Internal cooling circuits for CMC and method of manufacture
A method for forming a ceramic matrix composite (CMC) component with an internal cooling channel includes forming a first fiber member, forming a first depression in a surface of the first fiber member, covering the first depression with a second fiber member to form a near-net shape fiber preform of a component with an internal channel defined in part by the first depression, and densifying the fiber preform.
1. A method for forming a ceramic matrix composite (CMC) component with an internal cooling channel, the method comprising:
forming a first fiber member;
forming a first depression in a surface of the first fiber member by applying a force to the first fiber member with a shaped tool comprising a protrusion matching a shape of the first depression;
maintaining a shape of the first depression by at least one of:
applying a binder material to the first fiber member;
stitching the first fiber member with a fiber tow; and
passing a barbed needle through the first fiber member;
covering the first depression with a second fiber member to form a near-net shape fiber preform of a component with an open internal channel defined in part by the first depression; and
densifying the fiber preform.
2. The method of claim 1 and further comprising forming a second depression in a surface of the second fiber member, and wherein covering the first depression with the second fiber member comprises aligning the first depression with the second depression.
3. The method of claim 1 and further comprising forming a second depression in a surface of the second fiber member, and wherein covering the first depression with the second fiber member comprises offsetting the first depression from the second depression.
4. The method of claim 1 , wherein the first and second fiber members each comprise a plurality of fiber plies and wherein forming the first depression causes ends of the plurality of fiber plies to be displaced inward toward the first depression, and wherein ends are constrained from moving during densification.
5. The method of claim 1 and further comprising increasing a bond between the first and second fiber members, wherein increasing the bond comprises applying material between contacting surfaces of the first and second fiber members, the material selected from a group consisting of: chopped fibers, a pre-ceramic polymer adhesive, and combinations thereof.
6. The method of claim 1 , wherein forming the first fiber member comprises reducing an amount of fiber tows in a region of the first depression such that a region adjacent to the first depression has a greater amount of fiber tows than under the first depression.
7. The method of claim 1 , wherein forming the first fiber member comprises providing additional or larger fiber tows on either side of a location of the first depression.
8. The method of claim 7 , wherein the additional fiber tows have a larger diameter than a plurality of fiber tows disposed under the first depression.
9. The method of claim 7 , wherein the additional fiber tows are braided or twisted fiber tows.
10. The method of claim 1 , wherein maintaining the shape of the first depression includes stitching the first fiber member with a fiber tow.
11. The method of claim 1 , wherein maintaining the shape of the first depression includes passing a barbed needle through the first fiber member.
12. A method for forming a ceramic matrix composite (CMC) component with an internal cooling channel, the method comprising:
forming a first fiber member, wherein the first fiber member is a prepreg;
forming a first depression in a surface of the first fiber member, wherein forming the depression comprises:
providing additional or larger fiber tows on either side of a location of the first depression; and
pressing the first fiber member with a roller having a protrusion in a shape of the first depression that presses between the additional or larger fiber tows;
covering the first depression with a second fiber member to form a near-net shape fiber preform of a component with an internal channel defined in part by the first depression; and
densifying the fiber preform.
13. The method of claim 12 , wherein the additional fiber tows have a larger diameter than a plurality of fiber tows disposed under the first depression.
14. The method of claim 12 , wherein the additional fiber tows are braided or twisted fiber tows.
15. A method for forming a ceramic matrix composite (CMC) component with an internal cooling channel, the method comprising:
forming a first fiber member, wherein forming the first fiber member comprises:
braiding fiber tows on a mandrel; and
forming helical protrusions, wherein a first depression is formed between the helical protrusions;
forming a first depression in a surface of the first fiber member;
covering the first depression with a second fiber member to form a near-net shape fiber preform of a component with an internal channel defined in part by the first depression; and
densifying the fiber preform.
16. The method of claim 15 , and further comprising rotating the mandrel to control positions of the helical protrusions.
17. The method of claim 15 , wherein forming the first depression comprises applying a force to an area between the helical protrusions with a shaped tool comprising a protrusion matching a shape of the first depression.
18. The method of claim 15 , wherein forming the first fiber member comprises braiding the fiber tows on a mandrel, wherein at least one of an axial fiber site or a biased fiber site comprises additional or larger fiber tows.