Treated geothermal brine compositions with reduced concentration of silica, iron and lithium
This invention relates to treated geothermal brine compositions containing reduced concentrations of lithium, iron and silica compared to the untreated brines. Exemplary compositions contain concentration of lithium ranges from 0 to 200 mg/kg, concentration of silica ranges from 0 to 30 mg/kg, concentration of iron ranges from 0 to 300 mg/kg. Exemplary compositions also contain reduced concentrations of elements like arsenic, barium, and lead.
1. A treated geothermal brine composition comprising a treated geothermal brine comprising lithium, silica, iron, boron, barium, and strontium having a concentration of lithium of no more than 200 mg/kg, a concentration of silica of no more than 10 mg/kg, and a concentration of iron of no more than 20 mg/kg.
2. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 150 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of boron is no more than 544 mg/kg.
3. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 150 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of boron is from 100 mg/kg to 544 mg/kg.
4. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of barium is no more than 250 mg/kg.
5. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of barium is no more than 100 mg/kg.
6. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 10 mg/kg, and the concentration of barium is no more than 250 mg/kg.
7. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 15 mg/kg, the concentration of iron is less than 10 mg/kg, and the concentration of barium is no more than 250 mg/kg.
8. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 15 mg/kg, the concentration of iron is less than 10 mg/kg, and the concentration of strontium is no more than 681 mg/kg.
9. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 10 mg/kg, and the concentration of strontium is no more than 681 mg/kg.
10. The treated geothermal brine composition of claim 1 , wherein the concentration of lithium is no more than 200 mg/kg, the concentration of silica is no more than the concentration of iron is less than 10 mg/kg, and the concentration of strontium is no more than 520 mg/kg.
11. The treated geothermal brine composition of claim 1 , further comprising a concentration of sodium ranging from 40,000 to 80,000 mg/kg, a concentration of calcium ranging from 30,000 to 46,000 mg/kg, and a concentration of potassium ranging from 10,000 to 26,000 mg/kg.
12. The treated geothermal brine composition of claim 1 , wherein the treated geothermal brine is a Salton Sea brine.
13. A method of using a treated geothermal brine composition, the method comprising extracting one or more minerals from the composition of claim 1 .
14. A method of using a treated geothermal brine composition, the method comprising a step of injecting the composition of claim 1 into a geothermal reservoir.
15. A treated geothermal brine composition comprising a treated geothermal brine comprising lithium, silica, iron, boron, barium, and strontium, and having a concentration of lithium of no more than 150 mg/kg, a concentration of silica of no more than 10 mg/kg, and a concentration of iron of no more than 20 mg/kg, wherein the treated geothermal brine is a Salton Sea brine.
16. The treated geothermal brine composition of claim 15 , wherein the concentration of lithium is no more than 150 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of boron is no more than 544 mg/kg.
17. The treated geothermal brine composition of claim 15 , wherein the concentration of lithium is no more than 150 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of boron is from 100 mg/l to 544 mg/kg.
18. The treated geothermal brine composition of claim 15 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of barium is no more than 250 mg/kg.
19. The treated geothermal brine composition of claim 15 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 20 mg/kg, and the concentration of barium is no more than 100 mg/kg.
20. The treated geothermal brine composition of claim 15 , wherein the concentration of lithium is no more than 50 mg/kg, the concentration of iron is less than 10 mg/kg, and the concentration of barium is no more than 250 mg/kg.