System and process for recovery of lithium from a geothermal brine

Inventors: John L. Featherstone (El Centro, CA); Paul J. Hanson (Imperial, CA); Michael J. Garska (Calipatria, CA); Charles R. Marston (Midland, MI)
Assignee: ENERGYSOURCE MINERALS LLC
C01D15/04B01D15/361C01D15/02C01D15/08
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,604,414
App. No.
16/010,286
Granted
Mar 31, 2020
Kind
B2
Abstract

This invention relates generally to a system and process for recovery of select minerals and lithium from a geothermal brine. The system and process are configured for the sequential recovery of zinc, manganese, and lithium from a Salton Sea Known Geothermal Resource Area brine. The system and process includes: 1) an impurity removal circuit; then 2) a continuous counter-current ion exchange (CCIX) circuit for selectively recovering lithium chloride from the brine flow and concentrating it using a CCIX unit; and then 3) a lithium chloride conversion circuit for converting lithium chloride to lithium carbonate or lithium hydroxide product.

Claims (79)

1. A process for recovery of lithium from a geothermal brine, said process comprising the steps of:

a. selectively removing impurities from said geothermal brine to form a polished brine;

b. then, selectively recovering lithium chloride from said polished brine and concentrating said lithium chloride using a continuous counter-current ion exchange to form a lithium chloride solution; said step b. of selectively recovering lithium chloride further comprises sequentially introducing said polished brine into individual process zones of said continuous counter-current ion exchange for a predetermined contact time, said continuous counter-current ion exchange comprises a plurality of ion exchange beds or columns containing a lithium selective adsorbent, said process zones configured in parallel, in series, or in combinations of parallel and series, flowing either in up flow or down flow modes; and

c. then, selectively converting said lithium chloride in said lithium chloride solution to lithium carbonate, lithium hydroxide, or both.

2. The process of claim 1 wherein said geothermal brine is a Salton Sea Known Geothermal Resource Area brine.

3. The process of claim 1 wherein said step a. of selectively removing impurities from said brine comprises the steps of:

a. selectively removing iron and silica from said geothermal brine using oxidation and co-precipitation to form a substantially iron and silica free brine; and

b. then, selectively removing manganese and zinc from said substantially iron and silica free brine using precipitation to form said polished brine.

4. The process of claim 3 further comprising the steps of:

producing a manganese and zinc-rich filter cake from said polished brine; and then

selectively recovering manganese from said filter cake using solvent extraction to form a concentrated manganese sulfate product liquor; and/or

selectively recovering zinc from said filter cake using solvent extraction to form a concentrated zinc sulfate product liquor.

5. The process of claim 1 wherein fluid flow through said continuous counter-current ion exchange is controlled by pumping flow rates and a predetermined timing of a rotating or indexing manifold valve system, wherein said exchange beds continually cycle through said individual process zones.

6. The process of claim 1 wherein said step c. of selectively converting said lithium chloride further comprises the steps of:

selectively converting said lithium chloride in said lithium chloride solution to lithium carbonate using a two-stage lithium carbonate crystallization process; and/or

selectively concentrating said lithium chloride in said lithium chloride solution using a solvent extraction process, and then, selectively converting said lithium chloride in said lithium chloride solution to lithium hydroxide using electrolysis or chemical conversion.

7. The process of claim 6 further comprising the steps of:

selectively recovering said lithium carbonate from said two-stage lithium carbonate crystallization process; and then

selectively converting said lithium carbonate to said lithium hydroxide.

8. The process of claim 6 further comprising the steps of:

selectively removing calcium, magnesium and/or boron from said lithium chloride solution to form a substantially calcium, magnesium and/or boron free brine.

9. The process of claim 8 wherein said step of selectively removing calcium, magnesium and/or boron from said lithium chloride solution further comprises the steps of:

selectively removing calcium and magnesium from said lithium chloride solution using precipitation to form a substantially calcium and magnesium free brine;

selectively removing boron from substantially calcium and magnesium free brine using a boron ion exchange circuit and/or solvent extraction to form said substantially calcium, magnesium and/or boron free brine; and

selectively removing any remaining divalent ions from said substantially calcium, magnesium and/or boron free brine using a divalent ion exchange circuit.

