ELECTRODE-DECOUPLED REDOX FLOW BATTERY

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
18/394,890
Abstract

Described herein is a novel electrode-decoupled redox flow battery, a novel reinforced electrode-decoupled redox flow battery, and methods of using same to store energy. Advantages of these novel electrode-decoupled redox flow batteries include long life, excellent rate capability, and stability.

Claims (34)

1 . A reinforced anion exchange membrane (AEM) comprising:

a block co-polymer; and

a hydrophobic reinforcement matrix.

2 . The reinforced AEM of claim 1 , wherein the block co-polymer is chloromethylated.

3 . The reinforced AEM of claim 1 , wherein the block co-polymer is functionalized with a functionalizing cation.

4 . The reinforced AEM of claim 1 , wherein the block co-polymer is a triblock co-polymer.

5 . The reinforced AEM of claim 1 , wherein the triblock co-polymer comprises polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene (SEBS).

6 . The reinforced AEM of claim 1 , wherein the SEBS triblock co-polymer is chloromethylated and functionalized with trimethylamine.

7 . The reinforced AEM of claim 1 , wherein the hydrophobic reinforcement matrix comprises porous extended polytetrafluoroethylene (e-PTFE).

8 . A method of using a redox flow battery:

the method comprising using the redox flow battery to store energy,

wherein the redox flow battery comprises:

a cathode;

a catholyte comprising a transition metal ion and a supporting electrolyte, wherein the transition metal ion and the supporting electrolyte form a first solvation structure having a diameter in a range of from about 0.1 nm to about 3 nm;

an anode;

an anolyte comprising a lanthanide ion and a supporting electrolyte, wherein the lanthanide ion and the supporting electrolyte form a second solvation structure having a diameter in a range of from about 0.1 nm to about 3 nm; and,

a permselective ion exchange membrane separating the cathode and the catholyte from the anode and the anolyte.

9 . The method of claim 8 , wherein the first supporting electrolyte and the second supporting electrolyte are identical.

10 . The method of claim 8 , wherein at least one of the first supporting electrolyte and the second supporting electrolyte do not comprise sulfuric acid.

11 . The method of claim 8 , wherein the first supporting electrolyte and the second supporting electrolyte are each independently a sulfonic acid selected from the group consisting of alkyl sulfonic acids, aryl sulfonic acids, methanesulfonic acid, ethanesulfonic acid, benzenesulfonic acid, o-toluenesulfonic acid, m-toluenesulfonic acid, p-toluenesulfonic acid, halogenated derivatives thereof, and combinations thereof.

12 . The method of claim 8 , wherein the lanthanide ion is selected from the group consisting of La, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, and combinations thereof.

13 . The method of claim 8 , wherein the lanthanide ion comprises Ce.

14 . The method of claim 8 , wherein the transition metal ion is selected from the group consisting of Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, Hf, Ta, W, Re, Os, Ir, Pt, Au, Hg, and combinations thereof.

15 . The method of claim 8 , wherein the transition metal ion is selected from the group consisting of Ti, V, and combinations thereof.

16 . The method of claim 8 , wherein the permselective ion exchange membrane is selected from the group consisting of membranes comprising SEBS membranes, quaternized cardo polyetherketone (QPEK) membranes, PTFE reinforced anion exchange membranes, block copolymers thereof, and combinations thereof.

17 . The method of claim 8 , wherein the capacity fade over 100 charge-discharge cycles is less than 0.1%.

reinforced anion exchange membrane (AEM) comprising:

a block co-polymer; and

a hydrophobic reinforcement matrix.

18 . The method of claim 8 , wherein the permselective ion exchange membrane is selected from the group consisting of an anion exchange membrane and a proton exchange membrane.

19 . The method of claim 8 , wherein the permselective ion exchange membrane is a reinforced anion exchange membrane (AEM) comprising:

a block co-polymer; and

a hydrophobic reinforcement matrix.

20 . The method of claim 19 , wherein the block co-polymer is chloromethylated.

Assignments (2)
CONFIRMATORY LICENSE Recorded Aug 28, 2024
From: WASHINGTON UNIVERSITY
To: US DEPARTMENT OF ENERGY
Reel/Frame 068798/0664 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 22, 2023
From: SANKARASUBRAMANIAN, SHRIHARI; RAMANI, VIJAY
To: WASHINGTON UNIVERSITY
Reel/Frame 065945/0623 →