Abstract

A method for treating battery waste includes: a first heat treatment step of heating the battery waste in an atmosphere containing at least one selected from the group consisting of nitrogen, carbon dioxide and water vapor; and after the first heat treatment step, a second heat treatment step of changing the atmosphere in the first heat treatment step and heating the battery waste in an atmosphere which is different from the atmosphere in the first heat treatment step and which contains a larger amount of oxygen than that in the first heat treatment step.

Claims (14)

1 . A method for treating battery waste, comprising:

a first heat treatment step of heating the battery waste in an atmosphere comprising at least one selected from the group consisting of nitrogen, carbon dioxide and water vapor; and

after the first heat treatment step, a second heat treatment step of changing the atmosphere in the first heat treatment step and heating the battery waste in an atmosphere which is different from the atmosphere in the first heat treatment step and which comprises a larger amount of oxygen than that in the first heat treatment step.

2 . The method for treating battery waste according to claim 1 , wherein the first heat treatment step and the second heat treatment step are continuously carried out in the same heat treatment furnace.

3 . The method for treating battery waste according to claim 1 , wherein a heating time in the second heat treatment step is 10% to 90% of a total of a time for retaining a highest temperature in the first heat treatment step and a time for retaining a highest temperature in the second heat treatment step.

4 . The method for treating battery waste according to claim 1 , wherein the second heat treatment step is carried out in an atmosphere containing 1.0% by volume or more of oxygen.

5 . The method for treating battery waste according to claim 1 , wherein the atmosphere in the second heat treatment step is an air atmosphere.

6 . The method for treating battery waste according to claim 1 , wherein the atmosphere in the first heat treatment step comprises oxygen.

7 . The method for treating battery waste according to claim 6 , wherein in the first heat treatment step, an oxygen partial pressure of the atmosphere is retained in a range of 5× 10 −4 atm to 4×10 −2 atm.

8 . The method for treating battery waste according to claim 6 , wherein, when heating the battery waste in the first heat treatment step, an atmospheric gas comprising oxygen and at least one selected from the group consisting of nitrogen, carbon dioxide and water vapor is allowed to flow in the heat treatment furnace.

9 . The method for treating battery waste according to claim 1 , wherein in the first heat treatment step, the highest temperature of the battery waste during heating is 400° C. to 800° C.

10 . The method for treating battery waste according to claim 1 , wherein in the second heat treatment step, the highest temperature of the battery waste during heating is 400° C. to 800° C.

11 . The method for treating battery waste according to claim 1 , wherein the battery waste is vehicle battery pack waste comprising a case forming an exterior and a vehicle battery module surrounded by the case, or vehicle battery module waste.

12 . The method for treating battery waste according to claim 1 , wherein the battery waste comprises a lithium ion battery.

Assignments (4)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 23, 2024
From: JX ADVANCED METALS CORPORATION
To: JX METALS CIRCULAR SOLUTIONS CO., LTD.
Reel/Frame 068665/0857 →
CHANGE OF NAME Recorded Jul 29, 2024
From: JX METALS CORPORATION
To: JX ADVANCED METALS CORPORATION
Reel/Frame 068179/0696 →
CHANGE OF NAME Recorded Jun 27, 2024
From: JX NIPPON MINING & METALS CORPORATION
To: JX METALS CORPORATION
Reel/Frame 068050/0527 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 8, 2022
From: MIYANAGA, HIROSHI; HAGA, YASUFUMI
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 060743/0025 →