10. A process for recovery of lithium from a brine, said process comprising the steps of:

a. optionally, removing an impurity from said brine to form a polished brine;

b. concentrating said lithium chloride in said brine using a continuous counter-current lithium extraction unit to form a lithium chloride solution, said continuous counter-current lithium extraction unit comprising a plurality of adsorption zones, each of said adsorption zones comprising an adsorbent bed or column, and at least one of said adsorption zones comprising a lithium selective adsorbent, said adsorption zones being configured in parallel, in series, or in combinations of parallel and series, flowing either in up flow or down flow modes;

c. converting said lithium chloride in said lithium chloride solution to lithium carbonate, lithium hydroxide, or both; and

d. recovering said lithium carbonate, said lithium hydroxide, or both.

11. The process of claim 10 further comprising the step of obtaining said brine and/or said polished brine, and wherein said brine and/or said polished brine comprise a geothermal brine containing lithium chloride.

12. The process of claim 10 further comprising the step of providing said brine and/or said polished brine, and wherein said brine and/or said polished brine comprise a geothermal brine containing lithium chloride.

13. The process of claim 10 further comprising the steps of:

a. selectively removing iron and silica from said brine using oxidation and co-precipitation to form a substantially iron and silica free brine; and

b. then, selectively removing manganese and zinc from said substantially iron and silica free brine using precipitation to form a polished brine.

14. The process of claim 13 further comprising the steps of:

selectively recovering manganese from said polished brine using solvent extraction to form a concentrated manganese sulfate product liquor; and/or

selectively recovering zinc from said polished brine using solvent extraction to form a concentrated zinc sulfate product liquor.

15. The process of claim 10 wherein fluid flow through said continuous counter-current ion exchange lithium extraction unit is controlled by pumping flow rates and a predetermined timing of a rotating or indexing manifold valve system, wherein said adsorbent beds continually cycle through said adsorption zones.

16. The process of claim 10 wherein said step c. of converting said lithium chloride further comprises the steps of:

selectively converting said lithium chloride in said lithium chloride solution to lithium carbonate using a two-stage lithium carbonate crystallization process; and/or

selectively concentrating said lithium chloride in said lithium chloride solution using a solvent extraction processes, and then, selectively converting said lithium chloride in said lithium chloride solution to lithium hydroxide using electrolysis or chemical conversion.

17. The process of claim 16 further comprising the steps of:

selectively recovering said lithium carbonate from said two-stage lithium carbonate crystallization process; and then

selectively converting said lithium carbonate to said lithium hydroxide.

18. The process of claim 16 further comprising the steps of:

selectively removing calcium, magnesium and/or boron from said lithium chloride solution to form a substantially calcium, magnesium and/or boron free brine.

19. The process of claim 18 wherein said step of selectively removing calcium, magnesium and/or boron from said lithium chloride solution further comprises the steps of:

selectively removing calcium and magnesium from said lithium chloride solution using precipitation to form a substantially calcium and magnesium free brine;

selectively removing boron from substantially calcium and magnesium free brine using a boron ion exchange circuit and/or solvent extraction to form said substantially calcium, magnesium and/or boron free brine; and

selectively removing any remaining divalent ions from said substantially calcium, magnesium and/or boron free brine using a divalent ion exchange circuit.

20. A process for selectively recovering lithium carbonate, lithium hydroxide, or both from a brine, said process comprising the steps of:

a. selectively removing an impurity from said brine to form a polished brine;

b. selectively recovering lithium chloride in said polished brine by sequentially concentrating said polished brine using a plurality of adsorption zones of a continuous counter-current ion exchange circuit to form a lithium chloride solution, said adsorption zones comprise a plurality of ion adsorbent beds or columns configured in parallel, in series, or in combinations of parallel and series, flowing either in up flow or down flow modes;

c. selectively converting said lithium chloride in said lithium chloride solution to said lithium carbonate, said lithium hydroxide, or both; and

d. selectively recovering said lithium carbonate, said lithium hydroxide, or both.

