IP Library Patent Application 16553352
Patent Application
App. No. 16/553,352

SOLIDIFICATION TECHNIQUES FOR LOW SOFTENING POINT PETROLEUM PITCH

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
16/553,352
Abstract

This alternative fuel is a reclaimed waste product which has a solid, particulate consistency at ambient temperature. The fuel comprises a composite of petroleum pitch and a powder coating. The powder coating penetrates into the surface of the pitch. The powder coating is recycled ash, pulverized coal, or pulverized petroleum coke.

Claims (18)

1 . A reclaimed waste product which has a solid, particulate consistency at ambient temperature comprising a composite of petroleum pitch and a powder coating.

2 . The product of claim 1 wherein the pitch is lower softening point petroleum pitch.

3 . The product of claim 1 wherein the pitch is solvent deasphalted (SDA) petroleum pitch.

4 . The product of claim 1 wherein the powder coating is pulverized coal.

5 . The product of claim 1 wherein the powder coating is recycled coal ash.

6 . The product of claim 1 wherein the powder coating penetrates the surface of the pitch.

7 . The product of claim 1 wherein the product is fuel.

8 . The product of claim 1 wherein the product is in the form of pastilles.

9 . The product of claim 1 wherein the product is in the form of briquets.

10 . A method for producing a reclaimed waste product which has a solid, particulate consistency at ambient temperature comprising the steps of:

cooling petroleum pitch;

coating the cooling pitch with a powder coating during the step of cooling; and

allowing the powder coating to penetrate more deeply into the pitch during the step of cooling.

11 . The method of claim 10 wherein the pitch is lower softening point petroleum pitch.

12 . The method of claim 10 wherein the pitch is solvent deasphalted (SDA) petroleum pitch.

13 . The method of claim 10 wherein the powder coating is pulverized coal.

14 . The method of claim 10 wherein the powder coating is recycled coal ash.

15 . The method of claim 10 wherein the powder coating penetrates the surface of the pitch.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 28, 2019
From: NICHOLSON, JEFFREY ALLEN
To: MARATHON PETROLEUM COMPANY LP
Reel/Frame 050196/0049 →