Nonwoven fabric for increasing the availability of chlorine in solution
Wipes for preventing chlorine depletion suitable for commercial applications (e.g., industrial and consumer disinfectant wipes) are provided. The wipe includes at least one nonwoven layer, at least one pulp layer, and a nonionic modified siloxane additive. The at least one nonwoven layer and the at least one pulp layer may be hydroentangled to form a hydroentangled nonwoven fabric having a first surface and a second surface. Additionally, the nonionic modified siloxane additive may be disposed on at least one of the first surface or the second surface.
1. A method for producing a wipe, comprising:
(a) hydroentangling (i) a first nonwoven layer comprising a first group of continuous filaments, (ii) a second nonwoven layer comprising a second group of continuous filaments, (iii) a third nonwoven layer comprising acrylic staple fibers, and (iv) at least one pulp layer together to form a hydroentangled nonwoven fabric having a first surface and a second surface; wherein the at least one pulp player is disposed directly between the third nonwoven layer and the second nonwoven layer and the third nonwoven layer is disposed directly between the first nonwoven layer and the at least one pulp layer; and
(b) applying a nonionic siloxane additive onto at least one of the first surface or the second surface;
wherein the hydroentangled nonwoven fabric is devoid of meltblown fibers.
2. The method according to claim 1 , further comprising:
(c) positioning the first surface of the hydroentangled nonwoven fabric directly or indirectly onto an image transfer device having a three-dimensional pattern; and
(d) applying jets of fluid directly or indirectly to the second surface of the hydroentangled nonwoven fabric to impart a three-dimensional pattern onto the hydroentangled nonwoven fabric.
3. The method according to claim 1 , wherein the step of applying the nonionic siloxane additive onto at least one of the first surface or the second surface comprises applying the nonionic siloxane additive via one or more of a spray nozzle, a foam applicator, a pad, or a kiss roll.
4. The method according to claim 1 , wherein the first nonwoven layer comprises a first spunbond layer and the second nonwoven layer comprises a second spunbond layer.
5. The method of claim 1 , wherein the first group of continuous filaments comprise a polyolefin.
6. The method of claim 1 , wherein the second group of continuous filaments comprise synthetic polymer filaments.
7. The method of claim 6 , wherein the synthetic polymer filaments comprise at least one of a polyolefin, a polyester, a polyamide, or any combination thereof.
8. The method of claim 7 , wherein the synthetic polymer filaments comprise a polypropylene.
9. The method of claim 7 , wherein the synthetic polymer filaments have a denier comprising from 0.5 to 3.
10. The method of claim 1 , wherein the pulp of the at least one pulp layer comprises organic pulp, synthetic pulp, or any combination thereof.
11. The method of claim 1 , wherein the hydroentangled nonwoven fabric comprises from 30-70 wt % of a polyolefin and from 30-70 wt % of a cellulosic pulp.
12. The method of claim 1 , wherein the hydroentangled nonwoven fabric has a basis weight comprising from 10 to 80 gsm.
13. The method of claim 1 , wherein the nonionic siloxane additive comprises a nonionic polyoxyalkyl-modified polydimethyl siloxane additive and has a basis weight comprising from 0.1 to 3 gsm.
14. The method of claim 1 , wherein the nonionic siloxane additive is hydrophilic.
15. The method of claim 1 , wherein the wipe maintains a substantially constant chlorine concentration in a disinfectant solution when the wipe is disposed therein.
16. The method of claim 15 , wherein the substantially constant chlorine concentration in the disinfectant solution is defined as a less than a 10% reduction over a four hour time period.
17. The method of claim 1 , wherein the hydroentangled nonwoven fabric comprises a three-dimensional pattern imaged onto the first surface and the second surface.
18. The method of claim 1 , wherein the hydroentangled nonwoven fabric comprises from 55-70 wt % of pulp.
19. The method of claim 1 , wherein the third nonwoven layer has a basis weight from 0.5 to 15 gsm and the at least one pulp layer has a basis weight from 10 to 30 gsm.
20. The method of claim 1 , wherein the nonionic siloxane additive comprises a polyoxyalkyl-modified polydimethyl siloxane additive.