Method for injecting strand-blocked cable
A method for rejuvenating a strand-blocked cable having a conductor comprised of a plurality of conductor strands with interstitial volume therebetween blocked by a PIB based strand-block mastic, the conductor being surrounded by a polymeric cable insulation. The method including pre-injection of compressed gas into the conductor strands of the cable at a pressure less than the elastic limit of the cable insulation, and injection of a rejuvenation fluid into the conductor strands of the cable at a pressure less than the elastic limit of the cable insulation.
1. A method for rejuvenating a strand-blocked cable, comprising:
a. positioning a longitudinally strand-blocked cable having a conductor comprised of a plurality of conductor strands with interstitial volume therebetween longitudinally blocked by a polyisobutylene (PIB) based strand-block mastic and surrounded by a polymeric cable insulation to receive injection of a compressed carbon dioxide gas into the interstitial volume of the strand-blocked cable at a first cable location along the strand-blocked cable;
b. next, injecting the compressed gas into the interstitial volume of the strand-blocked cable at a pressure that opens a continuous flow path along a length of the strand-blocked cable extending between the first cable location and a longitudinally separated second cable location along the strand-blocked cable and expand the continuous flow path by altering the physical properties and/or structure of the PIB based strand-block mastic through which a rejuvenation fluid can be injected to treat the strand-blocked cable, the pressure being less than the elastic limit of the cable insulation;
c. after the continuous flow path is formed by the injection of the compressed gas, depressurizing at least a portion of the strand-blocked cable; and
d. after depressurizing the portion of the strand-blocked cable, injecting the rejuvenation fluid into the conductor strands of the strand-blocked cable along the continuous flow path at a pressure less than the elastic limit of the cable insulation.
2. The method of claim 1 , where the injection of the compressed gas forms the continuous flow path along the entire length of the strand-blocked cable and the depressurizing depressurizes the entire length of the strand-blocked cable.
3. The method of claim 1 , where a receiving end of the strand-blocked cable is closed off to pressurize the entire length of the strand-blocked cable before depressurizing the portion of the cable.
4. The method of claim 3 , where the receiving end of the strand-blocked cable is closed off to pressurize the entire length of the strand-blocked cable for at least 1 minute before depressurizing the portion of the strand-blocked cable.
5. The method of claim 3 , where the receiving end of the strand-blocked cable is closed off and the entire length of strand-blocked cable is pressurized to at least 200 psi and then the portion of the strand-blocked cable is depressurized.
6. The method of claim 3 , where the injection of compressed gas is at a pressure sufficient to expand the PIB based strand-block mastic by at least 20% and preferably more than 200% after pressurization and depressurization.
7. The method of claim 3 , where the injection of compressed gas is at a pressure sufficient to reduce the density of the PIB based strand-block mastic of at least 10% after 30 minutes following pressurization and depressurization.
8. The method of claim 3 , where the injection of compressed gas is at a pressure sufficient to reduce the hardness of the PIB based strand-block mastic by about 20% after 30 minutes following pressurization and depressurization.
9. The method of claim 3 , where the injection of compressed gas is at a pressure sufficient to reduce the viscosity of the PIB based strand-block mastic by slope-magnitude of about 40%.
10. The method of claim 1 , where the conductor temperature is about 40° C. over ambient during the injection of compressed gas.
11. The method of claim 1 , where the conductor temperature is reduced to below 30° C. during the injection of the rejuvenation fluid.
12. The method of claim 1 , where the rejuvenation fluid is comprised primarily from dialkoxysilanes mixed with a hydrolosysis-condensation catalyst.
13. The method of claim 12 , where the rejuvenation fluid is comprised primarily of a mixture of tolylethylmethyldimethoxysilane (TEM) and cyanobutylmethyldimethoxysilane (CBM).
14. The method of claim 12 , where the hydrolysis-condensation catalyst is selected from a list of dodecylbenzene sulfonic acid (DDBSA) and tetra-isopropyl titanate (TiPT).
15. A method for rejuvenating a strand-blocked cable, comprising:
a. positioning a longitudinally strand-blocked cable having a conductor comprised of a plurality of conductor strands with interstitial volume therebetween longitudinally blocked by a polyisobutylene (PIB) based strand-block mastic and surrounded by a polymeric cable insulation to receive injection of a compressed carbon dioxide gas into the interstitial volume of the strand-blocked cable;
b. next, injecting the compressed gas into the interstitial volume of the strand-blocked cable at a pressure that opens a continuous flow path along a length of the strand-blocked cable by altering the physical properties and/or structure of the PIB based strand-block mastic through which a rejuvenation fluid can be injected to treat the strand-blocked cable, the pressure being less than the elastic limit of the cable insulation;
c. after the continuous flow path is formed by the injection of the compressed gas, depressurizing at least a portion of the strand-blocked cable;
d. repeating steps b and c at least one additional time to expand the continuous flow path by further altering the physical properties and/or structure of the PIB based strand-block mastic through which a rejuvenation fluid can be injected to treat the strand-blocked cable, the pressure being less than the elastic limit of the cable insulation; and
e. after repeating steps b and c at least one additional time, injecting the rejuvenation fluid into the conductor strands of the strand-blocked cable along the continuous flow path at a pressure less than the elastic limit of the cable insulation.
16. A method for rejuvenating a strand-blocked cable, comprising:
a. positioning a longitudinally strand-blocked cable having a conductor comprised of a plurality of conductor strands with interstitial volume therebetween longitudinally blocked by a polyisobutylene (PIB) based strand-block mastic and surrounded by a polymeric cable insulation to receive injection of a compressed carbon dioxide gas into the interstitial volume of the strand-blocked cable;
b. next, injecting the compressed gas into the interstitial volume of the strand-blocked cable at a pressure that opens a continuous flow path along the entire length of the strand-blocked cable and expand the continuous flow path by altering the physical properties and/or structure of the PIB based strand-block mastic through which a rejuvenation fluid can be injected to treat the strand-blocked cable, the pressure being less than the elastic limit of the cable insulation;
c. after the continuous flow path is formed by the injection of the compressed gas, depressurizing the entire length of the strand-blocked cable; and
d. after depressurizing the entire length of the strand-blocked cable, injecting the rejuvenation fluid into the conductor strands of the strand-blocked cable along the continuous flow path at a pressure less than the elastic limit of the cable insulation.
17. The method of claim 16 , where steps b and c are performed at least one additional time before performing step d.