IP Library Granted Patent US 11,261,331
Granted Patent B2
US 11,261,331 · App. 16/688,308 · Granted Mar 1, 2022

Natural rubber skim block in asphalt compositions and non-asphalt solvent-based coatings

Inventors: Rodney G. Armstrong, III (Cuyahoga Falls, OH); Christopher D. Shepherd (Brecksville, OH); Tom Marsh (Sarasota, FL)
Assignee: Corrie Maccoll North America
C08L95/00C09D195/00C08L2201/56C08L2205/03C08L2205/08C08L2555/74C08L2555/84
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,261,331
App. No.
16/688,308
Granted
Mar 1, 2022
Kind
B2
Abstract

A skim block composition includes a carrier mixed with a skim block addition, the skim block addition including from 0 to less than 100 wt % synthetic polymer, and from greater than 0 to 100% skim block. This provides productive use for the typical waste product skim block, which is the neutralized and coagulated product of skim latex formed during the production of natural rubber latex concentrate by centrifugation.

Claims (65)

1. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

from zero to less than 100 weight % synthetic polymer, and

from greater than zero to 100 weight % skim block;

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation, and wherein the skim block is characterized by a weight average molecular weight (Mw) of from about 250,000 to about 450,000.

2. The skim block composition of claim 1 , wherein the skim block addition includes from zero to about 98 weight % synthetic polymer and from about 2 to 100 weight % skim block.

3. The skim block composition of claim 1 , comprising from zero to about 95 weight % synthetic polymer and from about 5 to 100 weight % skim block.

4. The skim block composition of claim 1 , wherein the skim block addition includes from zero to about 50 weight % synthetic polymer and from about 50 to 100 weight % skim block.

5. The skim block composition of claim 1 , devoid of synthetic polymer.

6. The skim block composition of claim 1 , wherein the skim block is characterized by having a Mooney viscosity (ML1+4) of from about 25 to about 45.

7. The skim block composition of claim 6 , wherein the skim block is characterized by having a solution viscosity of from about 3,000 to about 7,000 cPs.

8. The skim block composition of claim 1 , wherein the carrier is asphalt.

9. The skim block composition of claim 8 , wherein the skim block composition is selected from aggregate binders, hot applied asphalt joint and crack sealants, solvent-based asphalt coatings, asphalt based roofing materials, and asphalt cutback adhesives.

10. The skim block composition of claim 9 , wherein the skim block composition is an aggregate binder including from about 2 to about 6 weight % skim block addition and from about 94 to about 98 weight % asphalt.

11. The skim block composition of claim 9 , wherein the skim block composition is a solvent-based asphalt coating including from about 5 to about 15 weight % skim block addition and from about 50 to about 65 weight % asphalt.

12. The skim block composition of claim 9 , wherein the skim block composition is an asphalt cutback adhesive including from about 5 to about 15 weight % skim block addition, from about 25 to about 65 weight % asphalt.

13. The skim block composition of claim 9 , wherein the skim block composition is a hot applied asphalt and roofing material including from about 5 to about 15 weight % skim block addition and from about 50 to about 70 weight % asphalt.

14. The skim block composition of claim 1 , wherein the skim block composition is a hot applied asphalt joint and crack sealant including skim block and synthetic polymer at a weight ratio of from about 2:3 to about 2:5.

15. The skim block composition of claim 1 , wherein the skim block composition is a hot applied asphalt joint and crack sealant having about 55 to about 65 weight % asphalt, from about 4 to about 6 weight % skim block, and from about 8 to about 12 weight % synthetic polymer.

16. The skim block composition of claim 1 , wherein the skim block composition is a hot applied asphalt joint and crack sealant including about 60 weight % asphalt, about 12 weight % extender oil, about 10 weight % synthetic polymer, about 5 weight % skim block, about 1 weight % adhesion promoter, and about 12 weight % inorganic fillers.

17. The skim block composition of claim 1 , wherein the carrier is solvent, the skim block composition is devoid of asphalt, and the skim block composition is a non-asphalt solvent based coating including from about 5 to about 40 weight % skim block addition and from about 20 to about 60 weight % solvent.

18. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

from zero to less than 100 weight % synthetic polymer, and

from greater than zero to 100 weight % skim block; and

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation, and wherein the skim block is characterized by having a Mooney viscosity (ML1+4) of from about 25 to about 45.

19. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

from zero to less than 100 weight % synthetic polymer, and

from greater than zero to 100 weight % skim block; and

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation, and wherein the skim block is characterized by having a solution viscosity of from about 3,000 to about 7,000 cPs.

20. The skim block composition of claim 19 , wherein the skim block is characterized by a weight average molecular weight (Mw) of from about 250,000 to about 450,000.

21. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

from greater than zero to less than 100 weight % synthetic polymer, and

from greater than zero to 100 weight % skim block; and

wherein the synthetic polymer is selected from linear, branched, or coupled polymers including one or more of polydienes or polydiene copolymers with non-diene comonomers and wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation.

22. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

from zero to less than 100 weight % synthetic polymer, and

from greater than zero to 100 weight % skim block;

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation;

wherein the carrier is asphalt; and

wherein the skim block composition is a hot applied asphalt joint and crack sealant including skim block and synthetic polymer at a weight ratio of from about 2:3 to about 2:5.

23. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

synthetic polymer, and

skim block;

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation;

wherein the carrier is asphalt; and

wherein the skim block composition is a hot applied asphalt joint and crack sealant having about 55 to about 65 weight % asphalt, from about 4 to about 6 weight % skim block, and from about 8 to about 12 weight % synthetic polymer.

24. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

synthetic polymer, and

skim block;

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation;

wherein the carrier is asphalt; and

wherein the skim block composition is a hot applied asphalt joint and crack sealant including about 55 to about 65 weight % asphalt, from about 10 to about 14 weight % extender oil, from zero to about 2 weight % wax, from about 8 to about 12 weight % synthetic polymer, from about 4 to about 6 weight % skim block, from about 0.5 to about 1.5 weight % adhesion promoter, and from about 10 to about 14 weight % inorganic fillers.

25. A skim block composition comprising:

a carrier mixed with a skim block addition, the skim block addition including:

synthetic polymer, and

skim block;

wherein the skim block is formed as the neutralized and coagulated product of skim latex during the production of natural rubber latex concentrate by centrifugation;

wherein the carrier is asphalt; and

wherein the skim block composition is a hot applied asphalt joint and crack sealant including about 60 weight % asphalt, about 12 weight % extender oil, about 10 weight % synthetic polymer, about 5 weight % skim block, about 1 weight % adhesion promoter, and about 12 weight % inorganic fillers.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 19, 2019
From: ARMSTRONG, RODNEY G., III; SHEPHERD, CHRISTOPHER D.; MARSH, TOM
To: CORRIE MACCOLL NORTH AMERICA
Reel/Frame 051052/0752 →
Continuity (1)
Related Publication 20210147687A1 · May 20, 2021