Heating system for fiber-reinforced thermoplastic feedstock and workpiece

Inventors: Zachary Aaron August (Santa Clara, CA); Hemant Bheda (Saratoga, CA); Leonid Michael Treyger (Orlando, FL)
Assignee: Arevo, Inc.
B29C64/141B23K26/0093B23K26/034B23K26/0608B23K26/0626B23K26/0652B23K26/0876B23K26/1464B23K26/342B29C64/393B33Y10/00B33Y50/02B33Y70/00B23K26/0006B29K2101/12B29K2307/04B33Y30/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,312,068
App. No.
16/889,830
Granted
Apr 26, 2022
Kind
B2
Abstract

An additive manufacturing system is disclosed that comprises two or more lasers for precisely heating a fiber-reinforced thermoplastic feedstock and a fiber-reinforced thermoplastic workpiece in preparation for depositing and tamping the feedstock onto the workpiece. The system employs feedforward, a variety of sensors, and feedback to ensure that the feedstock and workpiece are properly heated.

Claims (109)

1. A method for additive manufacturing, the method comprising:

irradiating and heating:

(i) a first segment of a feedstock with a first average power during a first time-interval, and

(ii) a second segment of the feedstock with a second average power during a second time-interval, wherein the second time-interval is after, and is mutually exclusive of, the first time-interval,

with a first laser beam generated by a first laser;

irradiating and heating:

(i) a first portion of a workpiece with a third average power during a third time-interval, and

(ii) a second portion of the workpiece with a fourth average power during a fourth time-interval, wherein the fourth time-interval is after, and is mutually exclusive of, the third time-interval,

with a second laser beam generated by a second laser;

tamping:

(i) the first segment of the feedstock onto the first portion of the workpiece during a fifth time-interval, wherein the fifth time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the fifth time-interval is after, and is mutually exclusive of, the third time-interval, and

(ii) the second segment of the feedstock onto the second portion of the workpiece during a sixth time-interval, wherein the sixth time-interval is after, and is mutually exclusive of, the second time-interval, and wherein the sixth time-interval is after, and is mutually exclusive of, the fourth time-interval,

with a tamping tool;

depositing the feedstock onto the workpiece at a non-uniform rate; and

directing the first laser to generate the first laser beam with the first average power during the first time-interval based on:

(i) a thermal model of the feedstock, and

(ii) a prediction of the interval between the first time-interval and the third time-interval.

2. The method of claim 1 further comprising:

measuring a temperature of the second segment of the feedstock in the first time-interval; and

directing the first laser to generate the first laser beam with the second average power during the second time-interval based on the temperature.

3. The method of claim 1 further comprising:

measuring a temperature of the second segment of the feedstock in the second time-interval; and

directing the first laser to generate the first laser beam with the second average power during the second time-interval based on the temperature.

4. The method of claim 1 further comprising:

measuring a temperature of the first segment of the feedstock in the second time-interval; and

directing the first laser to generate the first laser beam with the second average power during the second time-interval based on the temperature.

5. The method of claim 1 further comprising:

measuring a temperature of the second segment of the feedstock in the first time-interval; and

adjusting the length of feedstock being irradiated by the first laser beam based on the temperature.

6. The method of claim 1 further comprising:

measuring a temperature of the second segment of the feedstock in the second time-interval; and

adjusting the length of feedstock being irradiated by the first laser beam based on the temperature.

7. The method of claim 1 further comprising:

measuring a temperature of the first segment of the feedstock in the second time-interval; and

adjusting the length of feedstock being irradiated by the first laser beam based on the temperature.

8. A method for additive manufacturing, the method comprising:

irradiating and heating:

(i) a first segment of a feedstock with a first average power during a first time-interval, and

(ii) a second segment of the feedstock with a second average power during a second time-interval, wherein the second time-interval is after, and is mutually exclusive of, the first time-interval,

with a first laser beam generated by a first laser;

irradiating and heating:

(i) a first portion of a workpiece with a third average power during a third time-interval, and

(ii) a second portion of the workpiece with a fourth average power during a fourth time-interval, wherein the fourth time-interval is after, and is mutually exclusive of, the third time-interval,

with a second laser beam generated by a second laser;

tamping:

(i) the first segment of the feedstock onto the first portion of the workpiece during a fifth time-interval, wherein the fifth time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the fifth time-interval is after, and is mutually exclusive of, the third time-interval, and

(ii) the second segment of the feedstock onto the second portion of the workpiece during a sixth time-interval, wherein the sixth time-interval is after, and is mutually exclusive of, the second time-interval, and wherein the sixth time-interval is after, and is mutually exclusive of, the fourth time-interval,

with a tamping tool;

depositing the feedstock onto the workpiece at a non-uniform rate; and

directing the second laser to generate the second laser beam with the third average power during the third time-interval based on:

(i) a thermal model of the workpiece, and

(ii) a prediction of the interval between the third time-interval and the fifth time-interval.

9. The method of claim 8 further comprising:

measuring a temperature of the second portion of the workpiece in the third time-interval; and

directing the second laser to generate the second laser beam with the fourth average power during the fourth time-interval based on the temperature.

