IP Library Granted Patent US 9,689,157
Granted Patent B1
US 9,689,157 · App. 14/455,398 · Granted Jun 27, 2017

Fire and water resistant expansion and seismic joint system

Inventors: Lester Hensley (Westborough, MA); Bill Witherspoon (Guelph, CA)
Assignee: EMSEAL JOINT SYSTEMS LTD.
E04B1/68C09K21/00E04B1/66E04B1/94E04B1/98
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,689,157
App. No.
14/455,398
Granted
Jun 27, 2017
Kind
B1
Abstract

A fire and water resistant expansion joint system has a cover plate; a spline attached to the cover plate along a first edge of the spline; and two portions of foam, each portion being located on an opposing face of the spline. The foam has a fire-retardant material infused therein. The spline depends from the cover plate and is positioned in a gap between substantially coplanar substrates such that the cover plate overlies the gap. Each portion of the foam is compressed between a respective face of the spline and a face of one of the coplanar substrates.

Claims (28)

1. A fire and water resistant expansion joint system, comprising:

a cover plate;

a spline attached to the cover plate;

foam having a fire retardant material infused therein located on a first face and a second face of the spline;

wherein the spline depends from the cover plate and is configured to be positioned in a gap between substrates such that the cover plate overlies the gap; and

wherein the foam is compressible between the first face of the spline and one of the substrates and the foam is compressible between the second face of the spline and the other of the substrates, wherein the fire retardant infused foam has a density when compressed in a range of about 200 kg/m 3 to about 700 kg/m 3 , and the fire and water resistant expansion joint system and the fire retardant infused foam are capable of withstanding exposure to a temperature of about 540° C. at about five minutes, and are configured to pass testing mandated by UL 2079.

2. The expansion joint system of claim 1 , wherein a ratio of fire retardant material infused into the first foam and the second foam is in a range of about 3.5:1 to about 4:1.

3. The expansion joint system of claim 2 , wherein the fire retardant material infused into the foam comprises aluminum tri-hydrate.

4. The expansion joint system of claim 1 , wherein the foam comprises a plurality of laminations into which the fire retardant material is infused.

5. The expansion joint system of claim 1 , wherein the foam comprises a block of foam.

6. The expansion joint system of claim 5 , wherein the spline is of monolithic construction.

7. The expansion joint system of claim 1 , comprising a layer of elastomer on the foam.

8. The fire and water resistant expansion joint system of claim 1 , wherein the fire and water resistant expansion joint system and the fire retardant infused foam are capable of withstanding exposure to a temperature of about 930° C. at about one hour.

9. The fire and water resistant expansion joint system of claim 1 , wherein the fire and water resistant expansion joint system and the fire retardant infused foam are capable of withstanding exposure to a temperature of about 1010° C. at about two hours.

10. The fire and water resistant expansion joint system of claim 1 , wherein the fire and water resistant expansion joint system and the fire retardant infused foam are capable of withstanding exposure to a temperature of about 1260° C. at about eight hours.

11. A fire and water resistant expansion joint system, comprising:

a cover plate;

a spline attached to the cover plate;

foam having a fire retardant material infused therein located on a first face and a second face of the spline;

wherein the spline depends from the cover plate and is configured to be positioned in a gap between substrates such that the cover plate overlies the gap; and

wherein the foam is compressible between the first face of the spline and one of the substrates and the foam is compressible between the second face of the spline and the other of the substrates, wherein the fire retardant infused foam has a density when compressed in a range of about 200 kg/m 3 to about 700 kg/m 3 , and the fire and water resistant expansion joint system and the fire retardant infused foam are configured to maintain fire resistance at a temperature of about 540° C. at about five minutes, and are configured to pass testing mandated by UL 2079.

12. The fire and water resistant expansion joint system of claim 1 , wherein the fire and water resistant expansion joint system and the fire retardant infused foam are capable of withstanding exposure to a temperature of about 1052° C. at about three hours.

13. The fire and water resistant expansion joint system of claim 1 , wherein the fire and water resistant expansion joint system and the fire retardant infused foam are capable of withstanding exposure to a temperature of about 1093° C. at about four hours.

14. The expansion joint system of claim 11 , wherein the system and the fire retardant infused foam are configured to maintain fire resistance at a temperature of about 930° C. at about one hour.

15. The expansion joint system of claim 11 , wherein the system and the fire retardant infused foam are configured to maintain fire resistance at a temperature of about 1010° C. at about two hours.

16. The expansion joint system of claim 11 , wherein the system and the fire retardant infused foam are configured to maintain fire resistance at a temperature of about 1052° C. at about three hour.

17. The expansion joint system of claim 11 , wherein the system and the fire retardant infused foam are configured to maintain fire resistance at a temperature of about 1093° C. at about four hours.

18. The expansion joint system of claim 11 , wherein the system and the fire retardant infused foam are configured to maintain fire resistance at a temperature of about 1260° C. at about eight hours.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 16, 2014
From: HENSLEY, LESTER; WITHERSPOON, BILL
To: EMSEAL JOINT SYSTEMS LTD.
Reel/Frame 033963/0971 →
Continuity (3)
Continuation 13723605 · Dec 21, 2012
Continuation 12730354 · Mar 24, 2010
Provisional Application 61162820 · Mar 24, 2009