Electrooxidation at elevated pressures

Inventor: Bryan J. Kumfer (Ringle, WI)
Assignee: SIEMENS ENERGY, INC.
C02F1/4672C02F2001/46128C02F2001/46147C02F2101/34C02F2103/365C02F2201/005C02F2201/4611C02F2201/4614C02F2201/46145C02F2201/46155C02F2209/03
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,513,448
App. No.
16/075,189
Granted
Dec 24, 2019
Kind
B2
Abstract

There are provided electrooxidation systems and processes which provide an elevated pressure at which components are oxidized in an electrooxidation cell. The elevated pressure reduces power consumption for the cell at least in part by reducing the formation of gas bubbles, which typically leads to increased resistance and an increased power output.

Claims (13)

1. A process for treating a fluid comprising at least one oxidizable component comprising:

delivering the fluid to an electrooxidation cell for treatment of the at least one oxidizable organic component;

increasing and maintaining pressure within an electrooxidation zone of the electrooxidation cell to provide an elevated pressure of from 10 psi to 50 psi and a pressure drop across the electrooxidation cell of between 5 psi and 10 psi; and

oxidizing the oxidizable component within the electrooxidation cell at the elevated pressure at a current density of from 10,000 amps/m 2 to 40,000 amps/m 2 ; and

wherein the electrooxidation cell comprises at least an anode, a cathode, a bipolar electrode between the anode and the cathode, and a power source for the cell, the bipolar electrode further comprising a diamond material doped with a conductive dopant material.

2. The process of claim 1 , wherein the elevated pressure is from 20 psi to 45 psi.

3. The process of claim 1 , wherein the oxidizing is done at a current density of from 25,000 amps/m 2 to 35,000 amps/m 2 .

4. The process of claim 1 , wherein the dopant material is selected from the group consisting of lithium, beryllium, nitrogen, phosphorous, sulfur, chlorine, arsenic, selenium, and boron.

5. The process of claim 4 , wherein the dopant material comprises boron.

6. The process of claim 1 , wherein the increasing pressure within the electrooxidation cell is done by at least one of:

providing an orifice plate having a plurality of openings within a flowpath of the fluid dimensioned to increase pressure to a desired degree;

regulating a flow of the fluid with a flow control valve at an inlet and an outlet to the electrooxidation cell; or

increasing a height of a source of the fluid relative to a flowpath leading to and from the electrooxidation cell or to the electrooxidation cell.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 13, 2023
From: SIEMENS ENERGY, INC.
To: LUMMUS TECHNOLOGY LLC
Reel/Frame 064241/0044 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 25, 2018
From: KUMFER, BRYAN J.
To: SIEMENS ENERGY, INC.
Reel/Frame 047308/0659 →