IP Library Granted Patent US 11,078,331
Granted Patent B2
US 11,078,331 · App. 16/376,669 · Granted Aug 3, 2021

Acid neutralizing polymer materal and method of making same

Inventors: Matthew James Borowiak, Jr. (Buffalo, NY); Richard Earl Partch (Hannawa Falls, NY)
Assignees: Workers First LLC; Clarkson University
C08G69/48
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,078,331
App. No.
16/376,669
Granted
Aug 3, 2021
Kind
B2
Abstract

A method of preparing an acid reactive functionalized polyamide includes preparing a first reaction product by contacting and reacting virgin polyamide fabric material with tert-butoxide in a first aliquot of a polar aprotic solvent and preparing a second reaction product by adding an amine to a second aliquot of the polar aprotic solvent. A third reaction product is prepared by mixing the first reaction product and the second reaction product where the third reaction product is the acid reactive functionalized polyamide. The preparation of each respective reaction product is for a period of time and at a temperature sufficient to produce the respective reaction product.

Claims (13)

1. A method of preparing an acid neutralizing polyamide, comprising:

a) preparing a first reaction product by contacting and reacting virgin polyamide fabric material with tert-butoxide in a first aliquot of a polar aprotic solvent;

b) preparing a mixture of 2-chloro-N, N-dimethylamine and a second aliquot of the polar aprotic solvent; and

c) preparing a second reaction product being the acid neutralizing polyamide by mixing the first reaction product and the mixture,

wherein each of steps a) and c) is for a period of time and at a temperature sufficient to produce the respective first and second reaction products.

2. The method of claim 1 wherein the virgin polyamide fabric material comprises nylon 6 or nylon 66.

3. The method of claim 1 wherein the polar aprotic solvent is either dimethyl sulfoxide (DMSO) or dimethylformamide (DMF).

4. The method of claim 1 wherein the first reaction product is prepared under stirring at room temperature for at least 1 hour.

5. The method of claim 1 wherein the the mixture of step b) is prepared under stirring at room temperature for at least 2 hours.

6. The method of claim 1 wherein the third second reaction product is prepared under stirring at room temperature for at least 12 hours.

7. The method of claim 1 further comprising the step of:

d) following the preparation step c), washing the second reaction product sequentially with the polar aprotic solvent, tetrahydrofuran (THF) and water.

8. An acid neutralizing polyamide fabric material produced according to the method of claim 1 .

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 30, 2020
From: PARTCH, RICHARD EARL, DR.
To: CLARKSON UNIVERSITY
Reel/Frame 053091/0256 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 5, 2019
From: BOROWIAK, MATTHEW JAMES, JR
To: WORKERS FIRST LLC
Reel/Frame 048807/0644 →
Continuity (2)
Provisional Application 62653788 · Apr 6, 2018
Related Publication 20190309128A1 · Oct 10, 2019