Flocculant composition and method of forming same

Inventor: Jess Ornum (Andover, NJ)
Assignee: KOMLINE-SANDERSON CORPORATION
B01D21/01C02F5/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,826,676
App. No.
17/406,476
Granted
Nov 28, 2023
Kind
B2
Abstract

According to some embodiments, a flocculated material, product and method for making the product are provided including providing a methanotrophic material having an amount of 2.68% Total Suspended Solids (TSS); treating the methanotrophic material with phosphoric acid; providing a lime solution in an amount of 0.0212 M; combining the treated methanotrophic material with the lime to increase a pH of the solution and to precipitate calcium phosphate; generating a flocculated material by flocculating the combined lime and treated methanotrophic material. Numerous other aspects are provided.

Claims (26)

1. A method comprising:

providing a methanotrophic material having an amount of 2.68% Total Suspended Solids (TSS);

treating the methanotrophic material with phosphoric acid;

providing a lime solution in an amount of 0.0212 M;

combining the treated methanotrophic material with the lime to increase a pH of the solution and to precipitate calcium phosphate;

generating a flocculated material by flocculating the combined lime and treated methanotrophic material.

2. The method of claim 1 , wherein the ratio of treated methanotrophic material to lime is about 83 to 1.

3. The method of claim 1 , wherein the flocculation is alkaline flocculation.

4. The method of claim 1 , wherein the methanotrophic material is provided in a medium.

5. The method of claim 4 , further comprising:

deliquoring the flocculated material from the medium.

6. The method of claim 5 , further comprising:

drying the deliquored flocculated material at a temperature of 60 degrees Celsius via a vacuum.

7. The method of claim 6 , wherein the drying is via an indirect dryer.

8. The method of claim 7 , wherein the dried deliquored flocculated material is anti-fouling.

9. The method of claim 1 , wherein the treated methanotrophic material has a pH of 4.5 and the flocculated material has a pH of 8.5-9.

10. A flocculated material comprising a methanotrophic material having an amount of 2.65% TSS suspended in a medium, the methanotrophic material including a dose of phosphoric acid, wherein the methanotrophic material is adapted to flocculate in lime, wherein the lime is in an amount of 0.0212M.

11. The flocculated material of claim 10 wherein the treated methanotrophic material has a pH of 4.5 and the flocculated material has a pH of 8.5-9.

12. The flocculated material of claim 10 , wherein the flocculated material is anti-fouling.

13. A product prepared by:

mixing a methanotrophic material with a medium to form a first mixture, wherein the methanotrophic material in the first mixture is present in a concentration of 1-3% TSS, wherein the methanotrophic material is treated with phosphoric acid prior to mixing;

adding a lime solution to the first mixture to form a second mixture, wherein a ratio of the first mixture to the lime solution is about 83 to 1; and

flocculating the second mixture to form a plurality of flocs, wherein the flocs are a product.

14. The product of claim 13 , wherein the flocked material is deliquored and dried at 60 degrees Celsius temperature until a dryness level is about 95% Total Solids (TS).

15. The product of claim 13 , wherein the methanotrophic material is provided in an amount of one to two grams, and the medium is provided in an amount of 98-99 grams.

16. The product of claim 13 , wherein the methanotrophic material is present in a concentration of 2.65% TSS.

Assignments (2)
SECURITY INTEREST Recorded Sep 6, 2024
From: KOMLINE-SANDERSON CORPORATION; AQUASHIELD, INC.
To: JPMORGAN CHASE BANK, N.A., AS AGENT
Reel/Frame 068513/0227 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 19, 2021
From: ORNUM, JESS
To: KOMLINE-SANDERSON CORPORATION
Reel/Frame 057229/0940 →