SECONDARY BATTERY AND METHOD FOR MANUFACTURING SAME

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
16/380,292
Abstract

An object of the present invention is to provide a high-quality secondary battery having high electric characteristics and high reliability, the secondary battery preventing a shortcut between a positive electrode and a negative electrode by means of an insulating material and preventing or reducing an increase in volume and deformation of a battery electrode assembly, and a method for manufacturing the same. Secondary battery 100 according to the present invention includes a battery electrode assembly including positive electrode 1 and negative electrode 6 alternately stacked via separator 20. Positive electrode 1 and negative electrode 2 each includes current collector 3 or 8 and active material 2 or 7 applied to current collector 3 or 8. Active material 2 A positioned on one surface of positive electrode 1 of current collector 3 includes flat portion 2 A 1 and small-thickness portion (thin-layer portion) 2 A 3 positioned on the end portion side relative to flat portion 2 A 1 , the small-thickness portion 2 A 3 having a thickness that is smaller than that of flat portion 2 A 1 . A portion of active material 2 B positioned on another surface of current collector 3 of positive electrode 1, the portion facing thin-layer portion 2 A 3 of active material 2 A positioned on the one surface via current collector 3 is a flat portion having a constant thickness.

Claims (8)

1 . A secondary battery manufacturing method comprising:

forming a positive electrode by applying a positive-electrode active material to each of opposite surfaces of a positive-electrode current collector;

forming a negative electrode by applying a negative-electrode active material to each of opposite surfaces of a negative-electrode current collector; and

alternately stacking the positive electrode and the negative electrode via a separator, wherein

the forming of the positive electrode includes applying a positive-electrode active material layer to a surface of the positive-electrode current collector to form a positive-electrode active material layer consisting essentially of a flat portion, and then

applying a positive-electrode active material layer to a surface on an opposite side of the surface with the positive-electrode active material consisting essentially of a flat portion formed thereon to form a positive-electrode active material layer including a large-thickness portion and a small-thickness portion having a thickness that is smaller than that of the large-thickness portion.

2 . The secondary battery manufacturing method according to claim 1 ,

further comprising disposing an insulating material to cover a boundary portion between a coated portion to which the positive-electrode active material has been applied and a non-coated portion to which the positive-electrode active material has not been applied in the positive electrode.

Assignments (1)
CHANGE OF NAME Recorded Jun 21, 2019
From: NEC ENERGY DEVICES, LTD.
To: ENVISION AESC ENERGY DEVICES, LTD.