Composite scaffold for the repair, reconstruction, and regeneration of soft tissues
A composite scaffold having a highly porous interior with increased surface area and void volume is surrounded by a flexible support structure that substantially maintains its three-dimensional shape under tension and provides mechanical reinforcement during repair or reconstruction of soft tissue while simultaneously facilitating regeneration of functional tissue.
1. A method of making a composite scaffold comprising:
A) constructing a three-dimensional support structure by knitting a scaffold comprising first and second layers spaced apart to define an interior space therebetween but attached together by a plurality of spacer elements extending through the interior space, the support structure extending along a length dimension between first and second ends thereof; and
B) forming a microporous matrix within the interior space, the microporous matrix having a multitude of interconnected pores in fluid communication with exterior surfaces of the support structure,
wherein a plurality of the interconnected pores are oriented relative to a dimensional characteristics of the support structure.
2. The method of claim 1 wherein the plurality of interconnected pores are oriented radially inward into the interior space from exterior surfaces of the support structure.
3. The method of claim 1 wherein the plurality of interconnected pores are oriented towards the length dimension of the support structure.
4. The method of claim 1 wherein the support structure has an exterior profile and B) comprises:
B1) disposing the support structure into a solution filled mold having a cross-sectional profile which at least partially mimics the exterior profile of the support structure, and
B2) changing the temperature of the mold to cause crystallization of the solution within the interior space of the support structure.
5. The method of claim 1 further comprising:
C) at least partially covering the support structure with a hydrophilic substance.
6. The method of claim 5 wherein at least partially covering the three-dimensional support structure with a hydrophilic substance occurs before disposing a microporous matrix within the interior space.
7. The method of claim 5 wherein the hydrophilic substance at least partially comprises polyethylene glycol (PEG).
8. The method of claim 1 wherein the microporous matrix comprises one of collagen and hydrogel.
9. The method of claim 1 wherein the support structure comprises a scaffold comprises any combination of synthetic bioresorbable polymers, natural polymers and/or additives.
10. The method of claim 9 wherein the scaffold comprises monofilament, multifilament, or multifilament and textured yarns, or any combination thereof, knitted into a three-dimensional structure.
11. The method of claim 1 wherein the microporous matrix comprises any of a sponge, foam, or textured fibers or yarns, or any combination thereof.
12. The method of claim 1 wherein the microporous matrix comprises any of a freeze-dried sponge, open cell extrusion foam, particulate leached sponge, or any combination thereof.
13. The method of claim 1 wherein B) comprises forming the microporous matrix by any of lyophilization, particulate leaching, open cell extrusion, solvent casting, solid-state foaming, and cross-linking.