21. The process of claim 20 wherein at least one of said adsorption zones comprising a lithium selective adsorbent.

22. The process of claim 20 further comprising the step of obtaining said brine and/or said polished brine, and wherein said brine and/or said polished brine comprise a geothermal brine containing lithium chloride.

23. The process of claim 20 further comprising the step of providing said brine and/or said polished brine, and wherein said brine and/or said polished brine comprise a geothermal brine containing lithium chloride.

24. The process of claim 20 wherein said step a. of selectively removing said impurity comprises the steps of:

a. selectively removing iron and silica from said brine using oxidation and co-precipitation to form a substantially iron and silica free brine; and

b. then, selectively removing manganese and zinc from said substantially iron and silica free brine using precipitation to form said polished brine.

25. The process of claim 24 further comprising the steps of:

optionally, producing a manganese and zinc-rich filter cake from said polished brine; and then

selectively recovering manganese from said filter cake using solvent extraction to form a concentrated manganese sulfate product liquor; and/or

selectively recovering zinc from said filter cake using solvent extraction to form a concentrated zinc sulfate product liquor.

26. The process of claim 20 wherein fluid flow through said continuous counter-current ion exchange ion exchange circuit is controlled by pumping flow rates and a predetermined timing of a rotating or indexing manifold valve system, wherein said exchange beds continually cycle through said adsorption zones.

27. The process of claim 20 wherein said step c. of selectively converting said lithium chloride further comprises the steps of:

selectively converting said lithium chloride in said lithium chloride solution to lithium carbonate using a two-stage lithium carbonate crystallization process; and/or

selectively concentrating said lithium chloride in said lithium chloride solution using a solvent extraction process, and then selectively converting said lithium chloride in said lithium chloride solution to lithium hydroxide using electrolysis.

28. The process of claim 27 further comprising the steps of:

selectively recovering said lithium carbonate from said two-stage lithium carbonate crystallization process; and then

selectively converting said lithium carbonate to said lithium hydroxide.

29. The process of claim 27 further comprising the steps of:

selectively removing calcium, magnesium and/or boron from said lithium chloride solution to form a substantially calcium, magnesium and/or boron free brine.

30. The process of claim 29 wherein said step of selectively removing calcium, magnesium and/or boron from said lithium chloride solution further comprises the steps of:

selectively removing calcium and magnesium from said lithium chloride solution using precipitation to form a substantially calcium and magnesium free brine;

selectively removing boron from substantially calcium and magnesium free brine using a boron ion exchange circuit and/or solvent extraction to form said substantially calcium, magnesium and/or boron free brine; and

selectively removing any remaining divalent ions from said substantially calcium, magnesium and/or boron free brine using a divalent ion exchange circuit.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 10, 2024
From: ENERGYSOURCE MINERALS, LLC
To: ILIAD IP COMPANY, LLC
Reel/Frame 066086/0415 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 2, 2019
From: MARSTON, CHARLES R.
To: ENERGYSOURCE MINERALS LLC
Reel/Frame 049064/0335 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 6, 2018
From: FEATHERSTONE, JOHN L.; HANSON, PAUL J.; GARSKA, MICHAEL J.
To: ENERGYSOURCE MINERALS LLC
Reel/Frame 046280/0941 →
Continuity (3)
Provisional Application 62671489 · May 15, 2018
Provisional Application 62520024 · Jun 15, 2017
Related Publication 20190248667A1 · Aug 15, 2019
Cited By (11)
US 12,257,529 US 12,280,322 US 12,370,468 US 12,374,679 US 12,421,137 US 12,447,418 US 12,458,905 US 12,491,476 US 12,533,605 US 12,565,430 US 12,702,987