IP Library Granted Patent US 12,008,745
Granted Patent B2
US 12,008,745 · App. 17/116,539 · Granted Jun 11, 2024

System and methods for printing defect detection

Inventors: George Hudelson (Billerica, MA); Matthew McCambridge (Burlington, MA); Jake Dec (Burlington, MA); Alexander Legendre (Boston, MA)
Assignee: Desktop Metal, Inc.
G06T7/0004B22F1/10B22F3/105B33Y50/02B22F10/85B22F2203/00B33Y10/00G06T7/001G06T2207/30144
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,008,745
App. No.
17/116,539
Granted
Jun 11, 2024
Kind
B2
Abstract

An additive manufacturing method includes depositing a first amount of metal powder onto a powder bed of a printing system, spreading the first amount of metal powder across the powder bed to form a first layer, and depositing a first amount of binder material on the first layer. The additive manufacturing method also includes exposing the first layer to a first lighting condition, imaging the first layer under the first lighting condition to generate a first image, analyzing the first image of the first layer, and determining whether to adjust at least one printing parameter based on the analyzing.

Claims (37)

1. A method of detecting and ameliorating defects during metal additive manufacturing, comprising the steps of:

spreading a metal powder on a powder bed of a metal additive manufacturing system and depositing a predetermined pattern of binder to the metal powder to form a layer of a green part;

illuminating the layer of the green part with a first light source;

capturing via an imaging device a first image of the illuminated layer of the green part;

analyzing the first image and identifying a first defect in the layer of the green part, wherein the first defect is one of a blister, a divot, beading, a smear and a jet-out condition;

and adjusting at least one printing parameter in response to identifying the first defect to ameliorate the first defect.

2. The method of claim 1 wherein an axis of the first light source is angled with respect to the powder bed by 1 degree to 10 degrees.

3. The method of claim 1 wherein an axis of the first light source is angled with respect to the powder bed by 70 degree to 110 degrees.

4. The method of claim 1 wherein the step of analyzing includes identifying at least one shadow in the first image.

5. The method of claim 1 , wherein the step of analyzing includes identifying at least one region that is brighter than an average brightness of the layer of the green part.

6. The method of claim 1 wherein the step of analyzing includes detecting a bright spot and an associated shadow.

7. The method of claim 1 wherein step of analyzing includes detecting at least one of a region of missing binder material, a bright region and a shadow in the first image.

8. The method of claim 1 wherein the printing parameter is one of a vapor deposition rate, a binder deposition rate, and a negative feature pattern.

9. The method of claim 1 , further comprising the steps of, illuminating the layer of the green part with a second light source;

capturing via a second imaging device a second image of the illuminated layer of the green part;

analyzing the second image and identifying a second defect in the layer of the green part; and

adjusting at least one printing parameter in response to identifying the second defect to ameliorate the second defect.

10. A method of detecting defects during metal additive manufacturing, comprising the steps of:

spreading a metal powder on a powder bed of a metal additive manufacturing system and depositing a predetermined pattern of binder to the metal powder to form a layer of a green part;

generating a first illumination condition and capturing a first image of the illuminated layer of the green part with a first imaging device;

generating a second illumination condition and capturing a second image of the illuminated layer of the green part with a second imaging device; and

comparing the first image and second image to at least one of each other, a design file and a third image and identifying a first defect in the layer of the green part, wherein the defect is one of a blister, a divot, a smear, beading and a jet-out condition.

11. The method of claim 10 wherein an axis of the first light source is angled with respect to the powder bed by 1 degree to 10 degrees.

12. The method of claim 11 wherein an axis of the second light source is angled with respect to the powder bed by 70 degree to 110 degrees.

13. The method of claim 10 wherein the step of analyzing includes identifying at least one shadow in one of the first image and second image.

14. The method of claim 10 , wherein the step of analyzing includes identifying at least one region that is brighter than an average brightness of the layer of the green part.

15. The method of claim 10 wherein the step of analyzing includes detecting a bright spot and an associated shadow.

16. The method of claim 10 wherein step of analyzing includes detecting at least one of a region of missing binder material, a bright region and a shadow in one of the first image and the second image.

17. The method of claim 10 further comprising adjusting at least one printing parameter in response to identifying the first defect, wherein the printing parameter is one of a vapor deposition rate, a binder deposition rate, and a negative feature pattern.

18. The method of claim 10 wherein the third image is an image of a preceding layer in the green part.

19. A method of identifying and clearing clogged jetting orifices in a binder jetting metal additive manufacturing system, comprising the steps of:

spreading from a printhead a metal powder on a powder bed of a metal additive manufacturing system and depositing a predetermined pattern of binder to the metal powder to form a layer of a green part;

illuminating the layer of the green part with a high angle light source;

capturing an image of the illuminated layer of the green part with an imaging device;

identifying areas of unbound powder according to the brightness an amount of reflected light;

comparing the areas of unbound powder to a design file and identifying a defect indicating a jet-out condition; and

subjecting the printhead to a maintenance cycle.

Assignments (3)
SECURITY INTEREST Recorded Apr 24, 2026
From: ARC IMPACT ACQUISITION CORPORATION
To: IRON HORSE CREDIT LLC
Reel/Frame 075458/0351 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 9, 2024
From: HUDELSON, GEORGE; MCCAMBRIDGE, MATTHEW; DEC, JAKE; LEGENDRE, ALEXANDER
To: DESKTOP METAL, INC.
Reel/Frame 067355/0929 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 27, 2021
From: HUDELSON, GEORGE; MCCAMBRIDGE, MATTHEW; DEC, JAKE; LEGENDRE, ALEXANDER
To: DESKTOP METAL, INC.
Reel/Frame 056377/0786 →
Continuity (2)
Provisional Application 62945359 · Dec 9, 2019
Related Publication 20210170483A1 · Jun 10, 2021