IP Library Granted Patent US 10,464,258
Granted Patent B2
US 10,464,258 · App. 16/384,055 · Granted Nov 5, 2019

Method for producing an object by melting a polymer powder in a powder sintering device

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,464,258
App. No.
16/384,055
Granted
Nov 5, 2019
Kind
B2
Abstract

A graft copolymer comprising: a core polymer comprising a crosslinked or non-crosslinked polysaccharide, a plurality of primary graft polymers covalently grafted to the core polymer, a plurality of secondary graft polymers covalently grafted to each primary graft polymer, an injectable dermal aesthetic formulation comprising such a graft copolymer and a method of preparing such a graft copolymer.

Claims (9)

1. A composition comprising a semicrystalline polymer having a viscosity of between 800 and 20,000 Pa·s over a time of more than 5 minutes, the viscosity measurements being carried out in a plate-plate rheometer device at a stress frequency of less than 5 rad/s, said composition being supercooled to a temperature T below the melting temperature after exposure to a temperature Tmax above its melting point, wherein the composition is configured for use in a device for manufacturing objects by melting polymer powders.

2. The composition of claim 1 , wherein the composition is a polyamide.

3. The composition of claim 1 , wherein the composition is a filled polyamide.

4. The composition of claim 1 , wherein the composition is a polyaryletherketone.

5. The composition of claim 1 , wherein the composition is a filled polyaryletherketone.

6. The composition of claim 1 , wherein the semicrystalline polymer has a viscosity of between 800 and 20,000 Pa·s over a time of more than 10 minutes.

7. The composition of claim 1 , wherein the semicrystalline polymer has a viscosity of between 1000 and 10,000 Pa·s over a time of more than 5 minutes.

8. The composition of claim 1 , wherein the semicrystalline polymer has a viscosity of between 1000 and 10,000 Pa·s over a time of more than 10 minutes.

9. The composition of claim 1 , wherein the composition is configured for use in a device for manufacturing objects by laser sintering of polymers.

Assignments (2)
CHANGE OF ADDRESS Recorded Jul 4, 2025
From: ARKEMA FRANCE
To: ARKEMA FRANCE
Reel/Frame 071814/0739 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 15, 2019
From: BRULE, BENOÎT; DECRAEMER, NADINE
To: ARKEMA FRANCE
Reel/Frame 048884/0141 →