IP Library Granted Patent US 11,059,213
Granted Patent B2
US 11,059,213 · App. 16/019,810 · Granted Jul 13, 2021

Method of blow molding a plastic container

Inventors: Eric B. Ungrady, III (Mt. Wolf, PA); Matthew A. Russell (Red Lion, PA); Hope Lee Townsend (Suwanee, GA); Michael L. James (Hamilton, OH)
Assignee: GRAHAM PACKAGING COMPANY, L.P.
B29C49/0078B29C33/3842B29C49/48B65D1/023B65D1/0207B65D1/0246B29C2049/4897B29K2067/003B29K2105/258B29L2031/7158B65D2255/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,059,213
App. No.
16/019,810
Granted
Jul 13, 2021
Kind
B2
Abstract

A plastic container has a main body portion, a neck portion and a molded feature such as an anti-rotation lug adjacent to the neck portion. The molded feature has a volume that is less than a volume that would be defined by the maximum external dimensions of the feature. This reduces the shrinkage differential between the molded feature and the neck portion, which could otherwise cause sealing problems with a closure as a result of deformation of the neck portion. A method of blow molding a plastic container with a reduced volume of the molded feature is also disclosed.

Claims (30)

1. A method of blow molding a plastic container, comprising:

disposing a molten plastic in a mold;

blow molding the molten plastic in the mold to form a blow molded article comprising a main body portion defining an interior space, a cylindrical neck portion having an opening that is in communication with the interior space, and a molded feature that is adjacent to the neck portion, the molded feature being configured to reduce ovalization of the neck portion, wherein the molded feature has a cavity defined therein so that the molded feature occupies a volume that is less than a volume defined by maximum external dimensions of the molded feature, the molded feature having a first portion that is integral with the neck portion and a second portion with a surface defining an opening into the cavity of the molded feature that faces in a direction that is substantially opposite from the neck portion to increase a surface area of the molded feature relative to what the surface area would have been if the molded feature were solid and without an opening; and

removing the blow molded article from the mold.

2. The method of a blow molding the plastic container according to claim 1 , wherein the volume of the molded feature is reduced by mold tooling.

3. The method of blow molding the plastic container according to claim 1 , wherein the molded feature comprises an anti-rotation lug.

4. The method of blow molding the plastic container according to claim 1 , wherein the molded feature has a generally triangular shape when viewed in side elevation.

5. The method of blow molding the plastic container according to claim 1 , wherein a ratio of the volume occupied by the molded feature to the volume defined by the maximum external dimensions of the molded feature is within a range of about 0.1 to about 0.8.

6. The method of blow molding the plastic container according to claim 5 , wherein the ratio is within a range of about 0.3 to about 0.6.

7. The method of blow molding the plastic container according to claim 1 , wherein the molded feature has a maximum wall thickness, and wherein a ratio of the maximum wall thickness to the maximum external dimension of the molded feature is within a range of about 0.05 to about 0.45.

8. The method of blow molding the plastic container according to claim 1 , wherein the main body portion, the neck portion, and the molded feature are fabricated from a material comprising high-density polyethylene.

9. The method of blow molding the plastic container according to claim 5 , wherein the ratio is within a range of about 0.2 to about 0.7.

10. The method of blow molding the plastic container according to claim 7 , wherein the ratio of the maximum wall thickness to the maximum external dimension of the molded feature is within a range of about 0.1 to about 0.35.

11. The method of blow molding the plastic container according to claim 10 , wherein the ratio of the maximum wall thickness to the maximum external dimension of the molded feature is within a range of about 0.2 to about 0.3.

12. The method of blow molding the plastic container according to claim 1 , wherein the increase in surface area is at least about 10%.

13. The method of blow molding the plastic container according to claim 1 , further comprising the step of evaluating whether the container has a sealing problem.

