Wellbore composition
View Patent ↗The embodiments described herein generally relate to methods and chemical compositions for use with wellbore treatment processes. In one embodiment, a composition is provided comprising a mineral acid and a retardation agent selected from the group of an amine containing compound, an amide containing compound, lignosulfonate, and combinations thereof.
1. A composition, comprising:
from 5.0 to 28 wt % of a mineral acid; and
a retardation agent comprising:
an amine-containing resin; and
lignosulfonate; and
a viscosity modifier, wherein the amine-containing resin, comprises from 0.01 to 5.0 wt % of the composition.
2. The composition of claim 1 , wherein the composition further comprises water.
3. The composition of claim 1 , wherein the mineral acid is selected from the group consisting of hydrochloric acid, nitric acid, phosphoric acid, sulfuric acid, hydrofluoric acid, hydrobromic acid, perchloric acid, hydroiodic acid, and combinations thereof.
4. The composition of claim 1 , wherein the amine-containing resins are selected from the group consisting of urea-formaldehyde, urea-formaldehyde derivative, and combinations thereof.
5. The composition of claim 1 , wherein the composition further comprises an additive selected from the group consisting of a corrosion inhibitor, an anti-sludge agent, a chelating agent, an hydrogen sulfide scavenger, and combinations thereof.
6. The composition of claim 1 , wherein the lignosulfonate exerts a degree of sulfonation ranging from about 0.2 to about 5.0.
7. The composition of claim 1 , wherein the lignosulfonate comprises one or more cations selected from the group consisting of ammonium cations, lithium cations, sodium cations, potassium cations, silver cations, calcium cations, magnesium cations, zinc cations, iron cations, copper cations, cobalt cations, manganese cations, nickel cations, titanium cations, aluminum cations, and combinations thereof.
8. The composition of claim 4 , wherein the amine-containing resins are selected from the group consisting of urea-formaldehyde resin, melamine-formaldehyde resins, melamine-urea-formaldehyde resins, derivations thereof, and combinations thereof.
9. The composition of claim 1 , wherein the
mineral acid and
retardation agent
comprise a wt % ratio of mineral acid to retardation agent from 1:1 to 5:1.
10. The composition of claim 1 , wherein the composition comprises:
from 5.0 to 28 wt % hydrochloric acid;
from 0.01 to 5.0 wt % sulfuric acid;
from 0.01 to 5.0 wt % urea-formaldehyde, urea-formaldehyde derivative, or both;
from 0.01 to 20 wt % lignosulfonate; and
from 42 to 94.97 wt % water, wherein the amount of the components totals 100 wt. %.
11. The composition of claim 5 , wherein the composition comprises:
from about 0.01 to about 5.0 wt % of the additive selected from the group consisting of a corrosion inhibitor, an anti-sludge agent, a chelating agent, a hydrogen sulfide scavenger, and combinations thereof.
12. The composition of claim 5 , wherein the composition comprises:
from about 5.0 to about 28 wt % hydrochloric acid;
from about 0.01 to about 5.0 wt % sulfuric acid;
from about 0.01 to about 5.0 wt % urea-formaldehyde, urea-formaldehyde derivative, or both;
from about 0.01 to about 20 wt % lignosulfonate;
from about 0.01 to about 5.0 wt % viscosity modifier, a corrosion inhibitor, an anti-sludge agent, a chelating agent, a hydrogen sulfide scavenger, and combinations thereof; and
from about 37 to about 94.96 wt % water, wherein the amount of the components totals 100 wt. %.
13. The composition of claim 5 , wherein the composition comprises:
from 5.0 to 28 wt % hydrochloric acid;
from 0.01 to 5.0 wt % urea-formaldehyde, urea-formaldehyde derivative, or both;
from 0.01 to 20 wt % lignosulfonate;
from 0.01 to 5.0 wt % viscosity modifier; and
from 42 to 94.97 wt % water, wherein the amount of the components totals 100 wt. %.
14. The composition of claim 5 , wherein a composition comprises:
from 5.0 to 28 wt % hydrochloric acid;
from 0.01 to 5.0 wt % sulfuric acid;
from 0.01 to 20 wt % lignosulfonate;
from 0.01 to 5.0 wt % viscosity modifier; and
from 42 to 94.97 wt % water, wherein the amount of the components totals 100 wt. %.
15. The composition of claim 1 , wherein the retardation agent and the mineral acid comprise a molar ratio from about 0.1 to about 2.0.
16. A process for using a composition, comprising:
providing the composition of claim 1 ; and
depositing the composition downhole of a wellbore.
17. The process of claim 16 , wherein the composition comprises solid powders.
18. The process of claim 16 , wherein the composition comprises aqueous slurries.
19. The process of claim 16 , wherein the composition is pre-blended with concentrated mineral acid in an acid tank, a transportation vessel, a downhole flowline, or a combination thereof.
20. A process for using a composition, comprising:
providing the composition of claim 1 ; and
blending into an acidizing treatment fluid for the purpose of metal pickling.