IP Library Granted Patent US 11,107,939
Granted Patent B2
US 11,107,939 · App. 16/257,569 · Granted Aug 31, 2021

Systems and methods for shingling cells using an adhesive film

Inventors: Todd Allen Krajewski (Mountain View, CA); Jason Tolentino (San Jose, CA)
Assignee: UTICA LEASECO, LLC
H01L31/0481C09J7/381H01L31/05H01L31/18B32B7/12B32B2457/12C09J7/29
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,107,939
App. No.
16/257,569
Granted
Aug 31, 2021
Kind
B2
Abstract

This disclosure describes various structures, devices, and arrangements that replace a PSA used to hold shingled cells together with an adhesive film. For example, in an aspect, the present disclosure is directed to a shingled arrangement of photovoltaic (PV) cells. In some aspects, the shingled arrangement of PV cells may include a first PV cell, a second PV cell, and an adhesive film placed between a backside the first PV cell and a front side of the second PV cell. The adhesive film may be thermally bonded to the first PV cell and to the second PV cell after the application of localized heat and pressure and holds the first PV cell and the second PV cell together. Additionally, a bus bar of the second PV cell may be electrically connected to the first PV cell by a conductive via formed through the adhesive film.

Claims (63)

1. A shingled arrangement of photovoltaic (PV) cells comprising;

a first PV cell;

a second PV cell; and

an adhesive film placed between a backside the first PV cell and a front side of the second PV cell, the adhesive film is thermally bonded to the first PV cell and to the second PV cell after an application of localized heat and pressure and holds the first PV cell and the second PV cell together,

wherein a bus bar of the second PV cell is electrically connected to the first PV cell by a conductive via formed through the adhesive film, and

wherein the adhesive film is a single strip of film having a same width of the bus bar of the second PV cell.

2. The shingled arrangement of PV cells of claim 1 , wherein the adhesive film comprises a single layer of a thermoplastic or a thermoset.

3. The shingled arrangement of PV cells of claim 2 , wherein the thermoplastic or the thermoset comprises a modified low-density polyethylene resin, a modified ethylene vinyl acetate, a modified ethylene acetate, an anhydride-modified high-density polyethylene, an anhydride-modified linear low-density polyethylene, an anhydride-modified polypropylene, an acid-modified ethylene terpolymer, an ethylene/acrylate copolymer resin, an ionomer, a polyolefin (POE), an ethylene-vinyl acetate (EVA), a thermoplastic polyurethane (TPUR, TPU), or a polyethylene (PE).

4. The shingled arrangement of PV cells of claim 1 , wherein:

the adhesive film is an adhesive film stack that comprises a first adhesive film adjacent to the backside of the first PV cell, a second adhesive film adjacent to the front side of the second PV cell, and a carrier film between the first adhesive film and the second adhesive film,

the carrier film is configured to increase a stiffness of the adhesive film stack, and

each of the first adhesive film and the second adhesive film is made of a single layer of a thermoplastic or a thermoset.

5. The shingled arrangement of PV cells of claim 4 , wherein the carrier film is treated using an adhesion improvement technique.

6. The shingled arrangement of PV cells of claim 4 , further comprising a tie layer formed on a backside of the carrier film to improve adhesion.

7. The shingled arrangement of PV cells of claim 4 , wherein the thermoplastic or the thermoset comprises a modified low-density polyethylene resin, a modified ethylene vinyl acetate, a modified ethylene acetate, an anhydride-modified high-density polyethylene, an anhydride-modified linear low-density polyethylene, an anhydride-modified polypropylene, an acid-modified ethylene terpolymer, an ethylene/acrylate copolymer resin, an ionomer, a polyolefin (POE), an ethylene-vinyl acetate (EVA), a thermoplastic polyurethane (TPUR, TPU), or a polyethylene (PE).

8. The shingled arrangement of PV cells of claim 4 , wherein a thickness of the first adhesive film and a thickness of the second adhesive film are both smaller than a thickness of the carrier film.

9. The shingled arrangement of PV cells of claim 1 , wherein:

the adhesive film is an adhesive film stack that comprises a first adhesive film adjacent to the backside of the first PV cell, a second adhesive film adjacent to the front side of the second PV cell, and a carrier film between the first adhesive film and the second adhesive film,

the carrier film is configured to increase a stiffness of the adhesive film stack,

the first adhesive film is made of a pressure-sensitive adhesive (PSA), and

the second adhesive film is made of a single layer of a thermoplastic or a thermoset.

10. The shingled arrangement of PV cells of claim 9 , wherein the thermoplastic or the thermoset comprises a modified low-density polyethylene resin, a modified ethylene vinyl acetate, a modified ethylene acetate, an anhydride-modified high-density polyethylene, an anhydride-modified linear low-density polyethylene, an anhydride-modified polypropylene, an acid-modified ethylene terpolymer, an ethylene/acrylate copolymer resin, an ionomer, a polyolefin (POE), an ethylene-vinyl acetate (EVA), a thermoplastic polyurethane (TPUR, TPU), or a polyethylene (PE).

11. The shingled arrangement of PV cells of claim 9 , wherein a thickness of the first adhesive film is smaller than a thickness of the second adhesive film, and a thickness of the carrier film is greater than both the thickness of the first adhesive film and the thickness of the second adhesive film.

