IP Library Granted Patent US 10,497,970
Granted Patent B2
US 10,497,970 · App. 16/023,959 · Granted Dec 3, 2019

Alkali ion conducting plastic crystals

Inventors: Charles Austen Angell (Mesa, AZ); Iolanda Santana Klein (Tempe, AZ); Telpriore Greg Tucker (Phoenix, AZ)
Assignee: Arizona Board of Regents on behalf of Arizona State University
H01M10/0564H01M10/0525C07F7/025H01M10/056H01M10/0561H01M10/0562H01M2300/006H01M2300/0065H01M2300/0068H01M2300/0091
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,497,970
App. No.
16/023,959
Granted
Dec 3, 2019
Kind
B2
Abstract

A solid electrolyte represented by general formula Li y SiR x (MO 4 ), where x is an integer from 1 to 3 inclusive, y=4−x, each R present is independently C1-C3 alkyl or C1-C3 alkoxy, and M is sulfur, selenium, or tellurium. Methods of making the solid electrolyte include combining a phenylsilane and a first acid to yield mixture including benzene and a second acid, and combining at least one of an alkali halide, and alkali amide, and an alkali alkoxide with the second acid to yield a product d represented by general formula Li y SiR x (MO 4 ) y . The second acid may be in the form of a liquid or a solid. The phenylsilane includes at least one C1-C3 alkyl substituent or at least one C1-C3 alkoxy substituent, and the first acid includes at least one of sulfuric acid, selenic acid, and telluric acid.

Claims (28)

1. A solid electrolyte represented by general formula Li y SiR x (MO 4 ) y , wherein:

x is an integer from 1 to 3 inclusive,

y=4−Z,

each R present is independently C1-C2 alkoxy, and

M is sulfur or selenium.

2. The solid electrolyte of claim 1 , wherein each R present is independently C1-C2 alkoxy.

3. The solid electrolyte of claim 2 , wherein at least one R is methoxy.

4. The solid electrolyte of claim 2 , wherein at least one R is ethoxy.

5. The solid electrolyte of claim 1 , wherein x is 1.

6. The solid electrolyte of claim 1 , wherein x is 2.

7. The solid electrolyte of claim 1 , wherein x is 3.

8. A composition comprising a mixture of two or more different solid electrolytes of claim 1 .

9. A method of making a solid electrolyte, the method comprising:

combining a phenylsilane and a first acid to yield a mixture comprising benzene and a second acid, wherein the phenylsilane comprises at least one C1-C3 alkyl substituent or at least one C1-C2 alkoxy substituent and the first acid comprises a diprotic acid;

combining at least one of an alkali halide, an alkali amide, or an alkali alkoxide with the second acid to yield a product comprising a solid electrolyte represented by general formula Li y SiR x (MO 4 ) y , wherein:

x is an integer from 1 to 3 inclusive, y=4−X,

each R present is independently C1-C2 alkoxy, and

M is sulfur or selenium.

10. The method of claim 9 , wherein the phenylsilane is selected from the group consisting of trimethylphenylsilane, trimethoxyphenylsilane, methyldiethylphenylsilane, dimethylethylphenylsilane, diphenyldimethylsilane, dimethyldiphenylsilane, monomethyltriphenylsilane, triethylphenylsilane, methyldimethoxyphenylsilane, dimethylmethoxyphenylsilane, dimethylethoxyphenylsilane, methyldiethoxyphenylsilane, methylmethoxyethoxyphenylsilane, ethylmethoxyethoxyphenylsilane, triethoxyphenylsilane, methylethylpropylphenylsilane, methyldipropylphenylsilane, ethyldipropylphenylsilane, methypropyldiphenylsilane, methylpropyldiphenylsilane, ethylpropyldiphenylsilane, methylethylpropoxyphenylsilane, methyldipropoxyphenylsilane, dipropoxydiphenylsilane, methylethoxypropoxyphenylsilane, and ethoxypropoxydiphenylsilane.

11. The method of claim 9 , wherein the alkali amide is selected from the group consisting of lithium amides, sodium amides, and potassium amides.

12. The method of claim 9 , wherein the alkali alkoxide is selected from the group consisting of lithium alkoxides, sodium alkoxides, and potassium alkoxides.

13. The method of claim 9 , wherein combining the phenylsilane and the first acid replaces a phenyl group of the phenylsilane with a hydrogen oxyacid group to yield a silane, and the oxyacid group comprises sulfate or selenite.

14. The method of claim 9 , wherein the solid electrolyte is a first solid electrolyte, and further comprising combining the first solid electrolyte and a second solid electrolyte to yield a composite solid electrolyte.

15. The method of claim 9 , wherein the diprotic acid comprises at least one of sulfuric acid or selenic acid.

16. The method of claim 9 , wherein the alkali halide is selected from the group consisting of lithium halides, sodium halides, and potassium halides.

17. The method of claim 16 , wherein the alkali halide is an alkali chloride.

18. The method of claim 9 , wherein the second acid is in the form of a liquid or a solid.

19. The method of claim 9 , wherein the product is in the form of a waxy solid.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 18, 2018
From: ANGELL, CHARLES AUSTEN; KLEIN, IOLANDA SANTANA; TUCKER, TELPRIORE GREG
To: ARIZONA BOARD OF REGENTS ON BEHALF OF ARIZONA STATE UNIVERSITY
Reel/Frame 046895/0606 →
Continuity (4)
Continuation In Part 14775215
Provisional Application 62526963 · Jun 29, 2017
Provisional Application 61782292 · Mar 14, 2013
Related Publication 20190020060A1 · Jan 17, 2019