High temperature fiber and method of making
Disclosed is a method of making high temperature fiber including incorporating an inorganic atom into a polymer precursor fiber to form a modified polymer precursor fiber and converting the modified polymer precursor fiber to a high temperature fiber having a bonded inorganic atom.
1. A method of making high temperature fiber comprising incorporating an inorganic species into a polymer precursor fiber to form a modified polymer precursor fiber and converting the modified polymer precursor fiber to a high temperature fiber having a bonded inorganic atom,
wherein the polymer precursor fiber comprises polycarbosilanes.
2. The method of claim 1 , wherein the bonded inorganic atom is bound to nitrogen, oxygen, silicon, boron, or carbon.
3. The method of claim 1 , wherein the inorganic atom comprises a lanthanide.
4. The method of claim 3 , wherein the bonded inorganic atom comprises a refractory metal bound to carbon.
5. The method of claim 1 , wherein the inorganic species is incorporated into the polymer precursor fiber by atomic layer deposition (ALD), molecular layer deposition (MLD), sequential vapor infiltration (SVI) or a combination thereof.
6. The method of claim 1 , wherein the polymer precursor fiber comprises an existing inorganic atom.
7. The method of claim 6 , wherein the inorganic species comprises an inorganic atom that is chemically different from the existing inorganic atom.
8. The method of claim 6 , wherein the inorganic species comprises an inorganic atom that is chemically the same as the existing inorganic atom.