IP Library Granted Patent US 12,586,792
Granted Patent B2
US 12,586,792 · App. 18/198,844 · Granted Mar 24, 2026

Negative electrode plate and preparation method therefor, secondary battery, battery module, battery pack and power consuming device

Inventors: Xihui Wang (Ningde, CN); Wenzhu Xu (Ningde, CN); Xiaoming Ge (Ningde, CN)
Assignee: CONTEMPORARY AMPEREX TECHNOLOGY (HONG KONG) LIMITED
H01M4/583H01M4/0416H01M4/386H01M4/387H01M4/485H01M10/0525H01M10/0562H01M2004/021H01M2004/027H01M2220/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,586,792
App. No.
18/198,844
Granted
Mar 24, 2026
Kind
B2
Abstract

A negative electrode plate may comprise a negative electrode current collector and a negative electrode film layer provided on at least one surface of the negative electrode current collector; the negative electrode film layer may comprise a first region and a second region along the width direction, the first region may not comprise a solid electrolyte, while the second region may comprise a solid electrolyte.

Claims (26)

1 . A negative electrode plate, comprising a negative electrode current collector and a negative electrode film layer provided on at least one surface of the negative electrode current collector; wherein the negative electrode film layer comprises a first region and a second region along a width direction of the negative electrode film layer, the first region does not comprise a solid electrolyte, and the second region comprises a solid electrolyte, wherein both the first region and the second region comprise a negative electrode active material.

2 . The negative electrode plate according to claim 1 , wherein the first region comprises a first film layer region and a second film layer region along the width direction of the negative electrode film layer, and the second region is located between the first film layer region and the second film layer region; a width of the negative electrode film layer is denoted as L, a width of the first film layer region is denoted as L 1 , a width of the second region is denoted as L 2 , and a width of the second film layer region is denoted as L 3 .

3 . The negative electrode plate according to claim 2 , wherein 0<L 1 /L≤0.75.

4 . The negative electrode plate according to claim 2 , wherein 0<L 3 /L≤0.75.

5 . The negative electrode plate according to claim 2 , wherein 0<L 2 /L≤0.75.

6 . The negative electrode plate according to claim 2 , wherein L 1 =L 3 .

7 . The negative electrode plate according to claim 2 , wherein L 1 =L 2 =L 3 .

8 . The negative electrode plate according to claim 1 , wherein a mass percentage of the solid electrolyte in the second region is greater than 0 and not greater than 30%.

9 . The negative electrode plate according to claim 1 , wherein the solid electrolyte comprises at least one selected from the group consisting of oxide solid electrolyte, sulfide solid electrolyte and polymer solid electrolyte.

10 . The negative electrode plate according to claim 1 , wherein

the negative electrode active material in the first region and the second region each independently comprises at least one selected from the group consisting of artificial graphite, natural graphite, soft carbon, hard carbon, a silicon-based material, a tin-based material and lithium titanate.

11 . The negative electrode plate according to claim 1 , wherein the first region has a porosity of ≥24%.

12 . The negative electrode plate according to claim 1 , wherein the second region has a porosity of ≥20%.

13 . A secondary battery, comprising the negative electrode plate according to claim 1 .

14 . A power consuming device, comprising the secondary battery according to claim 13 .

15 . A method for preparing a negative electrode plate, comprising the steps of:

dividing at least one surface of the negative electrode current collector into a first section and a second section along a width direction of the negative electrode current collector;

providing a first negative electrode slurry and a second negative electrode slurry, wherein the first negative electrode slurry does not comprise a solid electrolyte, and the second negative electrode slurry comprises a solid electrolyte; and

coating the first section with the first negative electrode slurry, and coating the second section with the second negative electrode slurry,

wherein both the first region and the second region comprise a negative electrode active material.

16 . The method according to claim 15 , further comprising: dividing the first section into a first portion and a second portion along the width direction of the negative electrode current collector, and the second section is located between the first portion and the second portion.

17 . The method according to claim 15 , wherein a ratio of a width of the first portion to a width of the negative electrode current collector is greater than 0 and not greater than 0.75.

18 . The method according to claim 15 , wherein a ratio of a width of the second portion to a width of the negative electrode current collector is greater than 0 and not greater than 0.75, and/or

wherein a ratio of a width of the second section to a width of the negative electrode current collector is greater than 0 and not greater than 0.75.

19 . The method according to claim 15 , wherein a width of the first portion is equal to that of the second portion.

20 . The method according to claim 15 , wherein a mass content of the solid electrolyte in the second negative electrode slurry is greater than 0 and not greater than 30%.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 6, 2024
From: CONTEMPORARY AMPEREX TECHNOLOGY CO., LIMITED
To: CONTEMPORARY AMPEREX TECHNOLOGY (HONG KONG) LIMITED
Reel/Frame 068338/0402 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 18, 2023
From: WANG, XIHUI; XU, WENZHU; GE, XIAOMING
To: CONTEMPORARY AMPEREX TECHNOLOGY CO., LIMITED
Reel/Frame 063679/0491 →
Continuity (2)
Continuation PCTCN2021131507 · Nov 18, 2021
Related Publication 20230343958A1 · Oct 26, 2023
References Cited (12)
CN 206134845U · 2017 [cited by applicant]
CN 109524710A · 2019 [cited by applicant]
CN 107403904B · 2020 [cited by applicant]
CN 111095625A · 2020 [cited by applicant]
JP 2005209411A · 2005 [cited by applicant]
JP 2011154902A · 2011 [cited by applicant]
JP 2012169071A · 2012 [cited by applicant]
JP 2013182712A · 2013 [cited by applicant]
JP 2016201231A · 2016 [cited by applicant]
WO 2020059549A1 · 2020 [cited by applicant]
Fukunaga et al, WO 2020059549, English Translation from WIPO (Year: 2020). [cited by examiner]
International Search Report mailed on Jul. 27, 2022, received for PCT Application PCT/CN2021/131507, filed on Nov. 18, 2021, 6 pages including English Translation. [cited by applicant]