10. The method of claim 8 further comprising:

measuring a temperature of the second portion of the workpiece in the fourth time-interval; and

directing the second laser to generate the second laser beam with the fourth average power during the fourth time-interval based on the temperature.

11. The method of claim 8 further comprising:

measuring a temperature of the first portion of the workpiece in the fourth time-interval; and

directing the second laser to generate the second laser beam with the fourth average power during the fourth time-interval based on the temperature.

12. The method of claim 8 further comprising:

measuring a temperature of the second portion of the workpiece in the fourth time-interval; and

adjusting the distance between a pinch line segment on the tamping tool and the second laser beam based on the temperature.

13. The method of claim 8 further comprising:

measuring a temperature of the first portion of the workpiece in the fourth time-interval; and

adjusting the distance between a pinch line segment on the tamping tool and the second laser beam based on the temperature.

14. The method of claim 8 further comprising:

measuring a temperature of the second portion of the workpiece in the third time-interval; and

adjusting the angle of incidence of the second laser beam on the workpiece based on the temperature.

15. The method of claim 8 further comprising:

measuring a temperature of the second portion of the workpiece in the fourth time-interval; and

adjusting the angle of incidence of the second laser beam on the workpiece based on the temperature.

16. The method of claim 8 further comprising:

measuring a temperature of the first portion of the workpiece in the fourth time-interval; and

adjusting the angle of incidence of the second laser beam on the workpiece based on the temperature.

17. A method for additive manufacturing, the method comprising:

irradiating and heating:

(i) a first segment of a feedstock with a first average power during a first time-interval, and

(ii) a second segment of the feedstock with a second average power during a second time-interval, wherein the second time-interval is after, and is mutually exclusive of, the first time-interval,

with a first laser beam generated by a first laser;

irradiating and heating:

(i) a first portion of a workpiece with a third average power during a third time-interval, and

(ii) a second portion of the workpiece with a fourth average power during a fourth time-interval, wherein the fourth time-interval is after, and is mutually exclusive of, the third time-interval,

with a second laser beam generated by a second laser;

tamping:

(i) the first segment of the feedstock onto the first portion of the workpiece during a fifth time-interval, wherein the fifth time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the fifth time-interval is after, and is mutually exclusive of, the third time-interval, and

(ii) the second segment of the feedstock onto the second portion of the workpiece during a sixth time-interval, wherein the sixth time-interval is after, and is mutually exclusive of, the second time-interval, and wherein the sixth time-interval is after, and is mutually exclusive of, the fourth time-interval,

with a tamping tool; and

steering the second laser beam on the workpiece with an optical instrument based on a location of the deposition path on the workpiece.

18. The method of claim 17 :

wherein the first laser beam is characterized by a first wavelength;

wherein the second laser beam is characterized by a second wavelength; and

wherein the first wavelength does not equal the second wavelength; and further comprising:

a first optical beam splitter for receiving a spatial combination of the first laser beam and the second laser beam and for spatially separating the first laser beam and the second laser beam.

19. A method for additive manufacturing, the method comprising:

irradiating and heating:

(i) a first segment of a feedstock with a first average power during a first time-interval, and

(ii) a second segment of the feedstock with a second average power during a second time-interval, wherein the second time-interval is after, and is mutually exclusive of, the first time-interval,

with a first laser beam generated by a first laser;

irradiating and heating:

(i) a first portion of a workpiece with a third average power during a third time-interval, and

(ii) a second portion of the workpiece with a fourth average power during a fourth time-interval, wherein the fourth time-interval is after, and is mutually exclusive of, the third time-interval,

with a second laser beam generated by a second laser;

tamping:

(i) the first segment of the feedstock onto the first portion of the workpiece during a fifth time-interval, wherein the fifth time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the fifth time-interval is after, and is mutually exclusive of, the third time-interval, and

(ii) the second segment of the feedstock onto the second portion of the workpiece during a sixth time-interval, wherein the sixth time-interval is after, and is mutually exclusive of, the second time-interval, and wherein the sixth time-interval is after, and is mutually exclusive of, the fourth time-interval,

with a tamping tool; and

adjusting the length of workpiece being irradiated by the second laser beam based on a temperature of the workpiece.

Assignments (4)
RELEASE OF SECURITY INTEREST Recorded Sep 20, 2023
From: MCGEARY CUKOR LLC
To: AREVO INC
Reel/Frame 064959/0783 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 18, 2023
From: AREVO, INC.
To: STRATASYS, INC.
Reel/Frame 064942/0384 →
SECURITY INTEREST Recorded Aug 31, 2023
From: AREVO, INC
To: MCGEARY CUKOR LLC
Reel/Frame 064789/0954 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 4, 2020
From: AUGUST, ZACHARY AARON; BHEDA, HEMANT; TREYGER, LEONID MICHAEL
To: AREVO, INC.
Reel/Frame 052831/0777 →
Continuity (4)
Continuation In Part 16690765 · Nov 21, 2019
Provisional Application 63029172 · May 22, 2020
Provisional Application 63025109 · May 14, 2020