjacent to the coating portion on the one surface of the electrode foil and is not coated with the electrode active material and on which a pattern is disposed, the non-coating portion of the electrode foil having a first thickness outside of the pattern, the pattern extending on the one surface of the electrode foil only partially through a thickness of the electrode such that the pattern of the non-coating portion has a second thickness less than the first thickness, the pattern providing the non-coating portion with a first ductility that is greater than a second ductility of the coating portion, the coating portion and the non-coating portion on which the pattern is disposed having structural evidence of being subjected to working by rolling by simultaneous application of a pressure to the entirety of the coating portion and the non-coating portion by a roller rolling over the coating portion and the non-coating portion during formation of the pattern,

wherein the pattern has a plurality of concave grooves repeatedly arranged, the pattern having a strip shape in which the plurality of concave grooves extend perpendicularly from a peripheral edge of the coating portion, the pattern of the non-coating portion having structural evidence of being formed through punching or partially cutting the non-coating portion.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2021
From: LG CHEM, LTD.
To: LG ENERGY SOLUTION, LTD.
Reel/Frame 058295/0068 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 8, 2018
From: LEE, SANG KYUN; KIM, SEOK JIN; KU, CHA HUN
To: LG CHEM, LTD.
Reel/Frame 045142/0874 →