IP Library Granted Patent US 12,195,351
Granted Patent B2
US 12,195,351 · App. 16/979,021 · Granted Jan 14, 2025

Molybdenum oxychloride or tungsten oxychloride and production method thereof

Inventor: Hideyuki Takahashi (Ibaraki, JP)
Assignee: JX ADVANCED METALS CORPORATION
C01G41/00C01G39/00C01P2006/82
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,195,351
App. No.
16/979,021
Granted
Jan 14, 2025
Kind
B2
Abstract

A molybdenum oxychloride or a tungsten oxychloride, wherein the molybdenum oxychloride or the tungsten oxychloride has a moisture content of less than 1 wt %. A method of producing a molybdenum oxychloride or a tungsten oxychloride, wherein a molybdenum oxide or a tungsten oxide as a raw material is subject to dehydration treatment at 400° C. or higher and 800° C. or less, and the raw material that underwent dehydration treatment is thereafter reacted with a chlorine gas to synthesize a molybdenum oxychloride or a tungsten oxychloride. An object of the present invention is to provide a molybdenum oxychloride or a tungsten oxychloride having a low moisture content, as well as a production method thereof.

Claims (2)

1. A method of producing a molybdenum oxychloride or a tungsten oxychloride, wherein a molybdenum oxide or a tungsten oxide as a raw material is subject to dehydration treatment at 400° C. or higher and 800° C. or less while flowing inert gas, or inert gas mixed with oxygen, or air (O 2 +N 2 ), wherein the dehydration treatment time is set to be 3 hours or longer, and the raw material that underwent dehydration treatment is thereafter reacted with a chlorine gas to synthesize a molybdenum oxychloride or a tungsten oxychloride.

2. The method of producing a molybdenum oxychloride or a tungsten oxychloride according to claim 1 , wherein the dehydration treatment is at a temperature of 500° C. or higher and 750° C. or less.

Assignments (3)
CHANGE OF NAME Recorded Jul 31, 2024
From: JX METALS CORPORATION
To: JX ADVANCED METALS CORPORATION
Reel/Frame 068237/0944 →
CHANGE OF NAME Recorded Oct 12, 2023
From: JX NIPPON MINING & METALS CORPORATION
To: JX METALS CORPORATION
Reel/Frame 065221/0471 →