IP Library Granted Patent US 11,434,545
Granted Patent B2
US 11,434,545 · App. 16/499,170 · Granted Sep 6, 2022

Lithium recovery method

Inventor: Junichi Arakawa (Tsuruga, JP)
Assignee: JX NIPPON MINING & METALS CORPORATION
C22B26/12C22B7/006C22B23/0453
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,434,545
App. No.
16/499,170
Granted
Sep 6, 2022
Kind
B2
Abstract

A method for recovering lithium according to this invention comprises separating sodium from a lithium-containing solution containing lithium ions and sodium ions to recover lithium, wherein the method comprises a solvent extraction step including: at least three-stage extraction process having a first extraction process, a second extraction process, and a third extraction process; and a lithium back extraction stage of back extracting the lithium ions from a solvent that have undergone the at least three-stage extraction process; and wherein, in the extraction process, the solvent undergoes the first extraction process, the second extraction process, and the third extraction process in this order, and a solution as the lithium-containing solution undergoes the respective processes in opposite order to the order of the solvent.

Claims (23)

1. A method for recovering lithium comprising separating sodium from a lithium-containing solution containing lithium ions and sodium ions, wherein the method comprises:

(A) a solvent extraction step including: at least three-stage extraction process including a first extraction process, a second extraction process, and a third extraction process; and

(B) a lithium back extraction process of back-extracting the lithium ions from a solvent that has undergone the at least three-stage extraction process;

wherein, in the at least three-stage extraction process, the solvent undergoes the first extraction process, the second extraction process, and the third extraction process in this order, and a solution of the lithium-containing solution undergoes the respective processes in opposite order to the order of the solvent, and

wherein a pH of a final extraction process in the at least three stage extraction process is from 3.5 to 4.5.

2. A method for recovering lithium comprising separating sodium from a lithium-containing solution containing lithium ions and sodium ions, wherein the method comprises:

(A) a solvent extraction step including: at least three-stage extraction process including a first extraction process, a second extraction process, and a third extraction process; and

(B) a lithium back extraction process of back-extracting the lithium ions from a solvent that has undergone the at least three-stage extraction process;

wherein, in the at least three-stage extraction process, the solvent undergoes the first extraction process, the second extraction process, and the third extraction process in this order, and a solution of the lithium-containing solution undergoes the respective processes in opposite order to the order of the solvent, and

wherein in the at least three stage extraction process, a pH of the first extraction process is from 6.0 to 6.5, and a pH of the at least three stage extraction process, except for the first extraction process and a final extraction process is from 5.5 to 6.0.

3. The method according to claim 1 or 2 , wherein the at least three stage extraction process comprises extracting the lithium ions and the sodium ions in the solution into the solvent during each of the extraction processes of the at least three stage extraction processes, except for a final extraction process, and back-extracting the sodium ions in the solvent into the solution in the final extraction process.

4. The method according to claim 1 or 2 , wherein a solvent after back-extracting the lithium ions in the lithium back extraction process is used as the solvent in the first extraction process.

5. The method according to claim 1 or 2 , wherein the lithium-containing solution has a pH of from 2.0 to 7.0.

6. The method according to claim 1 or 2 , wherein a molar ratio of a sodium concentration to a lithium concentration in the lithium-containing solution is from 2 to 100.

7. The method according to claim 1 or 2 , further comprising a nickel separation step of separating nickel from a solution containing lithium and nickel prior to the solvent extraction step, wherein the lithium-containing solution is obtained in the nickel separation step.

8. The method according to claim 7 , wherein nickel is separated by solvent extraction in the nickel separation step.

9. The method according to claim 8 , wherein a carboxylic acid-based extracting agent is used for the solvent extraction in the nickel separation step.

10. The method according to claim 1 or 2 ,

wherein the lithium-containing solution further contains nickel ions, and a back-extracted solution obtained in the lithium back-extraction process contains lithium ions and nickel ions, and

wherein the method further comprises, after the solvent extraction process, a neutralization step of neutralizing the back-extracted solution to remove nickel, and after the neutralization step, a carbonation step of obtaining lithium carbonate from a neutralized solution.

11. The method according to claim 1 or 2 , wherein the lithium-containing solution is obtained by processing lithium ion battery scrap.

12. The method according to claim 11 , wherein the processing to the lithium ion battery scrap comprises: a leaching step of leaching the lithium ion battery scrap; and

a recovery step of recovering metals dissolved in the resulting leached solution by solvent extraction.

Assignments (5)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 23, 2024
From: JX ADVANCED METALS CORPORATION
To: JX METALS CIRCULAR SOLUTIONS CO., LTD.
Reel/Frame 068665/0857 →
CHANGE OF NAME Recorded Jul 29, 2024
From: JX METALS CORPORATION
To: JX ADVANCED METALS CORPORATION
Reel/Frame 068179/0696 →
CHANGE OF NAME Recorded Jun 27, 2024
From: JX NIPPON MINING & METALS CORPORATION
To: JX METALS CORPORATION
Reel/Frame 068050/0527 →
CHANGE OF ADDRESS Recorded Jul 29, 2022
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 061005/0065 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 1, 2019
From: ARAKAWA, JUNICHI
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 050590/0758 →