Method for producing a gas-tight metal-ceramic join and use of the gas-tight metal-ceramic join

Inventors: Robert Hoffmann (Berlin, DE); Stefan Obermair (Stainz, AT)
Assignee: TDK ELECTRONICS AG
B23K1/0016B23K35/3006C04B37/023H01T4/12B23K2101/36B23K2103/52C04B2237/125C04B2237/405C04B2237/60C04B2237/76
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,154,945
App. No.
16/087,647
Granted
Oct 26, 2021
Kind
B2
Abstract

A method for producing a gas-tight metal-ceramic join is disclosed. In an embodiment a method includes providing at least one ceramic main body having a first end face and a second end face, applying a metallization to at least a partial region of the end faces of the main body, applying a nickel layer to the metallized partial region of the end faces, applying a brazing paste to the metallized partial region of the first end face and/or the second end face of the main body, drying the brazing paste, and firing the brazing paste.

Claims (43)

1. A method comprising:

providing at least one ceramic main body having a first end face and a second end face;

applying a metallization to at least a partial region of the first end face of the ceramic main body;

applying a metallization to at least a partial region of the second end face of the ceramic main body;

applying a nickel layer to the metallized partial region of the end faces;

applying a brazing paste to the metallized partial region of the first end face and to the metallized partial region of the second end face of the ceramic main body;

drying the brazing paste;

firing the brazing paste;

arranging a first metal electrode on the first end face of the ceramic main body and arranging a second metal electrode on the second end face of the ceramic main body after applying the brazing paste; and

connecting the first and second electrodes and the ceramic main body thereby producing a gas-tight connection between the metal electrodes and the ceramic main body.

2. The method according to claim 1 , wherein the ceramic main body is formed in an annular or cylindrical shape comprising a cavity, and wherein the end faces are arranged opposite one another and are connected to one another by a lateral surface of the ceramic main body.

3. The method according to claim 1 , wherein applying the brazing paste to the first and second end faces comprises applying the brazing paste to the first and second end faces simultaneously.

4. The method according to claim 1 , wherein the brazing paste is first applied to the first end face, dried and then applied to the second end face and dried.

5. The method according to claim 1 , wherein the brazing paste is applied to the end faces of the ceramic main body in a printing process.

6. The method according to claim 1 , wherein the brazing paste is applied to the end faces of the ceramic main body in a dipping process.

7. The method according to claim 1 , wherein the brazing paste comprises silver and copper.

8. The method according to claim 1 , wherein, apart from other constituents, the brazing paste comprises silver accounting for 35 to 65% by weight of the brazing paste and copper accounting for 13 to 30% by weight of the brazing paste.

9. The method according to claim 1 , wherein metals in powder form are provided for forming the brazing paste, and wherein a binder and a solvent are admixed in a liquid state with the metals.

10. The method according to claim 1 , wherein the connection of the first and second electrodes and the ceramic main body is performed at a temperature of 790° C. to 870° C. under a prescribed atmosphere.

11. The method according to claim 1 , wherein the ceramic main body comprises a cavity, and wherein the first and second electrodes on the end faces are at least partially introduced into the cavity and connected to the ceramic main body by the brazing paste.

12. The method according to claim 1 , wherein a plurality of ceramic main bodies are provided, and wherein the ceramic main bodies are inserted next to one another into a holder.

13. A method comprising:

providing at least one ceramic main body having a first end face and a second end face, the ceramic main body being formed in an annular or cylindrical shape comprising a cavity, and the end faces being arranged opposite one another and connected to one another by a lateral surface of the ceramic main body;

applying a metallization to at least a partial region of the first end face of the ceramic main body;

applying a metallization to at least a partial region of the second end face of the ceramic main body;

applying a nickel layer to the metallized partial region of the end faces;

applying a brazing paste to the metallized partial region of at least one of the first end face and the second end face of the ceramic main body;

drying the brazing paste;

firing the brazing paste;

arranging a first metal electrode on the first end face of the ceramic main body and arranging a second metal electrode on the second end face of the ceramic main body after applying the brazing paste; and

connecting the first and second electrodes and the ceramic main body thereby producing a gas-tight connection between the metal electrodes and the ceramic main body.

14. The method according to claim 1 , wherein connecting the first and second electrodes and the ceramic main body comprises brazing the first and second electrodes and the ceramic main body thereby producing the gas-tight connection between the metal electrodes and the ceramic main body.

15. The method according to claim 1 , wherein the first electrode has a form of a metal cap, and wherein the second electrode has a form of a metal cap.

16. A method comprising:

providing at least one ceramic main body having a first end face and a second end face;

applying a metallization to at least a partial region of the first end face of the ceramic main body;

applying a metallization to at least a partial region of the second end face of the ceramic main body;

applying a nickel layer to the metallized partial region of the end faces;

applying a brazing paste to the metallized partial region of the first end face and to the metallized partial region of the second end face of the ceramic main body;

drying the brazing paste;

firing the brazing paste;

arranging a first metal electrode on the first end face of the ceramic main body and arranging a second metal electrode on the second end face of the ceramic main body after firing the brazing paste; and

connecting the first and second electrodes and the ceramic main body thereby producing a gas-tight connection between the metal electrodes and the ceramic main body.

Assignments (4)
CHANGE OF NAME Recorded Mar 15, 2023
From: EPCOS AG
To: TDK ELECTRONICS AG
Reel/Frame 063101/0709 →
CORRECTIVE ASSIGNMENT TO CORRECT THE ASSIGNEE PREVIOUSLY RECORDED ON REEL 051704 FRAME 0310. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT OF INVENTOR'S INTEREST. Recorded Apr 16, 2021
From: OBERMAIR, STEFAN
To: TDK ELECTRONICS AG
Reel/Frame 055953/0471 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 3, 2020
From: OBERMAIR, STEFAN
To: TDK ELECTRONICS GMBH & CO OG
Reel/Frame 051704/0310 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 3, 2020
From: HOFFMANN, ROBERT
To: TDK ELECTRONICS AG
Reel/Frame 051704/0318 →
Priority Claims (1)
DE 10 2016 105 456.9 · Mar 23, 2016 · national
Continuity (1)
Related Publication 20200122257A1 · Apr 23, 2020