IP Library Granted Patent US 11,072,739
Granted Patent B2
US 11,072,739 · App. 16/963,115 · Granted Jul 27, 2021

Composition and method for improving performance of friction reducing polymers in high dissolved solids water

Inventors: David O. Trahan (Lafayette, LA); Jia Li (Lafayette, LA)
Assignee: Downhole Chemical Solutions, LLC
C09K8/882C09K8/602C09K8/665C09K8/68C09K8/845C09K2208/28
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,072,739
App. No.
16/963,115
Granted
Jul 27, 2021
Kind
B2
Abstract

Systems and methods include using a fracture fluid downhole for fracturing a formation. The method includes providing an aqueous solution comprising dissolved solids at a certain ionic strength, and adding a proppant to create a fracture fluid. The method continues by adding a polymeric additive and a surfactant to the fracture fluid, wherein the polymeric additive comprises friction reducing capabilities that can be decreased by the ionic strength present in the fracture fluid (i.e., ionic strength originally found in the water). The addition of the polymeric additive and the surfactant to the fracture fluid creates an enhanced fracture fluid, wherein the surfactant increases the performance of the friction reducing capabilities of the polymeric additive in the enhanced fracture fluid, which provides a more efficient fracturing operation. The method concludes by pumping the enhanced fracture fluid downhole for a more efficient fracture of the formation.

Claims (20)

1. A method of using a fracture fluid downhole for fracturing a formation, comprising:

storing water in a pump tank, wherein the water comprises dissolved solids at an ionic strength;

adding a proppant to the stored water to create the fracture fluid;

adding a water-soluble polymeric additive and a surfactant to create an enhanced fracture fluid, wherein the polymeric additive comprises friction reducing capabilities that are decreased by the ionic strength of the stored water, and wherein the surfactant comprises sodium lauryl ether sulfate and sodium dodecyl sulfate at a ratio between 2:1 and 1:2, and wherein the surfactant is concentrated in the enhanced fracture fluid between 60 ppm and 500 ppm; and

pumping the enhanced fracture fluid with the water-soluble polymeric additive and the surfactant into the formation for fracturing the formation.

2. The method of claim 1 , wherein the water-soluble polymeric additive comprises an anionic polyacrylamide.

3. The method of claim 1 , wherein the surfactant further comprises a carboxylate surfactant, a sulfonate surfactant, a sophorolipid surfactant or combinations thereof.

4. The method of claim 3 , wherein the sulfonate surfactant is concentrated in the enhanced fracture fluid between 30 ppm and 100 ppm.

5. The method of claim 3 , wherein the sophorolipid surfactant is concentrated in the enhanced fracture fluid between 10 ppm and 50 ppm.

6. A method of fracturing a formation, comprising:

pumping produced water from a wellbore, wherein the produced water comprises an ionic strength that is greater than fresh water;

adding a proppant to the produced water to create a fracture fluid;

adding a water-soluble polymeric additive and a surfactant comprising sodium lauryl ether sulfate and sodium dodecyl sulfate at a ratio between 2:1 and 1:2 to the fracture fluid to create an enhanced fracture fluid, wherein the water-soluble polymeric additive comprises friction reducing capabilities that are decreased by the ionic strength of the produced water, and wherein the surfactant is added at a concentration between 60 ppm and 500 ppm to increase friction reducing capabilities of the water-soluble polymeric additive in the enhanced fracture fluid; and

pumping the enhanced fracture fluid into the formation for fracturing the formation.

7. The method of claim 6 , wherein the wellbore providing the produced water is located adjacent to the formation being fractured.

8. The method of claim 6 , wherein the wellbore providing the produced water is located within a 100 m distance of the formation being fractured.

9. The method of claim 6 , wherein the water-soluble polymeric additive comprises an anionic polyacrylamide.

10. The method of claim 6 , wherein the surfactant further comprises a carboxylate surfactant, a sulfonate surfactant, a sophorolipid surfactant or combinations thereof.

11. The method of claim 10 , wherein the sulfonate surfactant is concentrated in the enhanced fracture fluid between 30 ppm and 100 ppm.

12. The method of claim 10 , wherein the sophorolipid surfactant is concentrated in the enhanced fracture fluid between 10 ppm and 50 ppm.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 18, 2020
From: LI, JIA
To: DOWNHOLE CHEMICAL SOLUTIONS, LLC
Reel/Frame 054408/0272 →
Continuity (2)
Provisional Application 62619591 · Jan 19, 2018
Related Publication 20200399531A1 · Dec 24, 2020