Paper products and pulps with surface enhanced pulp fibers and increased absorbency, and methods of making same
View Patent ↗Paper products such as tissues can be made using a furnish comprising surface enhanced pulp fibers (“SEPF”). In some embodiments, SEPF have a weighted average fiber length of at least 0.3 millimeters (mm) and an average hydrodynamic specific surface area of at least 10 square meters per gram (m 2 /g). In some embodiments, a furnish or a paper product can comprise at least 2 % SEPF by dry weight. In some embodiments, a paper product comprising SEPF can be formed from a furnish having a freeness of 650 ml Canadian Standard Freeness (CSF) or less, optionally 600 ml CSF or less.
1. A method of manufacturing tissue, the method comprising:
mixing at least a first pulp and a second pulp to generate a furnish, wherein:
the first pulp comprises surface enhanced pulp fibers having a length weighted average fiber length of at least 0.3 millimeters (mm) and an average hydrodynamic specific surface area of at least 10 square meters per gram (m 2 /g);
the second pulp comprises softwood fibers; and
mixing is performed such that the furnish comprises from 10% to 25% surface enhanced pulp fibers by dry weight of fiber in the furnish; and
beating, with a refiner, the furnish such that the furnish has a freeness less than or equal to 650 milliliters Canadian Standard Freeness (ml CSF).
2. The method of claim 1 , wherein beating is performed such that the furnish has a freeness of 600 ml CSF or less.
3. The method of claim 2 , wherein beating is performed such that the furnish has a freeness between 550 ml CSF and 600 ml CSF.
4. The method of claim 1 , wherein mixing is performed such that the furnish comprises between 5% and 25% surface enhanced pulp fibers by dry weight of fiber in the furnish.
5. The method of claim 1 , comprising forming one or more sheets of tissue using the furnish such that the sheet(s) have a grammage between 20 and 45 grams per square meter (g/m 2 ).
6. The method of claim 1 , wherein the softwood fibers of the second pulp comprise Northern bleached softwood kraft fibers.
7. The method of claim 1 , wherein beating is performed such that a decrease in the freeness of the furnish is less than or equal to 300 ml CSF.