IP Library Granted Patent US 11,365,357
Granted Patent B2
US 11,365,357 · App. 16/881,035 · Granted Jun 21, 2022

Cracking C

Inventors: Daryl Bitting (Longview, TX); Kenny Randolph Parker (Afton, TN); Michael Gary Polasek (Longview, TX); David Eugene Slivensky (Tatum, TX); Xianchun Wu (Longview, TX); Jerome Leonard Stavinoha, Jr. (Longview, TX)
Assignee: Eastman Chemical Company
C10G9/36C10B53/07C10G2300/1037C10G2300/1096C10G2400/02C10G2400/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,365,357
App. No.
16/881,035
Granted
Jun 21, 2022
Kind
B2
Abstract

A hydrocarbon cracker stream is combined with recycle content pyrolysis oil to form a combined cracker stream and the combined cracker stream is cracked in a cracker furnace to provide an olefin-containing effluent. The r-pyoil can be fed to the cracker feed. Alternatively, the r-pyoil with a predominantly c8+ fraction can be fed to the cracker feed. The furnace can be a gas fed furnace, or split cracker furnace.

Claims (22)

1. A cracker feedstock composition comprising a recycle content pyrolysis oil composition (r-pyoil), wherein said r-pyoil has a C 8+ content of at least 35 weight percent, based on the total weight of said r-pyoil; wherein said r-pyoil comprises not more than 30 weight percent total aromatics, based on the total weight of said r-pyoil.

2. The composition of claim 1 , wherein at least 1 weight percent of said r-pyoil is obtained from the pyrolysis of recycled waste.

3. The composition of claim 1 , wherein not more than 95 weight percent of said r-pyoil is obtained from the pyrolysis of recycled waste.

4. The composition of claim 3 , wherein said recycled waste comprises recycled waste plastic.

5. The composition of claim 3 , wherein said recycled waste comprises waste plastics, waste textiles, waste carpet fibers, waste modified cellulose, waste biomass, post-industrial waste streams, intermediate industrial waste streams, or combinations thereof.

6. The composition of claim 5 , wherein at least a portion of said r-pyoil is obtained from the pyrolysis of waste plastic.

7. The composition of claim 1 , wherein said cracker feedstock has not been hydrotreated.

8. The composition of claim 7 , wherein said r-pyoil is present in said cracker feedstock in an amount of not more than 40 weight percent and at least about 1 weight percent.

9. The composition of claim 8 , wherein said cracker feedstock composition comprises at least 60 weight percent and not more than 99 weight percent of non-recycle C 2 to C 4 hydrocarbons.

10. The composition of claim 1 , wherein said cracker feedstock composition comprises at least 60 weight percent and not more than 95 weight percent of non-recycle C 5 to C 22 hydrocarbons.

11. The composition of claim 1 , wherein said cracker feedstock composition comprises at least 60 weight percent and not more than 95 weight percent of non-recycle propane, ethane, or combinations thereof.

12. The composition of claim 1 , wherein said cracker feedstock comprises predominantly propane and ethane.

13. The composition of claim 12 , wherein said cracker feedstock has a 90% boiling point of not more than 360° C. and at least 200° C.

14. The composition of claim 13 , wherein said cracker feedstock has a total C 15+ content of not more than 25 weight percent, based on the total weight of the composition.

15. The composition of claim 14 , wherein said cracker feedstock has a total C 15+ content of at least 0.5 weight percent, based on the total weight of the composition.

16. The composition of claim 15 , wherein said r-pyoil comprises not more than 25 weight percent total aromatics, based on the total weight of said r-pyoil.

17. The composition of claim 16 , wherein said r-pyoil comprises at least 1 weight percent of total aromatics, based on the total weight of said r-pyoil.

18. The composition of claim 1 , wherein said r-pyoil comprises at least 15 weight percent and not more than 80 weight percent of paraffins, based on the total weight of said r-pyoil.

19. A method of making one or more olefins, said method comprising:

(a) introducing a cracker feed stream comprising a recycle content pyrolysis oil composition (r-pyoil) into a cracker furnace, wherein said r-pyoil introduced into said cracker furnace has a C 8+ content of at least 35% by weight, based on the total weight of the r-pyoil; wherein said r-pyoil comprises not more than 30 weight percent total aromatics, based on the total weight of said r-pyoil; and

(b) cracking said cracker feed stream in said cracker furnace to thereby form a cracked olefin-containing effluent stream.

20. The method of claim 19 , wherein at least a portion of said r-pyoil is obtained from the pyrolysis of waste plastic.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 20, 2025
From: EASTMAN CHEMICAL COMPANY
To: EXXONMOBIL PRODUCT SOLUTIONS COMPANY
Reel/Frame 073142/0954 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 26, 2021
From: BITTING, DARYL; PARKER, KENNY RANDOLPH; POLASEK, MICHAEL GARY; SLIVENSKY, DAVID EUGENE; WU, XIANCHUN; STAVINOHA, JEROME LEONARD, JR
To: EASTMAN CHEMICAL COMPANY
Reel/Frame 055727/0340 →
Continuity (2)
Provisional Application 62852359 · May 24, 2019
Related Publication 20210363432A1 · Nov 25, 2021
Cited By (12)
US 12,227,710 US 12,410,370 US 12,435,278 US 12,453,993 US 12,453,994 US 12,473,506 US 12,509,636 US 12,545,840 US 12,577,188 US 12,595,424 US 12,630,769 US 12,649,879