IP Library Granted Patent US 11,459,492
Granted Patent B2
US 11,459,492 · App. 16/466,679 · Granted Oct 4, 2022

Adhesive composition having anti-fogging property

Inventors: Tadahiko Mikami (Shiga, JP); Masahito Tanigawa (Shiga, JP)
Assignee: TOYOBO CO., LTD.
C09J167/00B65D65/40C09J7/20C09J11/06C09J167/02C08K5/06C08L2205/025C09J7/255C09J2203/00C09J2301/312C09J2301/408C09J2467/00C09J2467/006
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,459,492
App. No.
16/466,679
Granted
Oct 4, 2022
Kind
B2
Abstract

The present invention aims to provide an adhesive composition having excellent adhesive property and excellent anti-fogging property by way of simple and easy means such as co-extrusion with a substrate film, extrusion coating, solvent coating, etc. According to the present invention, there is provided an adhesive composition, characterized in that it contains a polyester resin (A) and an anti-fogging agent (C), and satisfies the following requirement (1): (1) Glass transition temperature of the polyester resin (A) is from −30 to 30° C.

Claims (14)

1. An adhesive composition, comprising a polyester resin (A), a polyester resin (B), and an anti-fogging agent (C),

wherein the polyester resin (A) is a copolymerized polyester resin consisting of a dicarboxylic acid component and a glycol component, wherein the dicarboxylic acid component comprises an aromatic dicarboxylic acid and an aliphatic dicarboxylic acid in a molar ratio in terms of aromatic dicarboxylic acid:aliphatic dicarboxylic acid of 70:30 to 55:45,

the polyester resin (A) satisfies the following requirement (1):

(1) Glass transition temperature of the polyester resin (A) is from −30 to 30° C.,

the polyester resin (B) satisfies the following requirement (2):

(2) Glass transition temperature of the polyester resin (B) is from 40 to 82° C., and

the adhesive composition comprises 1 to 5 part(s) by mass of the anti-fogging agent (C) to 100 parts by mass of the polyester resin (A).

2. The adhesive composition according to claim 1 , wherein the anti-fogging agent (C) is a nonionic surfactant.

3. A laminated film, which is prepared by laminating an adhesive layer comprising the adhesive composition according to claim 1 and a thermoplastic resin film.

4. The laminated film according to claim 3 , wherein the thermoplastic film is a polyester resin film.

5. The laminated film according to claim 3 , wherein a thickness of the adhesive layer is from 1 to 10 μm.

6. A packaging material, comprising the laminated film according to claim 5 as a constituting member.

7. A covering material for a food packaging container, comprising the packaging material according to claim 6 as a constituting member.

8. A food packaging container, which is prepared by laminating the covering material according to claim 7 and a polyester resin.

Assignments (3)
CHANGE OF ADDRESS Recorded Aug 7, 2023
From: TOYOBO CO., LTD.
To: TOYOBO CO., LTD.
Reel/Frame 064505/0124 →
DE-MERGER Recorded Aug 7, 2023
From: TOYOBO CO., LTD.
To: TOYOBO MC CORPORATION
Reel/Frame 064505/0803 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 5, 2019
From: MIKAMI, TADAHIKO; TANIGAWA, MASAHITO
To: TOYOBO CO., LTD.
Reel/Frame 049375/0344 →
Priority Claims (1)
JP JP2017-065332 · Mar 29, 2017 · national
Continuity (1)
Related Publication 20200063006A1 · Feb 27, 2020