IP Library Granted Patent US 11,000,458
Granted Patent B2
US 11,000,458 · App. 16/491,685 · Granted May 11, 2021

Method and product for producing formulations containing ceramide

Inventors: Ursula Maczkiewitz (Essen, DE); Maria Mecking (Bottrop, DE); Annika Schrader (Bremen, DE)
Assignee: Evonik Operations GmbH
A61K8/062A61K8/0216A61K8/31A61K8/342A61K8/361A61K8/375A61K8/68A61K8/922A61K8/925A61Q19/00A61K2800/10A61K2800/805
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,000,458
App. No.
16/491,685
Granted
May 11, 2021
Kind
B2
Abstract

The subject matter of the invention is a method for producing a formulation containing ceramide, comprising the method steps: A) Melting a mixture containing at least one wax and at least one ceramide, B) Cooling the melted mixture to obtain a solidified melt containing the at least one wax and the at least one ceramide, C) Incorporating the solidified melt into a formulation containing oil. The invention also relates to the solidified melt of the aforementioned mixture.

Claims (30)

1. A method for preparing a ceramide-containing formulation comprising the method steps of

A) melting a mixture comprising a wax and a ceramide,

B) cooling the molten mixture to obtain a solidified melt comprising the wax and the ceramide, and

C) incorporating the solidified melt into an oil-containing formulation,

wherein the ratio by weight of the wax to the ceramide is from 50:1 to 1:1.

2. The method according to claim 1 , wherein the wax is selected from the group consisting of natural waxes of plant or animal origin, mineral waxes, fats, fatty alcohols, fatty acids, fatty esters, ethers of fatty alcohols, esters of polyethylene oxide and fatty acids, ethers of polyethylene oxide and fatty alcohols and partial glycerol esters.

3. The method according to claim 1 , wherein the ceramide is selected from the group comprising Ceramide NP, Ceramide AP, Ceramide EOP, Ceramide NDS, Ceramide ADS, Ceramide EODS, Ceramide NS, Ceramide AS, Ceramide EOS, Ceramide NH, Ceramide AH and Ceramide EOH.

4. The method according to claim 3 , wherein the ratio by weight of the wax to the ceramide in method step A) is from 9:1 to 4:1.

5. The method according to claim 1 , wherein the ratio by weight of the wax to the ceramide is from

20:1 to 2:1.

6. The method according to claim 1 , wherein the mixture in method step A) and the solidified melt in method step B), based on the total mixture and total melt respectively,

comprise from 70% by weight to 100% by weight, of the wax and the ceramide.

7. The method according to claim 1 , wherein the mixture in method step A) is melted at a temperature of 80° C. to 105° C.

8. The method according to claim 1 , wherein the oil-containing formulation in method step C) is an emulsion and the method steps comprise

C1) heating an oil phase comprising the solidified melt,

C2) heating an aqueous phase

C3) homogenizing the combined oil phase and aqueous phase with each other.

9. The method according to claim 8 , wherein in method step C1) and C2)

the phases are heated to a temperature of 60° C. to 89° C.

10. The method according to claim 8 , wherein at least one oil and at least one emulsifier are present in the oil phase.

11. The method according to claim 8 , wherein

the ratio by weight of oil phase to aqueous phase is from 1:100 to 1:1.

12. The method according to claim 8 , wherein in method step C1) and C2)

the phases are heated to a temperature of 65° C. to 79° C.

13. The method according to claim 8 , wherein

the ratio by weight of oil phase to aqueous phase is from 1:50 to 1:1.5.

14. The method according to claim 1 , wherein the ratio by weight of the wax to the ceramide is from 9:1 to 4:1.

15. The method according to claim 1 , wherein the mixture in method step A) and the solidified melt in method step B), based on the total mixture and total melt respectively, comprise from 81% by weight to 99% by weight of the wax and the ceramide.

16. The method according to claim 1 , wherein the mixture in method step A) is melted at a temperature of 85° C. to 99° C.

17. The method according to claim 1 , wherein the mixture in method step A) and the solidified melt in method step B), based on the total mixture and total melt respectively, comprise from 95% by weight to 98% by weight of the wax and the ceramide.

Assignments (2)
CHANGE OF NAME Recorded Dec 27, 2019
From: EVONIK DEGUSSA GMBH
To: EVONIK OPERATIONS GMBH
Reel/Frame 051428/0710 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 6, 2019
From: MACZKIEWITZ, URSULA; MECKING, MARIA; SCHRADER, ANNIKA
To: EVONIK DEGUSSA GMBH
Reel/Frame 050290/0730 →
Priority Claims (1)
EP 17163002 · Mar 27, 2017 · regional
Continuity (1)
Related Publication 20200246228A1 · Aug 6, 2020