12. The shingled arrangement of PV cells of claim 1 , wherein:

the adhesive film includes a first strip and a second strip to a side of the first strip and separated from the first strip by a spacing, and

the conductive via formed through the adhesive film is formed in the spacing that separates the first strip from the second strip.

13. The shingled arrangement of PV cells of claim 1 , wherein:

the adhesive film includes a plurality of holes formed prior to placing the adhesive film between the first PV cell and the second PV cell, and

the conductive via formed through the adhesive film is formed through one of the plurality of holes formed in the adhesive film.

14. The shingled arrangement of PV cells of claim 1 , wherein:

the first PV cell includes a back surface film on the backside of the first PV cell,

the adhesive film is placed between the back surface film and the front side of the second PV cell, and

the conductive via is formed through the adhesive film and through a back surface layer.

15. The shingled arrangement of PV cells of claim 14 , wherein the back surface layer is made of polyethylene naphthalate (PEN) or polyethylene terephthalate (PET).

16. A method for shingling photovoltaic (PV) cells comprising:

applying an adhesive film to a backside of a first PV cell, the adhesive film comprising at least one of a thermoplastic or a thermoset;

filling one or more vias formed through the adhesive film with a conductive material;

aligning a bus bar on a front side of a second PV cell with the filled one or more vias;

placing a front side of the second PV cell against the adhesive film while maintaining the bus bar and the one or more vias aligned; and

bonding the first PV cell and the second PV cell with one another using at least one of localized heat or pressure;

wherein applying the adhesive film to the backside of the first PV cell comprises thermally bonding the adhesive film to the backside of the first PV cell.

17. The method of claim 16 , wherein the thermoplastic or the thermoset comprises a modified low-density polyethylene resin, a modified ethylene vinyl acetate, a modified ethylene acetate, an anhydride-modified high-density polyethylene, an anhydride-modified linear low-density polyethylene, an anhydride-modified polypropylene, an acid-modified ethylene terpolymer, an ethylene/acrylate copolymer resin, an ionomer, a polyolefin (POE), an ethylene-vinyl acetate (EVA), a thermoplastic polyurethane (TPUR, TPU), or a polyethylene (PE).

18. The method of claim 16 , wherein the adhesive film comprises a single, contiguous film of material, and the method further comprises forming the one or more vias through the adhesive film to expose a metal contact of the first PV cell.

19. The method of claim 16 , wherein the adhesive film is a single strip of film wider than a size of the bus bar of the second PV cell.

20. The method of claim 16 , wherein the adhesive film is a single strip of film having a same width of the bus bar of the second PV cell.

21. The method of claim 16 , wherein:

the adhesive film is an adhesive film stack that comprises a first adhesive film adjacent to the backside of the first PV cell, a second adhesive film adjacent to the front side of the second PV cell, and a carrier film between the first adhesive film and the second adhesive film,

the carrier film is configured to increase a stiffness of the adhesive film stack, and

each of the first adhesive film and the second adhesive film is made of a single layer of the thermoplastic or the thermoset.

22. The method of claim 16 , wherein:

the adhesive film is an adhesive film stack that comprises a first adhesive film adjacent to the backside of the first PV cell, a second adhesive film adjacent to the front side of the second PV cell, and a carrier film between the first adhesive film and the second adhesive film,

the carrier film is configured to increase a stiffness of the adhesive film stack,

the first adhesive film is made of a pressure-sensitive adhesive (PSA), and

the second adhesive film is made of a single layer of the thermoplastic or the thermoset.

23. The method of claim 16 , wherein:

a release layer is attached to a top portion of the adhesive film prior to an application of the adhesive film to the backside of the first PV cell,

applying the adhesive film to the backside of the first PV cell comprises applying a bottom portion of the adhesive film to the backside of the first PV cell and removing the release layer from the top portion of the adhesive film.

24. The method of claim 23 , wherein a thickness of the release layer is greater than a thickness of the adhesive film to increase stiffness for handling of the adhesive film.

25. The method of claim 16 , wherein:

the first PV cell includes a back surface film on the backside of the first PV cell,

applying the adhesive film to the backside of the first PV cell comprises applying the adhesive film to the back surface film of the first PV cell, and

filling the one or more vias comprises filling the one or more vias formed through the adhesive film and the back surface film.

26. The method of claim 25 , wherein the back surface film is made of polyethylene naphthalate (PEN) or polyethylene terephthalate (PET).

Assignments (4)
SECURITY INTEREST Recorded Aug 28, 2023
From: UTICA LEASECO, LLC
To: TIGER FINANCE, LLC
Reel/Frame 064731/0814 →
CORRECTIVE ASSIGNMENT TO CORRECT THE THE ASSIGNEE ADDRESS PREVIOUSLY RECORDED AT REEL: 055766 FRAME: 0279. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded Aug 9, 2021
From: UTICA LEASECO, LLC SECURED PARTY
To: UTICA LEASECO, LLC ASSIGNEE
Reel/Frame 057117/0811 →
CONFIRMATION OF FORECLOSURE TRANSFER OF PATENT RIGHTS Recorded Feb 25, 2021
From: UTICA LEASECO, LLC SECURED PARTY
To: UTICA LEASECO, LLC ASSIGNEE
Reel/Frame 055766/0279 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 25, 2019
From: KRAJEWSKI, TODD ALLEN; TOLENTINO, JASON
To: ALTA DEVICES, INC.
Reel/Frame 048136/0709 →