IP Library Granted Patent US 12,629,753
Granted Patent B2
US 12,629,753 · App. 18/022,326 · Granted May 19, 2026

Copper powder, and method for manufacturing copper powder

Inventor: Kazuhiro Moriwaki (Ibaraki, JP)
Assignee: JX Advanced Metals Corporation
B22F9/24B22F1/056B22F9/04H01B1/02B22F2009/044B22F2301/10B22F2304/058B22F2998/10
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,629,753
App. No.
18/022,326
Granted
May 19, 2026
Kind
B2
Abstract

A copper powder containing copper particulates, wherein the copper powder has a number of particles with a particle size of 1.5 μm or more of 10000 or less per 10 ml of a solution, as measured in the solution using an in-liquid particle counter, the solution having a copper ion concentration of 10 g/L and being obtained by dissolving the copper particulates of the copper powder in nitric acid.

Claims (7)

1 . A copper powder comprising copper particulates, wherein the copper powder has a number of particles with a particle size of 1.5 μm or more of 50 or more and 10000 or less per 10 mL of a solution, as measured in the solution using an in-liquid particle counter, the solution having a copper ion concentration of 10 g/L and being obtained by dissolving the copper particulates of the copper powder in nitric acid, and wherein the particles are particles with a particle size of 1.5 μm or more that remain undissolved in the solution.

2 . The copper powder according to claim 1 , wherein the number of particles is 7000 or less per 10 mL.

3 . A method for manufacturing a copper powder comprising copper particulates, the method comprising the following steps in order:

filtering at least one of raw material solutions through a filter, wherein the filter has a collection efficiency of 95% or more for particles having a particle size of 10 μm, and wherein the at least one of the raw material solutions includes at least one of an aqueous copper salt solution, an aqueous alkaline solution, and an aqueous reducing agent solution;

obtaining a slurry containing copper particulates from the at least one of the raw material solutions; and

washing the slurry with a washing liquid filtered through a filter having a collection efficiency of 95% or more for particles having a particle size of 10 μm.

4 . The method according to claim 3 , further comprising the steps of: obtaining a slurry containing cuprous oxide particulates from the at least one of the raw material solutions.

Assignments (3)
CHANGE OF NAME Recorded Apr 17, 2025
From: JX METALS CORPORATION
To: JX ADVANCED METALS CORPORATION
Reel/Frame 070887/0151 →
CHANGE OF NAME Recorded Apr 15, 2025
From: JX NIPPON MINING & METALS CORPORATION
To: JX METALS CORPORATION
Reel/Frame 070850/0835 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 14, 2023
From: MORIWAKI, KAZUHIRO
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 062980/0777 →