14. A method of blow molding a plastic container, comprising:

disposing a molten plastic in a mold;

blow molding the molten plastic in the mold to form a blow molded article comprising a main body portion defining an interior space, a cylindrical neck portion having an opening that is in communication with the interior space, and a molded feature that is adjacent to the neck portion and defines an anti-rotation lug having a generally triangular shape when viewed in side elevation, the molded feature being configured to reduce ovalization of the neck portion, wherein the molded feature has a cavity defined therein so that the molded feature occupies a volume that is less than a volume defined by maximum external dimensions of the molded feature, the molded feature having a first portion that is integral with the neck portion and a second portion with a surface defining an opening into the cavity of the molded feature that faces in a direction that is substantially opposite from the neck portion to increase a surface area of the molded feature relative to what the surface area would have been if the molded feature were solid and without an opening, wherein a ratio of the volume occupied by the molded feature to the volume defined by the maximum external dimensions of the molded feature is within a range of about 0.1 to about 0.8; and

removing the blow molded article from the mold.

15. The method of blow molding the plastic container according to claim 14 , wherein the volume of the molded feature is reduced by mold tooling.

16. The method of blow molding the plastic container according to claim 14 , wherein the molded feature has a maximum wall thickness, and wherein a ratio of the maximum wall thickness to the maximum external dimension of the molded feature is within a range of about 0.05 to about 0.45.

17. The method of blow molding the plastic container according to claim 14 , wherein the main body portion, the neck portion, and the molded feature are fabricated from a material comprising high-density polyethylene.

18. The method of blow molding the plastic container according to claim 14 , wherein the increase in surface area is at least about 10%.

19. The method of blow molding the plastic container according to claim 14 , further comprising the step of evaluating whether the container has a sealing problem.

20. A method of blow molding a plastic container, comprising:

the step of evaluating whether the container has a sealing problem;

disposing a molten plastic in a mold;

blow molding the molten plastic in the mold to form a blow molded article comprising a main body portion defining an interior space, a cylindrical neck portion having an opening that is in communication with the interior space, and a molded feature that is adjacent to the neck portion and defines an anti-rotation lug having a generally triangular shape when viewed in side elevation, the molded feature being configured to reduce ovalization of the neck portion, wherein the molded feature has a cavity defined therein so that the molded feature occupies a volume that is less than a volume defined by maximum external dimensions of the molded feature, the molded feature having a first portion that is integral with the neck portion and a second portion with a surface defining an opening into the cavity of the molded feature that faces in a direction that is substantially opposite the neck portion to increase by about 10% of a surface area of the molded feature relative to what the surface area would have been if the molded feature were solid and without an opening, wherein a ratio of the volume occupied by the molded feature to the volume defined by the maximum external dimensions of the molded feature is within a range of about 0.1 to about 0.8, wherein the molded feature has a maximum wall thickness, and wherein a ratio of the maximum wall thickness to the maximum external dimension of the molded feature is within a range of about 0.05 to about 0.45; and

removing the blow molded article from the mold.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Jan 26, 2026
From: UBS AG, STAMFORD BRANCH, AS COLLATERAL AGENT
To: GRAHAM PACKAGING COMPANY, L.P.; GRAHAM PACKAGING PET TECHNOLOGIES INC.; GRAHAM PACKAGING PLASTIC PRODUCTS LLC
Reel/Frame 074480/0105 →
SECURITY INTEREST Recorded Aug 4, 2020
From: GRAHAM PACKAGING COMPANY, L.P.; GRAHAM PACKAGING PET TECHNOLOGIES INC.; GRAHAM PACKAGING PLASTIC PRODUCTS LLC
To: CREDIT SUISSE AG, CAYMAN ISLANDS BRANCH, AS ADMINISTRATIVE AGENT
Reel/Frame 053398/0381 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 21, 2018
From: UNGRADY, ERIC B.; RUSSELL, MATTHEW A.; TOWNSEND, HOPE LEE; JAMES, MICHAEL L.
To: GRAHAM PACKAGING COMPANY, L.P.
Reel/Frame 046652/0547 →