IP Library Granted Patent US 11,358,311
Granted Patent B2
US 11,358,311 · App. 16/427,835 · Granted Jun 14, 2022

Optical element and method for manufacturing optical element

Inventors: Takehiko Goshima (Kunitachi, JP); Yoshihiro Okumura (Toyohashi, JP); Hiroshi Umetsu (Tachikawa, JP); Seiji Yuasa (Tama, JP)
Assignee: OTSUKA PHARMACEUTICAL CO., LTD
B29C45/0025B29C45/372B29D11/00644G02B1/04G02B3/00B29C45/2756B29K2101/12B29K2995/0013B29K2995/0072B29L2011/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,358,311
App. No.
16/427,835
Granted
Jun 14, 2022
Kind
B2
Abstract

To provide a method for manufacturing an optical element, which improves the surface precision of the optical surface as well as reducing the birefringence at a low cost. A method for manufacturing an optical element 1090 A having optical surfaces 1091 and 1092 and a non-optical surface 1093 A that is adjacent to the optical surface 1092 via a ridge by injection molding includes forming the non-optical surface 1093 A with a mold surface. The mold surface includes a sink forming area 1095 as a first area having a first surface roughness, and a high transfer area 1094 as a second area having a second surface roughness different from the first surface roughness. The second area is located outside the first area.

Claims (9)

1. A method for manufacturing an optical element having an optical surface and a non-optical surface that is adjacent to the optical surface via a ridge by injection molding, the method comprising:

forming the non-optical surface with a mold having a surface that includes a first area having a first thermal conductivity for forming a sink area, and a second area having a second thermal conductivity larger than the first thermal conductivity, the first area having a short side and a long side, the second area having a short side and a long side, and the second area being located between the first area and the optical surface,

wherein a length of the long side of the first area is the same as a length of the long side of the second area, and the long side of the first area is in contact with the long side of the second area in its entirety.

2. The method according to claim 1 , wherein

the first thermal conductivity is not less than 0.6 W/m·K and not more than 20 W/m·K, and

the second thermal conductivity is not less than 8 W/m·K and not more than 200 W/m·K.

3. The method according to claim 1 , wherein a difference between a surface roughness of the first area and a surface roughness of the second area is not less than Ra 0.3 μm and less than Ra 100 μm.

4. The method according to claim 1 , wherein the second area is located adjacent to a surface of the mold where the optical surface is formed.

5. The method according to claim 1 , wherein (a length of the short side of the second area)/(the length of the short side of the second area+a length of the short side of the first area)×100 is 15 to 60%.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 21, 2022
From: KONICA MINOLTA, INC.
To: OTSUKA PHARMACEUTICAL CO., LTD.
Reel/Frame 059747/0589 →
Priority Claims (1)
JP 2013-058838 · Mar 21, 2013 · national
Continuity (2)
Division 14776303
Related Publication 20190283290A1 · Sep 19, 2019