Heating system for fiber-reinforced thermoplastic feedstock and workpiece
An additive manufacturing system is disclosed that comprises two or more lasers for precisely heating a fiber-reinforced thermoplastic feedstock and a fiber-reinforced thermoplastic workpiece in preparation for depositing and tamping the feedstock onto the workpiece. The system employs feedforward, a variety of sensors, and feedback to ensure that the feedstock and workpiece are properly heated.
1. A method for additive manufacturing, the method comprising:
irradiating and heating a first segment of a feedstock with a first laser beam from a first laser during a first time-interval, wherein the first laser beam is characterized by a first average power during the first time-interval;
irradiating and heating a portion of a workpiece with a second laser beam from a second laser during a second time-interval, wherein the second laser beam is characterized by a second average power during the second time-interval;
tamping the first segment of feedstock onto the portion of the workpiece during a third time-interval, wherein the third time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the third time interval is after, and mutually exclusive of, the second time-interval;
depositing the feedstock onto the workpiece at a non-uniform rate; and
directing the first laser to generate the first laser beam with the first average power during the first time-interval based on:
(i) a thermal model of the feedstock, and
(ii) a prediction of the interval between the first time-interval and the third time-interval.
2. The method of claim 1 further comprising:
measuring a temperature of a second segment of the feedstock in the first time-interval; and
directing the first laser to generate the first laser beam with the first average power during the first time-interval based on the temperature.
3. The method of claim 1 further comprising:
measuring a temperature of a second segment of the feedstock in the first time-interval; and
adjusting the length of feedstock being irradiated by the first laser beam based on the temperature.
4. The method of claim 1 further comprising:
measuring a temperature of a second segment of the feedstock in the first time-interval; and
adjusting the distance between a pinch line segment on the tamping tool and the first laser beam based on the temperature.
5. The method of claim 1 further comprising:
measuring a temperature of a second segment of the feedstock in the first time-interval; and
adjusting the irradiance of the first laser beam in at least one unit-area based on the temperature.
6. The method of claim 1 further comprising:
measuring a temperature of a second segment of the feedstock in the first time-interval; and
adjusting the angle of incidence of the first laser beam on the feedstock based on the temperature.
7. A method for additive manufacturing, the method comprising:
irradiating and heating a segment of a feedstock with a first laser beam from a first laser during a first time-interval, wherein the first laser beam is characterized by a first average power during the first time-interval;
irradiating and heating a first portion of a workpiece with a second laser beam from a second laser during a second time-interval, wherein the second laser beam is characterized by a second average power during the second time-interval;
tamping the segment of feedstock onto the first portion of the workpiece during a third time-interval, wherein the third time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the third time interval is after, and mutually exclusive of, the second time-interval; and
directing the second laser to generate the second laser beam with the second average power during the second time-interval based on:
(i) a thermal model of the workpiece, and
(ii) a prediction of the interval between the second time-interval and the third time-interval.
8. The method of claim 7 further comprising:
measuring a temperature of a second portion of the workpiece in the second time-interval; and
directing the second laser to generate the second laser beam with the second average power during the second time-interval based on the temperature.
9. The method of claim 7 further comprising:
measuring a temperature of a second portion of the workpiece in the second time-interval; and
adjusting a linear dimension of the first portion based on the temperature.
10. The method of claim 7 further comprising:
measuring a temperature of a second portion of the workpiece in the second time-interval; and
adjusting a distance between a pinch line portion on the tamping tool and the second laser beam based on the temperature.
11. The method of claim 7 further comprising:
measuring a temperature of a second portion of the workpiece in the second time-interval; and
adjusting the irradiance of the second laser beam in at least one unit-area based on the temperature.
12. The method of claim 7 further comprising:
measuring a temperature of a second portion of the workpiece in the second time-interval; and
adjusting the angle of incidence of the second laser beam on the workpiece based on the temperature.
13. The method of claim 7 further comprising:
adjusting the angle of incidence of the second laser beam on the workpiece based on the contour of the workpiece in the first portion of the workpiece.
14. A method for additive manufacturing, the method comprising:
irradiating and heating a segment of a feedstock with a first laser beam from a first laser during a first time-interval, wherein the first laser beam is characterized by a first average power during the first time-interval;
irradiating and heating a portion of a workpiece with a second laser beam from a second laser during a second time-interval, wherein the second laser beam is characterized by a second average power during the second time-interval;
tamping the segment of feedstock onto the portion of the workpiece during a third time-interval, wherein the third time-interval is after, and is mutually exclusive of, the first time-interval, and wherein the third time interval is after, and mutually exclusive of, the second time-interval; and
steering the second laser beam on the workpiece with an active optical instrument based on a location of the deposition path on the workpiece.
15. The method of claim 14 :
wherein the first laser beam is characterized by a first wavelength;
wherein the second laser beam is characterized by a second wavelength; and
wherein the first wavelength equals the second wavelength.
16. The method of claim 14 :
wherein the first laser beam is characterized by a first wavelength;
wherein the second laser beam is characterized by a second wavelength; and
wherein the first wavelength does not equal the second wavelength.
17. The method of claim 14 :
wherein the first laser beam is characterized by a first wavelength;
wherein the second laser beam is characterized by a second wavelength; and
wherein the first wavelength does not equal the second wavelength; and further comprising:
a first optical beam splitter for receiving a spatial combination of the first laser beam and the second laser beam and for spatially separating the first laser beam and the second laser beam.
18. The method of claim 14 wherein the tamping tool is performed with a roller.
19. The method of claim 14 wherein the feedstock is a fiber-reinforced thermoplastic tape.