IP Library Granted Patent US 10,794,960
Granted Patent B2
US 10,794,960 · App. 16/078,532 · Granted Oct 6, 2020

Method and apparatus for detecting low voltage defect of secondary battery

Inventors: Sung-Tae Kim (Daejeon, KR); Joon-Sung Bae (Daejeon, KR); Nak-Gi Sung (Daejeon, KR)
Assignee: LG CHEM, LTD.
G01R31/3865G01R31/36G01R31/388H01M10/0525H01M10/4285H01M10/446H01M10/48H01M10/0404
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,794,960
App. No.
16/078,532
Granted
Oct 6, 2020
Kind
B2
Abstract

Disclosed is a technique for effectively detecting a low voltage defect that may occur at a secondary battery. A method for detecting a low voltage defect of a secondary battery includes an assembling step of assembling a secondary battery by accommodating an electrode assembly, in which a positive electrode plate and a negative electrode plate are stacked with a separator being interposed therebetween, and an electrolytic solution in a battery case; a primary aging step of aging the assembled secondary battery at a temperature of 20° C. to 40° C.; a primary formation step of charging the aged secondary battery at a C-rate of 0.1 C to 0.5 C; a high-rate charging step of charging the secondary battery at a C-rate of 2 C or above, after the primary formation step; and a detecting step of detecting a defect of the secondary battery, after the high-rate charging step.

Claims (25)

1. A method for detecting a low voltage defect of a secondary battery, comprising:

an assembling step of assembling a secondary battery by accommodating an electrode assembly, in which a positive electrode plate and a negative electrode plate are stacked with a separator being interposed therebetween, and an electrolytic solution in a battery case;

a primary aging step of aging the assembled secondary battery at a temperature of 20° C. to 40° C.;

a primary formation step of charging the aged secondary battery at a C-rate of 0.1 C to 0.5 C;

a high-rate charging step of charging the secondary battery at a C-rate of 2 C or above, after the primary formation step; and

a detecting step of detecting a defect of the secondary battery, after the high-rate charging step.

2. The method for detecting a low voltage defect of a secondary battery according to claim 1 ,

wherein the high-rate charging step is performed during 10 seconds to 20 seconds.

3. The method for detecting a low voltage defect of a secondary battery according to claim 1 ,

wherein the high-rate charging step is performed at a temperature of 20° C. to 40° C.

4. The method for detecting a low voltage defect of a secondary battery according to claim 1 ,

wherein in the high-rate charging step, the secondary battery is charged at a C-rate of 3 C or above.

5. The method for detecting a low voltage defect of a secondary battery according to claim 1 , after the primary formation step and before the high-rate charging step, further comprising:

a secondary aging step of aging the secondary battery at a temperature condition of 60° C. to 70° C. during 12 hours to 72 hours; and

a secondary formation step of charging the secondarily aged secondary battery at a C-rate of 0.1 C to 2 C.

6. The method for detecting a low voltage defect of a secondary battery according to claim 5 ,

wherein the high-rate charging step is performed within 20 minutes to 120 minutes after the secondary formation step.

7. The method for detecting a low voltage defect of a secondary battery according to claim 1 ,

wherein in the detecting step, after the high-rate charging step, a difference in OCV between two different time points is compared with a reference value to determine whether a defect occurs at the secondary battery.

8. An apparatus for detecting a low voltage defect of a secondary battery, comprising:

an assembling unit configured to assemble a secondary battery by accommodating an electrode assembly, in which a positive electrode plate and a negative electrode plate are stacked with a separator being interposed therebetween, and an electrolytic solution in a battery case;

a primary aging unit configured to age the secondary battery, assembled by the assembling unit, at a temperature of 20° C. to 40° C.;

a primary formation unit configured to charge the secondary battery, aged by the primary aging unit, at a C-rate of 0.1 C to 0.5 C;

a high-rate charging unit configured to charge the secondary battery at a C-rate of 2 C or above, after the secondary battery is charged by the primary formation unit; and

a detecting unit configured to detect a defect of the secondary battery, after the secondary battery is charged by the high-rate charging unit.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2021
From: LG CHEM, LTD.
To: LG ENERGY SOLUTION, LTD.
Reel/Frame 058295/0068 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 22, 2018
From: KIM, SUNG-TAE; BAE, JOON-SUNG; SUNG, NAK-GI
To: LG CHEM, LTD.
Reel/Frame 046666/0800 →