Hydrophilic-like sputtered AR coating

Inventors: Michael Marshall (Andover, MN); Jeffrey Brown (St. Louis Park, MN)
Assignee: HOYA Optical Labs Of America, Inc.
G02B1/115G02B1/18
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,332,406
App. No.
18/629,763
Granted
Jun 17, 2025
Kind
B2
Abstract

An ophthalmic article having a coating system which provides antireflective and easy clean properties to the ophthalmic article. The coating system includes alternating layers of low refractive index metal oxide and high refractive index metal oxynitrides and corresponding high refractive index metal oxides. The coating system provides favorable surface energy to the ophthalmic article when at least one layer of the high refractive index metal oxynitride is encapsulated between two layers of low refractive index metal oxide.

Claims (22)

1. An ophthalmic article, comprising:

a substrate having a top surface;

a plurality of alternating a low refractive index layer and a high refractive index layer deposited on the top surface;

wherein the high refractive index layer comprises a) at least one metal oxynitride layer, or b) at least one metal oxynitride layer and a metal oxide layer; and

wherein the at least one metal oxynitride layer comprising a zirconium oxynitride layer or a titanium oxynitride layer is positioned between two low refractive index layers to provide a surface free energy to the ophthalmic article in a range of about 50-70 mN/m for a prolonged period.

2. The ophthalmic article of claim 1 , wherein the ophthalmic article comprises a hydrophilic property and an antireflective property.

3. The ophthalmic article of claim 1 , wherein the low refractive index layer comprises a metal oxide layer.

4. The ophthalmic article of claim 3 , wherein the low refractive index layer comprising the metal oxide layer includes silicon dioxide.

5. The ophthalmic article of claim 1 , wherein the high refractive index layer comprising the metal oxide layer further comprises a titanium dioxide layer or a zirconium dioxide layer.

6. The ophthalmic article of claim 1 , wherein the zirconium oxynitride layer or titanium oxynitride layer positioned between the two low refractive index layers to provide a polar surface energy to the ophthalmic article in a range of about 15-40 mN/m for a prolonged period.

7. The ophthalmic article of claim 1 , wherein the zirconium oxynitride layer or the titanium oxynitride layer positioned between the two low refractive index layers to provide a surface cleanability ratio of greater than 90% of the ophthalmic article.

8. The ophthalmic article of claim 2 , wherein the ophthalmic article is easy to clean because of the hydrophilic property.

9. An anti-reflective and easy-cleaning coating on a surface of an ophthalmic lens, comprising:

at least one high refractive index layer comprising a metal oxynitride layer encapsulated between two low refractive index layers;

wherein the at least one high refractive index layer comprising the metal oxynitride layer further comprises a zirconium oxynitride layer or a titanium oxynitride layer and the two low refractive index layers comprise a silicon dioxide layer to obtain a surface free energy of the ophthalmic lens in a range of about 50-70 mN/m for about 40 days of time.

10. The anti-reflective and easy-cleaning coating of claim 9 , wherein the two low refractive index layers comprise silicon dioxide.

11. The anti-reflective and easy-cleaning coating of claim 9 , wherein the anti-reflective and easy-cleaning coating further comprises a second high refractive index layer comprising a metal oxide layer.

12. The anti-reflective and easy-cleaning coating of claim 11 , wherein the second high refractive index layer comprising the metal oxide layer further comprises a titanium dioxide layer or a zirconium dioxide layer.

13. The anti-reflective and easy-cleaning coating of claim 9 , wherein a surface cleanability ratio of the ophthalmic lens is greater than 90%.

14. The anti-reflective and easy-cleaning coating of claim 9 , wherein the ophthalmic lens comprises hydrophilic property.

15. The anti-reflective and easy-cleaning coating of claim 9 , wherein a polar surface energy of the ophthalmic lens remains in a range of about 15-40 mN/m for about 40 days of time.

16. The anti-reflective and easy-cleaning coating of claim 11 , wherein the high refractive index layer of the metal oxynitride and the second high refractive index layer of the metal oxide have about the same refractive indexes in a range of about 2.1276 to 2.1308.

Continuity (3)
Continuation 16927830 · Jul 13, 2020
Provisional Application 62873779 · Jul 12, 2019
Related Publication 20240288609A1 · Aug 29, 2024
References Cited (21)
US 5728456A · Adair et al. · 1998 [cited by applicant]
US 6830785B1 · Hayakawa et al. · 2004 [cited by applicant]
US 7527867B2 · Aumercier et al. · 2009 [cited by applicant]
US 20020051294A1 · Katayama et al. · 2002 [cited by applicant]
US 20030048538A1 · Tonar et al. · 2003 [cited by applicant]
US 20070279750A1 · Yaoita et al. · 2007 [cited by applicant]
US 20090029179A1 · Fukada et al. · 2009 [cited by applicant]
US 20130182328A1 · Stewart et al. · 2013 [cited by applicant]
US 20150146161A1 · Rigato et al. · 2015 [cited by applicant]
US 20170306475A1 · Imoto et al. · 2017 [cited by applicant]
US 20180067337A1 · Brown et al. · 2018 [cited by applicant]
US 20180321425A1 · Hart et al. · 2018 [cited by applicant]
CN 1890585A · 2007 [cited by applicant]
WO WO2008110560A1 · 2008 [cited by applicant]
Japanese Patent Office, Office Action dated Mar. 14, 2024 with English translation in Japanese Patent Application No. 2022-501224, 20 pages. [cited by applicant]
WIPO, U.S. International Search Authority, International Search Report and Written Opinion mailed Oct. 7, 2020 in International Patent Application No. PCT/US2020/041847, 11 pages. [cited by applicant]
Lan, Yucheng, et al., “Mini review on photocatalysis of titanium dioxide nanoparticles and their solar applications,” [cited by applicant]
Hashimoto, K. et al., “TiO [cited by applicant]
Asahi, R. et al., “Visible-Light Photocatalysis in Nitrogen-Doped Titanium Oxides,” [cited by applicant]
Rawal et al., “Effect of Power Variation on Wettability and Optical Properties of Co-Sputtered Titanium and Zirconium Oxynitride Films”, Bull Mater Sci 36, 403-409 (2013).E. [cited by applicant]
European Patent Office, Communication pursuant to Article 94(3) EPC dated Mar. 11, 2025 in European Patent Application No. 20841334.4, 5 pages. [cited by applicant]