IP Library Granted Patent US 11,274,063
Granted Patent B2
US 11,274,063 · App. 15/889,612 · Granted Mar 15, 2022

Glass plate with antifouling layer

Inventor: Kensuke Fujii (Chiyoda-ku, JP)
Assignee: AGC Inc.
C03C17/42B32B7/12C03C3/085C03C15/00C03C21/002C03C2217/213C03C2217/732C03C2217/734C03C2217/76C03C2218/119C03C2218/154C03C2218/34C03C2218/365G02B1/18
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,274,063
App. No.
15/889,612
Granted
Mar 15, 2022
Kind
B2
Abstract

A glass plate with an antifouling layer, including: a glass plate having a first principal surface, a second principal surface opposite to the first principal surface, and an end face connecting the first principal surface and the second principal surface; an adhesive layer formed from the first principal surface to the end face of the glass plate; and an antifouling layer formed on the adhesive layer.

Claims (46)

1. A glass plate with an antifouling layer, comprising:

a glass plate having a first principal surface, a second principal surface opposite to the first principal surface, and an end face connecting the first principal surface and the second principal surface;

a printed layer formed on a periphery of the second principal surface of the glass plate;

an adhesive layer formed on the first principal surface of the glass plate, the end face of the glass plate, and the printed layer, where the adhesive layer is a low-reflection film having an uppermost layer comprising silicon oxide; and

an antifouling layer formed on the adhesive layer,

wherein the adhesive layer and the antifouling layer are formed on the printed layer such that the adhesive layer and the antifouling layer exist outside an inner periphery of the printed layer and inside an outer periphery of the printed layer.

2. The glass plate with the antifouling layer according to claim 1 , wherein

the printed layer is continuously formed on the periphery of the second principal surface of the glass plate.

3. The glass plate with the antifouling layer according to claim 1 , wherein

the adhesive layer and the antifouling layer are formed on the printed layer such that the antifouling layer forms an outermost surface on a side of the second principal surface of the glass plate.

4. The glass plate with the antifouling layer according to claim 1 , wherein

the antifouling layer comprises a fluorine-containing organic group.

5. The glass plate with the antifouling layer according to claim 1 , wherein

the antifouling layer is formed of a cured matter of a film-forming composition comprising a fluorine-containing hydrolyzable silicon compound.

6. The glass plate with the antifouling layer according to claim 1 , wherein

the glass plate is a chemically tempered glass plate.

7. The glass plate with the antifouling layer according to claim 1 , wherein

the first principal surface of the glass plate has a projecting and recessed shape.

8. The glass plate with the antifouling layer according to claim 7 , wherein

the first principal surface of the glass plate has the projecting and recessed shape such that the glass plate has antiglare property.

9. The glass plate with the antifouling layer according to claim 1 , wherein

each of the adhesive layer and the antifouling layer is uniformly formed on the first principal surface of the glass plate.

10. The glass plate with the antifouling layer according to claim 1 , wherein

the low-reflection film comprises alternately laminated high-refractive-index layers having refractive index at a wavelength of 550 nm of 1.9 or more and low-refractive-index layers having refractive index at a wavelength of 550 nm of 1.6 or less.

11. The glass plate with the antifouling layer according to claim 10 , wherein

the high-refractive-index layers comprise at least one selected from the group consisting of niobium oxide (Nb 2 O 5 ) titanium oxide (TiO 2 ), zirconium oxide (ZrO 2 ), tantalum oxide (Ta 2 O 5 ), and silicon nitride (SiN), and

the low-refractive-index layers comprise at least one selected from the group consisting of silicon oxide (SiO 2 ), a material containing a mixed oxide of Si and Sn, a material containing a mixed oxide of Si and Zr, and a material containing a mixed oxide of Si and Al.

12. The glass plate with the antifouling layer according to claim 8 , wherein

the first principal surface of the glass plate has a surface roughness RMS of 0.01 μm or more and 0.5 μm or less.

13. The glass plate with the antifouling layer according to claim 1 , wherein

the glass plate has a thickness of 0.5 mm or more and 3 mm or less.

14. The glass plate with the antifouling layer according to claim 8 , wherein

the projecting and recessed shape is formed by frost treatment.

15. The glass plate with the antifouling layer according to claim 4 , wherein

the antifouling layer has a thickness of 2 nm or more and 20 nm or less.

16. The glass plate with the antifouling layer according to claim 4 , wherein

the fluorine-containing organic group is at least one selected from the group consisting of a perfluoropolyether group, a perfluoroalkylene group, and a perfluoroalkyl group.

17. A display device, comprising:

the glass plate with the antifouling layer according to claim 1 .

18. The display device according to claim 17 , wherein

the glass plate with the antifouling layer is disposed on a display part of the display device such that the second principal surface of the glass plate faces the display part.

19. The display device according to claim 18 , wherein

the glass plate with the antifouling layer is bonded to the display part of the display device by an adhesive material, and

the adhesive material is disposed on the printed layer.

20. A display device, comprising:

the glass plate with the antifouling layer according to claim 2 .

Assignments (2)
CHANGE OF NAME Recorded Aug 7, 2018
From: ASAHI GLASS COMPANY, LIMITED
To: AGC INC.
Reel/Frame 046730/0786 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 6, 2018
From: FUJII, KENSUKE
To: ASAHI GLASS COMPANY, LIMITED
Reel/Frame 044843/0104 →
Priority Claims (1)
JP JP2015-158418 · Aug 10, 2015 · national
Continuity (2)
Continuation PCTJP2016072555 · Aug 1, 2016
Related Publication 20180162771A1 · Jun 14, 2018