IP Library Granted Patent US 11,060,012
Granted Patent B2
US 11,060,012 · App. 16/092,420 · Granted Jul 13, 2021

Deposit disintegrator compositions

Inventors: Nirmal Tatavalli-Mittadar (Richmond, TX); Sunil Ashtekar (Houston, TX); Shekhar Jain (Houston, TX); Jian Lu (Bellaire, TX); Sujatha Degaleesan (Katy, TX); Kamran Akbar Zadeh (Katy, TX)
Assignee: SHELL OIL COMPANY
C09K8/524B08B9/027F16L55/24
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,060,012
App. No.
16/092,420
Granted
Jul 13, 2021
Kind
B2
Abstract

A solvent mixture comprising a solvent and a polar additive and associated methods.

Claims (28)

1. A method for disintegrating a wax deposit in oil and gas pipelines, the method comprising the steps of:

identifying a wax deposit site in a subsea pipeline or well;

providing a solvent mixture, wherein the solvent mixture comprises a non-polar solvent and dimethyl sulfoxide;

injecting the solvent mixture into the subsea pipeline or well, so that the solvent mixture contacts the wax deposit site be shutting-in the subsea pipeline of well, by providing a spacer fluid before and after the solvent mixture, or a combination thereof;

and allowing the solvent mixture to disintegrate the wax deposit.

2. The method of claim 1 , wherein the non-polar solvent is selected from the group consisting of xylene, tetralin, decalin, toluene, terpene, naphtha, diesel and combinations thereof.

3. The method of claim 1 , wherein the non-polar solvent is present in the solvent mixture in an amount in the range of from 30% to 98% by volume of the solvent mixture.

4. The method of claim 1 , wherein the dimethyl sulfoxide is present in the solvent mixture in an amount in the range of from 2% to 60% by volume of the solvent mixture.

5. The method of claim 1 , wherein the volume ratio of dimethyl sulfoxide to non-polar solvent in the solvent mixture is in the range of from 0.01 to 0.6.

6. The method of claim 1 , wherein the solvent mixture further comprises a second bulk solvent.

7. The method of claim 6 , wherein the second bulk solvent is selected from the group consisting of naphtha, terpene, decalin, a C5-C11 alkane, diesel, a cyclic aromatic compound, a bicyclic aromatic compound, and combinations thereof.

8. The method of claim 7 , wherein the second bulk solvent is present in the solvent mixture in an amount in the range of from 2% to 40% by volume of the solvent mixture.

9. The method of claim 1 , wherein the non-polar solvent is present in the solvent mixture in an amount in the range of from 75% to 95% by volume of the solvent mixture.

10. The method of claim 1 , wherein the dimethyl sulfoxide is present in the solvent mixture in an amount in the range of from 5% to 20% by volume of the solvent mixture.

11. A method for disintegrating a wax deposit in oil and gas pipelines, the method comprising the steps of:

identifying a wax deposit site in a subsea pipeline or well;

providing a solvent mixture, wherein the solvent mixture comprises a non-polar solvent selected from the group consisting of xylene, tetralin, terpene, and combinations thereof, and a polar additive;

injecting the solvent mixture into the subsea pipeline or well, so that the solvent mixture contacts the wax deposit site by shutting-in the subsea pipeline or well, by providing a spacer fluid before and after the solvent mixture, or a combination thereof;

and allowing the solvent mixture to the wax deposit.

12. The method of claim 11 , wherein the non-polar solvent is present in the solvent mixture in an amount in the range of from 30% to 98% by volume of the solvent mixture.

13. The method of claim 11 , wherein the polar additive is selected from the group consisting of di-methyl sulfoxide, dimethyl carbonate, dimethyl formamide, nitromethane and combinations thereof.

14. The method of claim 11 , wherein the polar additive is present in the solvent mixture in an amount in the range of from 2% to 60% by volume of the solvent mixture.

15. The method of claim 11 , wherein the volume ratio of polar additive to non-polar solvent in the solvent mixture is in the range of from 0.01 to 0.6.

16. The method of claim 11 , wherein the solvent mixture further comprises a second bulk solvent.

17. The method of claim 16 , wherein the second bulk solvent is selected from the group consisting of naphtha, terpene, decalin, a C5-C11 alkane, diesel, a cyclic aromatic compound, a bicyclic aromatic compound, and combinations thereof.

18. The method of claim 16 , wherein the second bulk solvent is present in the solvent mixture in an amount in the range of from 2% to 40% by volume of the solvent mixture.

19. The method of claim 11 , wherein the non-polar solvent is present in the solvent mixture in an amount in the range of from 75% to 95% by volume of the solvent mixture.

20. The method of claim 11 , wherein the dimethyl sulfoxide is present in the solvent mixture in an amount in the range of from 5% to 20% by volume of the solvent mixture.

Assignments (2)
CHANGE OF NAME Recorded Mar 7, 2022
From: SHELL OIL COMPANY
To: SHELL USA, INC.
Reel/Frame 059694/0819 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 14, 2021
From: TATAVALLI-MITTADAR, NIRMAL; ASHTEKAR, SUNIL; JAIN, SHEKHAR; LU, JIAN; DEGALEESAN, SUJATHA; AKBAR ZADEH, KAMRAN
To: SHELL OIL COMPANY
Reel/Frame 056561/0455 →